METHOD FOR PRODUCING HOMOPOLYMERS AND COPOLYMERS OF VINYLPHOSPHONIC ACID
    1.
    发明申请
    METHOD FOR PRODUCING HOMOPOLYMERS AND COPOLYMERS OF VINYLPHOSPHONIC ACID 审中-公开
    制备乙烯基膦酸的均聚物和共聚物的方法

    公开(公告)号:WO2008090153A3

    公开(公告)日:2008-09-18

    申请号:PCT/EP2008050705

    申请日:2008-01-22

    CPC classification number: C08F230/02

    Abstract: The invention relates to a method for producing homopolymers and copolymers of vinylphosphonic acid having a content of vinylphosphonic acid polymerized into it of at least 30% by weight, based on the overall weight of the homopolymer or copolymer, said method comprising the radical polymerization of a monomer composition that contains, based on the overall amount of the monomers in the monomer composition, a) > 30% by weight of vinylphosphonic acid in the form of its anhydride or an anhydride derivative or in the form of a mixture of vinylphosphonic acid and its anhydride or anhydride derivative (monomer a), and b)

    Abstract translation: 本发明涉及用于均聚物和具有至少30%(重量)共聚的乙烯基膦酸的含量乙烯基膦酸共聚物的制备方法,根据基于所述均聚物或共聚物包含单体组合物的自由基聚合反应的总重量 单体的单体组合物的总量,一)>在其酸酐的形式或和乙烯基膦酸的混合物及其酸酐或酸酐衍生物(单体形式的酸酐衍生物或30重量%的乙烯基膦酸a)和b)<70 重量%的除乙烯基膦酸以外的一种或多种烯键式不饱和单体(单体b),其中聚合反应在非水溶剂或稀释剂中进行。 本发明还涉及通过该方法可获得的均聚物和共聚物。

    2.
    发明专利
    未知

    公开(公告)号:DE10352876A1

    公开(公告)日:2005-06-23

    申请号:DE10352876

    申请日:2003-11-10

    Applicant: BASF AG

    Inventor: KLOPSCH RAINER

    Abstract: Polyisocyanates for the production of flexible polyurethane foam comprise prepolymers with NCO content = not more than 17.5 wt%, obtained by reacting 4,4'-MDI with polyether-alcohol(s) (with 10-20 wt% ethylene oxide units) to give a prepolymer with NCO content = 10-14 wt% and then reacting this with polyphenylene-polymethylene-polyisocyanates. A method for the production of flexible polyurethane foam with a density of 30-80 g/l by reacting (a) polyisocyanates with (b) compounds with at least 2 isocyanate-reactive hydrogen atoms in presence of (c) blowing agents. Component (a) comprises polyisocyanate prepolymers with an NCO content of not more than 17.5 wt%, obtained by (i) reacting 4,4'-MDI with polyether-alcohol(s) showing an OH number of 20-60 mg KOH/g and containing 10-20 wt% ethylene oxide units in the polyether chain (based on total alkylene oxide content), to give a prepolymer with an NCO content of 10-40 wt% and then (ii) mixing the prepolymer with polyphenylene-polymethylene-polyisocyanates. An independent claim is also included for flexible polyurethane foam with a density of 30-80 g/l obtained by this method.

    3.
    发明专利
    未知

    公开(公告)号:DE102005003116A1

    公开(公告)日:2006-07-27

    申请号:DE102005003116

    申请日:2005-01-21

    Applicant: BASF AG

    Abstract: Composition comprising a hydrogenated bisglycidyl ether and a crosslinker, wherein the hydrogenated bisglycidyl ether has the formula I where R is CH 3 or H, and is obtained by hydrogenation of the aromatic rings of a corresponding bisglycidyl ether of the formula II where the degree of hydrogenation is >98%, and the crosslinker has no aromatic structural elements. Process for preparing a crosslinked epoxy resin, in which the abovementioned composition is used. Crosslinked epoxy resins which can be prepared by the abovementioned process, and their uses.