Abstract:
A process for the post-treatment of a zeolitic material having an MWW framework structure, the process comprising (i) providing a zeolitic material having an MWW framework structure, wherein the framework structure of the zeolitic material comprises X2O3 and YO2, wherein Y is a tetravalent element and X is a trivalent element and wherein the molar ratio X2O3:YO2 is greater than 0.02:1; (ii) treating the zeolitic material provided in (i) with a liquid solvent system thereby obtaining a zeolitic material having a molar ratio X2O3:YO2 of at most 0.02:1, and at least partially separating the zeolitic material from the liquid solvent system; (iii) treating the zeolitic material obtained from (ii) with a liquid aqueous system having a pH in the range of 5.5 to 8 and a temperature of at least 75° C.
Abstract:
A process for the post-treatment of a zeolitic material, the process comprising (i) providing a zeolitic material, wherein the framework structure of the zeolitic material comprises YO2 and X2O3, wherein Y is a tetravalent element and X is a trivalent element; (ii) subjecting the zeolitic material provided in (i) to a method comprising (a) treating the zeolitic material with an aqueous solution having a pH of at most 5, (b) treating the zeolitic material obtained from (a) with a liquid aqueous system having a pH in the range of 5.5 to 8 and a temperature of at least 75° C.; wherein in (ii) and after (b), the zeolitic material is optionally subjected to at least one further treatment according to (a) and/or at least one further treatment according to (b).
Abstract:
A process for the post-treatment of a zeolitic material, the process comprising (i) providing a zeolitic material, wherein the framework structure of the zeolitic material comprises YO2 and X2O3, wherein Y is a tetravalent element and X is a trivalent element; (ii) subjecting the zeolitic material provided in (i) to a method comprising (a) treating the zeolitic material with an aqueous solution having a pH of at most 5, (b) treating the zeolitic material obtained from (a) with a liquid aqueous system having a pH in the range of 5.5 to 8 and a temperature of at least 75° C.; wherein in (ii) and after (b), the zeolitic material is optionally subjected to at least one further treatment according to (a) and/or at least one further treatment according to (b).
Abstract translation:一种用于后处理沸石材料的方法,所述方法包括(i)提供沸石材料,其中沸石材料的骨架结构包含YO 2和X 2 O 3,其中Y是四价元素,X是三价元素; (ii)使(i)中提供的沸石材料的方法包括(a)用pH至多为5的水溶液处理沸石材料的方法,(b)用液体(a)处理从(a)得到的沸石材料 水系统,其pH在5.5至8范围内,温度至少为75℃; 其中在(ii)和(b)中,所述沸石材料任选地根据(a)和/或根据(b)的至少一种另外的处理进行至少一种另外的处理。
Abstract:
The present invention relates to a process for process for the preparation of a zeolitic material which process comprises (i) providing a boron-containing zeolitic material and (ii) deboronating the boron-containing zeolitic material by treating the boron-containing zeolitic material with a liquid solvent system thereby obtaining a deboronated zeolitic material, which liquid solvent system does not contain an inorganic or organic acid, or a salt thereof.
Abstract:
The present invention relates to an organotemplate-free synthetic process for the production of a zeolitic material having a CHA-type framework structure comprising YO2, X2O3, and optionally comprising Z2O5, wherein said process comprises the steps of: (1) providing a mixture comprising one or more sources for YO2, one or more sources for X2O3, and seed crystals having a CHA framework structure, wherein the CHA framework structure of the seed crystals comprises YO2, X2O3, and optionally comprises Z2O5; and (2) crystallizing the mixture obtained in step (1); wherein Y is a tetravalent element, X is a trivalent element, and Z is a pentavalent element, wherein optionally one or more sources for Z2O5 are further provided in step (1), and wherein if the CHA framework of the seed crystals does not contain Z2O5, the seed crystals then have a YO2:X2O3 molar ratio of 5 or greater than 5.
