公开(公告)号:DE1445535A1
公开(公告)日:1969-01-16
申请号:DE1445535
申请日:1964-07-17
Applicant: BASF AG
Inventor: OTTO HERTEL DR , WALTER HENSEL DR
-
公开(公告)号:DE1910178A1
公开(公告)日:1970-09-10
申请号:DE1910178
申请日:1969-02-28
Applicant: BASF AG
Inventor: HANS-GEORG TRIESCHMANN DR DR , WOLFGANG BALL DR , WALTER HENSEL DR , RETTIG AUGUST
Abstract: To comps. of (100 pts.) bitumen and (1-200 pts.) ethylene polymer is added powdered separation agents (0.5-10%) comprising aluminium hydrosilicate, aluminium hydroxysilicate and aluminium magnesium silicate, for tubes, hose-pipes, films and shaped rods.
-
公开(公告)号:DE1495176A1
公开(公告)日:1969-01-02
申请号:DE1495176
申请日:1964-04-29
Applicant: BASF AG
Inventor: OTTO HERTEL DR , WALTER HENSEL DR
-
公开(公告)号:DE1927527A1
公开(公告)日:1970-12-03
申请号:DE1927527
申请日:1969-05-30
Applicant: BASF AG
Inventor: HELMUT PFANNMUELLER DR , FRIEDRICH URBAN DR , WALTER HENSEL DR , OSKA BUECHNER DR
Abstract: Polyethylenes are produced continuously from a mixture of 100 wt. parts ethylene, 0.5-1.5 ppm (based on ethylene) of a radical polymersn initiator, and 0.05-5 wt. parts of a polymerisn. regulator, at increased temp. and press of 1000-3000 atm., in a tubular reactor having length, diameter ratio of 5000:1-30000:1. The polymerisn, mixture in introduced at 70-120 degrees C and the temp. increases to 230-280 degrees C in the first 5/15 of the tube, is maintained within 5 degrees C of this temp. in the next 9/15 of the tube, and is cooled in the last 1/15 to 30-60 degrees C. The mixture is passed through at 3-30 m/sec. Polymer produced has narrow softening range and also shows good mechanical properties outside this range.
-
公开(公告)号:DE1495197A1
公开(公告)日:1969-02-06
申请号:DE1495197
申请日:1964-09-15
Applicant: BASF AG
Inventor: OTTO HERTEL DR , WALTER HENSEL DR
-
-
-
-