CPC classification number: C08L23/12 , C08F2/001 , C08K3/24 , C08K5/0083 , C08K5/053 , C08K5/521 , C08L23/16 , C08L2205/02 , C08L2205/24 , C08L2207/02 , C08L2314/02
Abstract: The invention relates to a heterophasic polypropylene compositions comprising 68-76 % by weight of a propylene homopolymer or copolymer matrix, 24-32 % by weight of an ethylene-propylene copolymer and a nucleating agent. The composition has an intrinsic viscosity of the xylene soluble fraction at room temperature up to 1.3 dl/g and a melt flow rate (230 °C, 2.16 kg) of 30 to 70 g/10 min. The compositions disclosed herein can be used to prepare molded articles, particularly by thin wall injection molding, that are endowed with excellent impact behaviour.
Abstract translation: 本发明涉及包含68-76重量%的丙烯均聚物或共聚物基质,24-32重量%的乙烯 - 丙烯共聚物和成核剂的多相聚丙烯组合物。 该组合物在室温下的二甲苯可溶级分的特性粘度高达1.3dl / g,熔体流动速率(230℃,2.16kg)为30-70g / 10min。 本文公开的组合物可用于制备具有优异冲击性能的模制品,特别是通过薄壁注射成型。
-
公开(公告)号:WO2019177180A8
公开(公告)日:2019-09-19
申请号:PCT/JP2019/012288
申请日:2019-03-15
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: TSUKAHARA, Takeshi , TSURUMI, Nobuyuki , KANNO, Shitoshi , YAMAMOTO, Kunio , NAKAJIMA, Takeshi
IPC: C08F210/06 , C08F210/16
Abstract: The present invention provides a polypropylene composition having an excellent balance between transparency and flexibility. A polypropylene composition comprising: as component (1), a propylene/ethylene copolymer containing 2 to 4% by weight of an ethylene-derived unit; and as component (2), an ethylene/propylene copolymer containing 65 to 87% by weight of an ethylene-derived unit; wherein the polypropylene composition satisfies the following requirements: 1) the weight ratio of component (1) to component (2) is in the range of 65:35 to 77:23, 2) the intrinsic viscosity of xylene solubles (XSIV) of the composition is in the range of 0.8 to 1.4 dl/g, 3) the MFR (at 230°C under a load of 2.16 kg) of the composition is in the range of 15 to 40 g/10 min., 4) no crystal nucleating agent is contained.
-
公开(公告)号:EP3765566A1
公开(公告)日:2021-01-20
申请号:EP19717621.7
申请日:2019-03-15
Applicant: Basell Poliolefine Italia S.r.l.
Inventor: TSUKAHARA, Takeshi , TSURUMI, Nobuyuki , KANNO, Shitoshi , YAMAMOTO, Kunio , NAKAJIMA, Takeshi
IPC: C08L23/12
-
公开(公告)号:EP3164421B1
公开(公告)日:2019-05-15
申请号:EP15726636.2
申请日:2015-06-08
Applicant: Basell Poliolefine Italia S.r.l.
Inventor: TSUKAHARA, Takeshi , TSURUMI, Nobuyuki , KANNO, Shitoshi , YAMAMOTO, Kunio , NAKAJIMA, Takeshi
-
公开(公告)号:EP3765534A1
公开(公告)日:2021-01-20
申请号:EP19717372.7
申请日:2019-03-15
Applicant: Basell Poliolefine Italia S.r.l.
Inventor: TSUKAHARA, Takeshi , TSURUMI, Nobuyuki , KANNO, Shitoshi , YAMAMOTO, Kunio , NAKAJIMA, Takeshi
IPC: C08F210/06 , C08F210/16
-
公开(公告)号:EP3164421A1
公开(公告)日:2017-05-10
申请号:EP15726636.2
申请日:2015-06-08
Applicant: Basell Poliolefine Italia S.r.l.
Inventor: TSUKAHARA, Takeshi , TSURUMI, Nobuyuki , KANNO, Shitoshi , YAMAMOTO, Kunio , NAKAJIMA, Takeshi
CPC classification number: C08L23/12 , C08F2/001 , C08F210/06 , C08K3/24 , C08K5/0083 , C08K5/053 , C08K5/521 , C08L23/16 , C08L2205/02 , C08L2205/24 , C08L2207/02 , C08L2314/02 , C08F210/16 , C08F4/651 , C08F110/06 , C08F2500/12 , C08F2500/17
Abstract: The present disclosure generally relates to a heterophasic polypropylene composition comprising 68-76% by weight of a propylene homopolymer or copolymer matrix, 24-32% by weight of an ethylene-propylene copolymer, and a nucleating agent. In some embodiments, the composition has an intrinsic viscosity of the xylene soluble (XSIV) fraction at room temperature of up to 1.3 dl/g and a melt flow rate (230° C., 2.16 kg) of 30 to 70 g/10 min. The compositions disclosed herein can be used in molded articles, using techniques such as thin wall injection molding, that are endowed with excellent impact behavior.
Abstract translation: 本发明涉及包含68-76重量%的丙烯均聚物或共聚物基体,24-32重量%的乙烯 - 丙烯共聚物和成核剂的多相聚丙烯组合物。 该组合物室温下二甲苯可溶部分的特性粘度为1.3dl / g,熔体流动速率(230℃,2.16kg)为30-70g / 10min。 本文公开的组合物可以用于制备模制品,特别是通过薄壁注射成型,其被赋予优异的冲击行为。
-
-
-
-
-