公开(公告)号:DE4103140A1
公开(公告)日:1992-08-13
申请号:DE4103140
申请日:1991-02-02
Applicant: BASF AG
Inventor: MUEHLBACH KLAUS DR , SEITZ FRIEDRICH DR , WICKER MICHAEL , HEITZ WALTER PROF DR
Abstract: Macromonomers of formula (I) are new., where R1, R2 are lower alkyl; R3 is H or lower alkyl; and n is polymerisation deg. of at least 5. Macromonomers of formula (Ia), partic. omega-(4-vinyl-)benzoyl-poly 2,6-dimethyl-1,4 phenylene ether (VB-PPE) of polymerisation deg. of the phenylene ether of 5-200 are specifically claimed. In (Ia), n = 5-200. USE/ADVANTAGE - Used for the prepn. of copolymers (claimed). Avoids prior art problems of sepg. copolymers and unreacted monomer. The graft polymers obtd. are useful as adhesives, compatabilisers in polymer alloys or rubber in materials. In an example, 30g poly-(2,6-dimethyl-1,4-phenylene ether) (PPE) (prepd. from p-chloro-2,6-dimethyl phenol) (Mn 13400) was dissolved in 350g pyridine. 10 mols. 4-vinyl benzoyl chloride were added at 0. deg. C, giving VB-PPE after 24 hrs.. 3g VB-PPE and 7g ethyl acrylate were dissolved in 50g toluene, 0.03 AIBN added and polymerisation occurred at 60 deg. C for 30 hrs.. The polymer was pptd. in 4 pts. vol. petroleum ether and 1 pt. vol. methanol and dried. The yield was 88%.