公开(公告)号:DE2730017A1
公开(公告)日:1979-01-18
申请号:DE2730017
申请日:1977-07-02
Applicant: BASF AG
Inventor: STRAUB FERDINAND DIPL CHEM DR , SPOOR HERBERT DIPL CHEM DR , SCHENCK HANS-UWE DIPL CHEM , SCHWARZ WOLFGANG DIPL CHEM DR
IPC: C08F2/00 , C08F2/04 , C08F4/00 , C08F4/28 , C08F4/32 , C08F6/00 , C08F6/06 , C08F6/10 , C08F26/00 , C08F26/06 , C08F26/10 , C08F218/00 , C08F218/02 , C08F218/04 , C08F218/08 , C08F226/06 , C08F226/10 , C08F263/02 , C08F271/00
Abstract: A process for reducing the residual monomer content of a copolymer prepared by copolymerizing vinyl esters and N-vinyl-lactams in a solvent in the presence of a free radical polymerization initiator. Following the main polymerization, from 0.05 to 0.5% by weight, based on the monomers employed, of di-tert.-butyl peroxide, di-tert.-amyl peroxide, dicumyl peroxide, 2,5-dimethyl-2,5-bis-(tert.-butylperoxy)-hexane, 2,2-bis-(tert.-butylperoxy)-butane, 1,1-bis-(tert.-butylperoxy)-3,3,5-trimethylcyclohexane, 4,4-di-(tert.-butylperoxy)-butyl valerate, or a mixture of these, is added to the reaction mixture and the after-polymerization is carried out at a higher temperature than the main polymerization.