Abstract translation:本发明涉及一种用于生产具有包含YO 2,X 2 O 3和任选地包含Z 2 O 5的CHA型骨架结构的沸石材料的有机模板合成方法,其中所述方法包括以下步骤:(1)提供包含 YO2的一种或多种来源,X 2 O 3的一种或多种来源和具有CHA骨架结构的晶种,其中晶种的CHA骨架结构包含YO 2,X 2 O 3,并且任选包含Z 2 O 5; 和(2)使步骤(1)中获得的混合物结晶; 其中Y是四价元素,X是三价元素,Z是五价元素,其中在步骤(1)中还可以任选地提供一种或多种Z2O5源,并且其中如果晶种的CHA骨架不包含 Z2O5,然后晶种的YO 2:X 2 O 3摩尔比为5或大于5。
Abstract:
The present invention relates to a process for the preparation of a zeolitic material having a CHA-type framework structure comprising YO2 and X2O3, wherein said process comprises the steps of: (1) providing a mixture comprising one or more sources for YO2, one or more sources for X2O3, one or more tetraalkylammonium cation R1R2R3R4N+-containing compounds, and one or more tetraalkylammonium cation R5R6R7R8N+-containing compounds as structure directing agent; (2) crystallizing the mixture obtained in step (1) for obtaining a zeolitic material having a CHA-type framework structure; wherein Y is a tetravalent element and X is a trivalent element, wherein R1, R2, R3, R4, R5, R6, and R7 independently from one another stand for alkyl, and wherein R8 stands for cycloalkyl, as well as to zeolitic materials which may be obtained according to the inventive process and to their use.
Abstract:
A process for the post-treatment of a zeolitic material having a BEA framework structure, the process comprising (i) providing a zeolitic material having a BEA framework structure, wherein the framework structure of the zeolitic material comprises X2O3 and YO2, wherein Y is a tetravalent element and X is a trivalent element and wherein the molar ratio X2O3:YO2 is greater than 0.02:1; (ii) treating the zeolitic material provided in (i) with a liquid solvent system thereby obtaining a zeolitic material having a molar ratio X2O3:YO2 of at most 0.02:1, and at least partially separating the zeolitic material from the liquid solvent system; (iii) treating the zeolitic material obtained from (ii) with a liquid aqueous system having a pH in the range of 5.5 to 8 and a temperature of at least 75° C.
Abstract:
The present invention relates to a process for process for the preparation of a zeolitic material which process comprises (i) providing a boron-containing zeolitic material and (ii) deboronating the boron-containing zeolitic material by treating the boron-containing zeolitic material with a liquid solvent system thereby obtaining a deboronated zeolitic material, which liquid solvent system does not contain an inorganic or organic acid, or a salt thereof.
Abstract:
The present invention relates to a process for process for the preparation of a zeolitic material which process comprises (i) providing a boron-containing zeolitic material and (ii) deboronating the boron-containing zeolitic material by treating the boron-containing zeolitic material with a liquid solvent system thereby obtaining a deboronated zeolitic material, which liquid solvent system does not contain an inorganic or organic acid, or a salt thereof.
Abstract:
The present invention relates to an organotemplate-free synthetic process for the production of a zeolitic material having a CHA-type framework structure comprising YO2, X2O3, and optionally comprising Z2O5, wherein said process comprises the steps of: (1) providing a mixture comprising one or more sources for YO2, one or more sources for X2O3, and seed crystals having a CHA framework structure, wherein the CHA framework structure of the seed crystals comprises YO2, X2O3, and optionally comprises Z2O5; and (2) crystallizing the mixture obtained in step (1); wherein Y is a tetravalent element, X is a trivalent element, and Z is a pentavalent element, wherein optionally one or more sources for Z2O5 are further provided in step (1), and wherein if the CHA framework of the seed crystals does not contain Z2O5, the seed crystals then have a YO2:X2O3 molar ratio of 5 or greater than 5.
Abstract translation:本发明涉及一种用于生产具有包含YO 2,X 2 O 3和任选地包含Z 2 O 5的CHA型骨架结构的沸石材料的有机模板合成方法,其中所述方法包括以下步骤:(1)提供包含 YO2的一种或多种来源,X 2 O 3的一种或多种来源和具有CHA骨架结构的晶种,其中晶种的CHA骨架结构包含YO 2,X 2 O 3,并且任选包含Z 2 O 5; 和(2)使步骤(1)中获得的混合物结晶; 其中Y是四价元素,X是三价元素,Z是五价元素,其中在步骤(1)中还可以任选地提供一种或多种Z2O5源,并且其中如果晶种的CHA骨架不包含 Z2O5,然后晶种的YO 2:X 2 O 3摩尔比为5或大于5。