公开(公告)号:DE502006003014D1
公开(公告)日:2009-04-16
申请号:DE502006003014
申请日:2006-03-20
Applicant: BASF SE
Inventor: WEISS AXEL , BOTHE MARC , NOLTE RAINER , KLAUSMANN MATTHIAS , AMRHEIN PATRICK , LANDHERR KENNETH , WILDBURG GERALD
IPC: C08J3/12
Abstract: The present invention relates to the production of a polymer powder with improved powder properties, and to its use as impact modifier for rigid polyvinyl chloride (PVC) applications. The impact modifier is composed of emulsion polymer particles which have a core-shell structure, where the shell is composed of a hard polymer and the core is composed of a soft, crosslinked rubber polymer.
-
公开(公告)号:PT1863866E
公开(公告)日:2009-04-08
申请号:PT06725178
申请日:2006-03-20
Applicant: BASF SE
Inventor: AMRHEIN PATRICK , WEISS AXEL , BOTHE MARC , NOLTE RAINER , KLAUSMANN MATTHIAS , LANDHERR KENNETH , WILDBURG GERALD
IPC: C08J3/12
-
公开(公告)号:AT424432T
公开(公告)日:2009-03-15
申请号:AT06725178
申请日:2006-03-20
Applicant: BASF SE
Inventor: WEISS AXEL , BOTHE MARC , NOLTE RAINER , KLAUSMANN MATTHIAS , AMRHEIN PATRICK , LANDHERR KENNETH , WILDBURG GERALD
IPC: C08J3/12
Abstract: The present invention relates to the production of a polymer powder with improved powder properties, and to its use as impact modifier for rigid polyvinyl chloride (PVC) applications. The impact modifier is composed of emulsion polymer particles which have a core-shell structure, where the shell is composed of a hard polymer and the core is composed of a soft, crosslinked rubber polymer.
-
公开(公告)号:ES2320803T3
公开(公告)日:2009-05-28
申请号:ES06725178
申请日:2006-03-20
Applicant: BASF SE
Inventor: WEISS AXEL , BOTHE MARC , NOLTE RAINER , KLAUSMANN MATTHIAS , AMRHEIN PATRICK , LANDHERR KENNETH
IPC: C08J3/12
Abstract: Procedimiento de elaboración de polvo de polímero a partir de una disolución acuosa de polímero, caracterizado porque la dispersión acuosa de las partículas de polímero II se obtiene mediante polimerización acuosa por emulsión radicalmente inducida de al menos un monómero etilénicamente insaturado C en presencia de partículas de polímero I dispersamente distribuidas, a) teniendo el polímero del, al menos uno, monómero insaturado C una temperatura de transición vítrea > 60ºC, b) obteniéndose las partículas de polímero I dispersamente distribuidas mediante polimerización acuosa por emulsión radicalmente inducida de una mezcla de monómeros I, que consiste en del 98,0 al 99,9% en peso de al menos un monómero etilénicamente insaturado A, cuyo polímero tiene una temperatura de transición vítrea 90% en peso:
-
-
-