Abstract:
PROBLEM TO BE SOLVED: To provide a mixing kneader having manufacture standard provided with a mechanical stable shaft with respect to generated high shearing force.SOLUTION: The mixing kneader is provided with at least two shafts 2, 3 and a kneading rod 4 is arranged on a web 5 in the surface of the shafts and the shafts are surrounded by the housing 6. In the housing 6, at least one opening 10 is formed on the shaft and at least one opening 11 for discharging a product is formed, the shafts 2, 3 are supported in both end parts, at least one end part is driven and the structure of the shaft is constituted so that the a value obtained by multiplying 100 to a value obtained by dividing the difference between the absolute value of bending natural frequency and exciting object frequency by the bending natural frequency may become 5.
Abstract:
PROBLEM TO BE SOLVED: To provide a method for continuously producing particulate crosslinked gelatinous polymers by copolymerizing water-soluble monoethylenically unsaturated monomers (a) with 0.001 to 5 mol% (based on the monomer (a)) of monomers (b) containing at least two polymerizable groups in a kneader. SOLUTION: The method for producing particulate crosslinked gelatinous polymers is characterized in that at least one of following conditions is satisfied: (1) the degree of charging of the monomers in the kneader is at least 71%; (2) the water-soluble monoethylenically unsaturated monomers contain hydroquinone hemi-ether up to 150 ppm; (3) the polymerization zone temperature is higher than 65°C; and (4) the kneader has back mixing ratio less than 0.33. Further, a material added to an inlet of the kneader is conveyed to an end part of the kneader in the axial direction. COPYRIGHT: (C)2010,JPO&INPIT
Abstract:
A process for preparing water-absorbing polymer beads with high permeability by polymerizing droplets of a monomer solution in a gas phase surrounding the droplets, wherein the monomer solution comprises at least 0.5% by weight of a crosslinker, based on the monomer, the polymerization in the droplet takes place in homogeneous phase, and the polymer beads have a mean diameter of at least 150 μm.
Abstract:
A process for preparing water-absorbing polymer beads with high permeability by polymerizing droplets of a monomer solution, comprising monomers bearing acid groups, in a gas phase surrounding the droplets, wherein the monomer solution comprises polyvalent cations and the polymer beads have a mean diameter of at least 150 μm.
Abstract:
A process for preparing water-absorbing polymer beads with high permeability by polymerizing droplets of a monomer solution in a gas phase surrounding the droplets, wherein a water-insoluble inorganic salt is suspended in the monomer solution and the polymer beads have a mean diameter of at least 150 μm.
Abstract:
A process for preparing postcrosslinked water-absorbing polymer beads with high absorption by polymerizing droplets of a monomer solution in a gas phase surrounding the droplets, wherein the solids content of the monomer solution is at least 35% by weight and the polymer beads have a mean diameter of at least 150 μm.