公开(公告)号:WO2003076509A1
公开(公告)日:2003-09-18
申请号:PCT/IB2003/000835
申请日:2003-03-06
Applicant: BASELL POLIOLEFINE ITALIA S.P.A.
Inventor: GLOGOVSKY, Todd , BUTALA, Robert, G. , HAN, Choong, Y. , ENNIS, Gerald, John , GOBERTI, Paolo
IPC: C08L23/10
CPC classification number: C08L23/16 , C08L23/10 , C08L23/142 , C08L2308/00 , C08L2666/06
Abstract: A polyolefin composition suitable for preparing single ply roofing membranes, comprising: (A) from about 15 to 40% by weight of a crystalline copolymer of propylene with at least one alpha-olefin of formula H 2 C=CHR 1 , where R 1 is H or a C 2-8 linear or branched alkyl, containing at least about 90% by weight of propylene, having solubility in xylene at room temperature lower than about 15% by weight; (B) from about 60 to about 85% by weight of an elastomeric fraction comprising: (1) a copolymer of propylene with ethylene containing about 20 to about 35% by weight ethylene, and having solubility in xylene at room temperature greater than about 70% by weight, the intrinsic viscosity of the xylene soluble fraction being higher than about 3.0dl/g; and (2) a copolymer of ethylene with at least one alpha-olefin of formula H 2 C=CHR 2 , where R 2 is a C 2-8 linear or branched alkyl, containing about 15% to 40% by weight alpha-olefin, and having solubility in xylene at room temperature greater than about 25% by weight, the intrinsic viscosity of the xylene soluble fraction ranging from about 0.5 to about 5.0dl/g; the (1) (2) weight ratio ranging from about 1:5 to about 5:1. The polyolefin composition of the invention, preferably prepared by sequential polymerization in at least three stages, has tensile strength at break ≥ 25 Mpa, elongation at break ≥ 700 Mpa and toughness ≥ 150 Mpa.
Abstract translation: 一种适于制备单层屋顶膜的聚烯烃组合物,其包含:A约15至40重量%的丙烯与至少一种式IIC = CHR1的α-烯烃的结晶共聚物,其中R 1为H或C 2-8 含有至少约90重量%丙烯的直链或支链烷基,其在室温下在二甲苯中的溶解度低于约15重量%B,约60至约85重量%的弹性体级分包括:1 丙烯与含有约20至约35重量%乙烯的乙烯,并且在室温下在二甲苯中的溶解度大于约70重量%,二甲苯可溶部分的特性粘度高于约3.0dl / g,2共聚物 的乙烯与至少一种式H2C = CHR2的α-烯烃,其中R2是C2-8直链或支链烷基,含有约15%至40%(重量)的α-烯烃,并且在室温下在二甲苯中的溶解度大于 约25% 重量,二甲苯可溶部分的特性粘度范围为约0.5至约5.0dl / g,重量比为约1:5至约5:1。 本发明的聚烯烃组合物优选通过至少三个阶段的顺序聚合制备,断裂强度> 25Mpa,断裂伸长率> 700Mpa,韧性> 150Mpa。
-
公开(公告)号:EP1483324A1
公开(公告)日:2004-12-08
申请号:EP03704900.4
申请日:2003-03-06
Applicant: Basell Poliolefine Italia S.p.A.
Inventor: GLOGOVSKY, Todd , BUTALA, Robert, G. , HAN, Choong, Y. , ENNIS, Gerald, John , GOBERTI, Paolo
CPC classification number: C08L23/16 , C08L23/10 , C08L23/142 , C08L2308/00 , C08L2666/06
Abstract: A polyolefin composition suitable for preparing single ply roofing membranes, comprising: (A) from about 15 to 40% by weight of a crystalline copolymer of propylene with at least one alpha-olefin of formula H2C=CHR1, where R1 is H or a C2-8 linear or branched alkyl, containing at least about 90% by weight of propylene, having solubility in xylene at room temperature lower than about 15% by weight; (B) from about 60 to about 85% by weight of an elastomeric fraction comprising: (1) a copolymer of propylene with ethylene containing about 20 to about 35% by weight ethylene, and having solubility in xylene at room temperature greater than about 70% by weight, the intrinsic viscosity of the xylene soluble fraction being higher than about 3.0dl/g; and (2) a copolymer of ethylene with at least one alpha-olefin of formula H2C=CHR2, where R2 is a C2-8 linear or branched alkyl, containing about 15% to 40% by weight alpha-olefin, and having solubility in xylene at room temperature greater than about 25% by weight, the intrinsic viscosity of the xylene soluble fraction ranging from about 0.5 to about 5.0dl/g; the (1) (2) weight ratio ranging from about 1:5 to about 5:1. The polyolefin composition of the invention, preferably prepared by sequential polymerization in at least three stages, has tensile strength at break ≥ 25 Mpa, elongation at break ≥ 700 Mpa and toughness ≥ 150 Mpa.
-