公开(公告)号:US20180126706A1
公开(公告)日:2018-05-10
申请号:US15575524
申请日:2016-05-31
Applicant: 3M INNOVATIVE PROPERTIES COMPANY
Inventor: Belma Erdogan-Haug , Albert I. Everaerts , David S. Hays , David J. Kinning , Maria A. Appeaning , Jong-Seob Won
CPC classification number: B32B25/20 , B32B1/00 , B32B3/00 , B32B7/00 , B32B7/02 , B32B7/04 , B32B7/10 , B32B7/12 , B32B25/00 , B32B25/04 , B32B25/08 , B32B25/14 , B32B27/00 , B32B27/06 , B32B27/08 , B32B27/26 , B32B27/28 , B32B2250/00 , B32B2250/03 , B32B2250/05 , B32B2250/40 , B32B2307/40 , B32B2307/412 , B32B2307/50 , B32B2307/51 , B32B2307/542 , B32B2307/546 , B32B2307/548 , B32B2307/732 , B32B2457/00 , B32B2457/20 , B32B2551/00
Abstract: The present invention is an assembly layer for a flexible device. The assembly layer is derived from precursors in eluding at least one of a physically cross-linked silicone elastomer and a covalently cross-linked silicone elastomer forming reagent mixture, and a MQ resin. Within a temperature range of between about −30 C to about 90 C, the assembly layer has a shear storage modulus at a frequency of 1 Hz that does not exceed about 2 MPa, a shear creep compliance (J) of at least about 6×10−6 1/Pa measured at 5 seconds with an applied shear stress between about 50 kPa and about 500 kPa, and a strain recovery of at least about 50% at at least one point of applied shear stress within the range of about 5 kPa to about 500 kPa within about 1 minute after removing the applied shear stress.
-
公开(公告)号:US11332642B2
公开(公告)日:2022-05-17
申请号:US16935339
申请日:2020-07-22
Applicant: 3M INNOVATIVE PROPERTIES COMPANY
Inventor: Belma Erdogan-Haug , Albert I. Everaerts , David S. Hays , David J. Kinning , Maria A. Appeaning , Jong-Seob Won , Ross E. Behling , Jason D. Clapper , Marie Aloshyna ep Lesuffleur
IPC: C09J7/10 , B32B7/12 , B32B27/40 , B32B27/36 , B32B25/14 , B32B27/30 , B32B3/04 , B32B27/32 , B32B27/08 , B32B25/20 , B32B27/28 , C09J7/38 , C08G77/455 , H01L51/00 , H01L51/52
Abstract: The present invention is an assembly layer for a flexible device. Within a temperature range of between about −30° C. to about 90° C., the assembly layer has a shear storage modulus at a frequency of 1 Hz that does not exceed about 2 MPa, a shear creep compliance (J) of at least about 6×10−6 1/Pa measured at 5 seconds with an applied shear stress between about 50 kPa and about 500 kPa, and a strain recovery of at least about 50% at at least one point of applied shear stress within the range of about 5 kPa to about 500 kPa within about 1 minute after removing the applied shear stress. The assembly layer includes at least one of a polyisoprene, a polybutadiene, an olefin block copolymer, a polyisobutylene, and high alkyl polyolefin.
-
公开(公告)号:US10752810B2
公开(公告)日:2020-08-25
申请号:US15575680
申请日:2016-05-31
Applicant: 3M INNOVATIVE PROPERTIES COMPANY
Inventor: Belma Erdogan-Haug , Albert I. Everaerts , David S. Hays , David J. Kinning , Maria A. Appeaning , Jong-Seob Won , Ross E. Behling , Jason D. Clapper , Marie Aloshyna ep Lesuffleur
IPC: C09J7/38 , B32B7/12 , B32B27/40 , B32B27/36 , C09J7/10 , B32B25/14 , B32B27/30 , B32B3/04 , B32B27/32 , B32B27/08 , B32B25/20 , B32B27/28 , C08G77/455 , H01L51/00 , H01L51/52
Abstract: The present invention is an assembly layer for a flexible device. Within a temperature range of between about −30° C. to about 90° C., the assembly layer has a shear storage modulus at a frequency of 1 Hz that does not exceed about 2 MPa, a shear creep compliance (J) of at least about 6×10−6 l/Pa measured at 5 seconds with an applied shear stress between about 50 kPa and about 500 kPa, and a strain recovery of at least about 50% at at least one point of applied shear stress within the range of about 5 kPa to about 500 kPa within about 1 minute after removing the applied shear stress.
-
公开(公告)号:US20200347271A1
公开(公告)日:2020-11-05
申请号:US16935339
申请日:2020-07-22
Applicant: 3M INNOVATIVE PROPERTIES COMPANY
Inventor: Belma Erdogan-Haug , Albert I. Everaerts , David S. Hays , David J. Kinning , Maria A. Appeaning , Jong-Seob Won , Ross E. Behling , Jason D. Clapper , Marie Aloshyna ep Lesuffleur
IPC: C09J7/10 , B32B7/12 , B32B27/40 , B32B27/36 , B32B25/14 , B32B27/30 , B32B3/04 , B32B27/32 , B32B27/08 , B32B25/20 , B32B27/28 , C09J7/38 , C08G77/455 , H01L51/00 , H01L51/52
Abstract: The present invention is an assembly layer for a flexible device. Within a temperature range of between about −30° C. to about 90° C., the assembly layer has a shear storage modulus at a frequency of 1 Hz that does not exceed about 2 MPa, a shear creep compliance (J) of at least about 6×10−6 1 /Pa measured at 5 seconds with an applied shear stress between about 50 kPa and about 500 kPa, and a strain recovery of at least about 50% at at least one point of applied shear stress within the range of about 5 kPa to about 500 kPa within about 1 minute after removing the applied shear stress. The assembly layer includes at least one of a polyisoprene, a polybutadiene, an olefin block copolymer, a polyisobutylene, and high alkyl polyolefin.
-
公开(公告)号:US20180291238A1
公开(公告)日:2018-10-11
申请号:US15575680
申请日:2016-05-31
Applicant: 3M INNOVATIVE PROPERTIES COMPANY
Inventor: Belma Erdogan-Haug , Albert I. Everaerts , David S. Hays , David J. Kinning , Maria A. Appeaning , Jong-Seob Won , Ross E. Behling , Jason D. Clapper , Marie Aloshyna ep Lesuffleur
IPC: C09J7/38 , C08G77/455 , H01L51/00 , H01L51/52 , B32B7/12
Abstract: The present invention is an assembly layer for a flexible device. Within a temperature range of between about −30° C. to about 90° C., the assembly layer has a shear storage modulus at a frequency of 1 Hz that does not exceed about 2 MPa, a shear creep compliance (J) of at least about 6×10−6/Pa measured at 5 seconds with an applied shear stress between about 50 kPa and about 500 kPa, and a strain recovery of at least about 50% at at least one point of applied shear stress within the range of about 5 kPa to about 500 kPa within about 1 minute after removing the applied shear stress.
-
-
-
-