公开(公告)号:US3576662A
公开(公告)日:1971-04-27
申请号:US3576662D
申请日:1969-08-01
Applicant: BASF AG
Inventor: DIEBOLD ADOLF , DOERR LUDWIG , RAICHLE LUDWIG , MARQUARDT SIEGFRIED
IPC: C08J7/04 , C09D175/04 , C23C18/20 , C25D5/56 , G11B5/702 , G11B5/72 , G11B5/73 , H01G13/06 , H05K3/18 , B44D1/16
CPC classification number: H05K3/188 , C08J7/047 , C09D175/04 , C23C18/206 , C25D5/56 , G11B5/7021 , G11B5/7022 , G11B5/72 , G11B5/7305 , H01G13/06 , Y10T428/12049 , Y10T428/12111 , Y10T428/12569 , Y10T428/31609 , C08L2666/54
Abstract: A METHOD FOR METALLIZING PLASTICS SURFACES BY COATING SAID SURFACES WITH A THIN LAYER OF IRONPARTICLES HAVING A MEAN PARTICLE SIZE OF ABOUT 0.1 TO 1 MICRO FINELY DISPERSED IN A POLYURETHANE BINDER, DRYING AND TREATING THE LAYER WITH AN ACIDIC AQUEOUS SOLUTION OF A SALT OF COPPER OR SILVER.
-
公开(公告)号:FR1486816A
公开(公告)日:1967-06-30
申请号:FR69543
申请日:1966-07-15
Applicant: BASF AG
Inventor: DIEBOLD ADOLF , MARQUARDT SIEGFRIED , DOERR LUDWIG , RAICHLE LUDWIG
-
公开(公告)号:GB1149033A
公开(公告)日:1969-04-16
申请号:GB3186666
申请日:1966-07-15
Applicant: BASF AG
Inventor: DIEBOLD ADOLF , MARQUARDT SIEGFRIED , DOERR LUDWIG , RAICHLE LUDWIG
IPC: C08J7/04 , C09D175/04 , C23C18/20 , C25D5/56 , G11B5/702 , G11B5/72 , G11B5/73 , H01G13/06 , H05K3/18
Abstract: 1,149,033. Coating with metals. BADISCHE ANILIN - & SODA-FABRIK A. G. No. 31866/66. Headings C7B and C7F. In an electroless process for coating a plastics sheet with copper or silver in which the plastics surface is first coated with iron powder in a binder, the binder contains at least 20% by weight of a polyisocyanate. The binder may also include vinyl copolymers, polyvinyl chloride, acetal, formal or butyral or soluble polyamide. The coating may be applied through a stencil, and the powdered iron coating may be annealed at a temperature up to 60 C. prior to deposition. A bath for depositing copper may comprise (g./l.) 150 copper sulphate, 40 triethanolamine, and 27 sulphuric acid. A silver layer may be deposited on the copper using a bath comprising 1À5 silver nitrate, 3 E.D.T.A., 3 sodium thiosulphate, and 2 tartaric acid. The copper surface may be electro-plated with a further layer of copper, using the same bath as for the electroless-plating, and then with Cr, Ni, Co or Rh, and the copper or silver surfaces may be electro-plated with Fe, Ni or Co or mixtures thereof.
-
公开(公告)号:GB1073006A
公开(公告)日:1967-06-21
申请号:GB3757164
申请日:1964-09-15
Applicant: BASF AG
Inventor: DIEBOLD ADOLF , DOERR LUDWIG
IPC: C23C18/20 , C23C18/38 , C23C18/52 , H01B1/00 , H01F41/24 , H01G13/06 , H05K3/10 , H05K3/18 , H05K3/24
Abstract: A plastics, e.g. polyester, tape is coated with copper by first coating with a dispersion of iron particles in e.g. polyvinyl chloride, and then passing through a bath of e.g. (parts by weight) 30 copper sulphate, 6 sulphuric acid, 6 tartaric acid, and 6 trimethylaminoacetic acid. A further coating of silver may be applied by passing through a bath of a mercury salt and then an ammoniacal bath of potassium silver cyanide. An electroless nickel coating may be applied to the copper. The iron layer may be applied, whilst subjected to a magnetic field, and to form a pattern e.g. by a stencil. A copper coated plastics tape may be electroplated with Cd, Sn, Au, Ag or Co - Ni e.g. by passing the tape as a cathode through an aqueous solution (pH 5 to 6) of E.D.T.A., cadmium acetate, and HCl or tin chloride and E.D.T.A. or nickel sulphanate, cobalt chloride, and trimethylaminoacetic acid.
-
-
公开(公告)号:DE1521152A1
公开(公告)日:1969-04-24
申请号:DE1521152
申请日:1965-07-16
Applicant: BASF AG
Inventor: DIEBOLD DR ADOLF , MARQUARDT SIEGFRIED , DOERR LUDWIG , LUDWIG RAICHLE DIPL ING
IPC: C08J7/04 , C09D175/04 , C23C18/20 , C25D5/56 , G11B5/702 , G11B5/72 , G11B5/73 , H01G13/06 , H05K3/18
Abstract: 1,149,033. Coating with metals. BADISCHE ANILIN - & SODA-FABRIK A. G. No. 31866/66. Headings C7B and C7F. In an electroless process for coating a plastics sheet with copper or silver in which the plastics surface is first coated with iron powder in a binder, the binder contains at least 20% by weight of a polyisocyanate. The binder may also include vinyl copolymers, polyvinyl chloride, acetal, formal or butyral or soluble polyamide. The coating may be applied through a stencil, and the powdered iron coating may be annealed at a temperature up to 60 C. prior to deposition. A bath for depositing copper may comprise (g./l.) 150 copper sulphate, 40 triethanolamine, and 27 sulphuric acid. A silver layer may be deposited on the copper using a bath comprising 1À5 silver nitrate, 3 E.D.T.A., 3 sodium thiosulphate, and 2 tartaric acid. The copper surface may be electro-plated with a further layer of copper, using the same bath as for the electroless-plating, and then with Cr, Ni, Co or Rh, and the copper or silver surfaces may be electro-plated with Fe, Ni or Co or mixtures thereof.
-
-
-
-
-