公开(公告)号:US20220251358A1
公开(公告)日:2022-08-11
申请号:US17618739
申请日:2020-06-15
Applicant: BOREALIS AG
Inventor: Johan Defoer , Marc Knaepen
Abstract: The present invention relates to a propylene copolymer composition comprising (A) from 50.0 to 95.0 wt %, based on the total amount of the propylene copolymer composition, of a heterophasic propylene copolymer having a matrix phase and an elastomeric phase dispersed in said matrix phase, wherein the matrix phase is a propylene random copolymer, the heterophasic propylene copolymer further having a melt flow rate MFR2 of 0.2 to 12.0 g/10 min, determined according to ISO 1133 at a temperature of 230° C. and a load of 2.16 kg, and a xylene cold solubles (XCS) fraction in the range of from 20.0 to 50.0 wt % based on the total amount of the heterophasic propylene copolymer (A), determined according to ISO 16152 at a temperature of 25° C., and (B) from 5.0 to 25.0 wt %, based on the total amount of the propylene copolymer composition, of a propylene based plastomer having a density in the range of from 845 to 870 kg/m3, determined according to ASTM D 1505 on compression moulded test specimens and a melt flow rate MFR2 of 1.0 to 30.0 g/10 min, determined according to ASTM D1238 at a temperature of 230° C. and a load of 2.16 kg, wherein the propylene copolymer composition has a tensile modulus of below 300 MPa, determined according to ISO 527-2, measured on injection moulded test specimens, and follows the following inequation: tensile modulus [MPa]
-
公开(公告)号:US12281220B2
公开(公告)日:2025-04-22
申请号:US17618739
申请日:2020-06-15
Applicant: BOREALIS AG
Inventor: Johan Defoer , Marc Knaepen
Abstract: The present invention relates to a propylene copolymer composition comprising (A) from 50.0 to 95.0 wt %, based on the total amount of the propylene copolymer composition, of a heterophasic propylene copolymer having a matrix phase and an elastomeric phase dispersed in said matrix phase, wherein the matrix phase is a propylene random copolymer, the heterophasic propylene copolymer further having a melt flow rate MFR2 of 0.2 to 12.0 g/10 min, determined according to ISO 1133 at a temperature of 230° C. and a load of 2.16 kg, and a xylene cold solubles (XCS) fraction in the range of from 20.0 to 50.0 wt % based on the total amount of the heterophasic propylene copolymer (A), determined according to ISO 16152 at a temperature of 25° C., and (B) from 5.0 to 25.0 wt %, based on the total amount of the propylene copolymer composition, of a propylene based plastomer having a density in the range of from 845 to 870 kg/m3, determined according to ASTM D 1505 on compression moulded test specimens and a melt flow rate MFR2 of 1.0 to 30.0 g/10 min, determined according to ASTM D1238 at a temperature of 230° C. and a load of 2.16 kg, wherein the propylene copolymer composition has a tensile modulus of below 300 MPa, determined according to ISO 527-2, measured on injection moulded test specimens, and follows the following inequation: tensile modulus [MPa]
-
公开(公告)号:US20220251357A1
公开(公告)日:2022-08-11
申请号:US17618571
申请日:2020-06-15
Applicant: Borealis AG
Inventor: Johan DeFoer , Marc Knaepen
Abstract: A propylene copolymer composition is provided, wherein the composition includes from 50.0 to 90.0 wt %, based on the total amount of the propylene copolymer composition, of a heterophasic propylene copolymer having a matrix phase and an elastomeric phase dispersed in said matrix phase, wherein the matrix phase is a propylene random copolymer.
The composition also includes from 5.0 to 25.0 wt %, based on the total amount of the propylene copolymer composition, of a propylene based plastomer from 5.0 to 25.0 wt %, based on the total amount of the propylene copolymer composition, of an ethylene based plastomer. An article comprising said propylene copolymer composition and the use of said propylene copolymer composition in a single ply roofing membrane is also provided.-
公开(公告)号:US20210024789A1
公开(公告)日:2021-01-28
申请号:US17012665
申请日:2020-09-04
Applicant: BOREALIS AG
Inventor: Tuan Anh Tran , Marc Knaepen
IPC: C09J123/08 , C08F210/02 , C08F8/50 , C08F10/02 , C08F210/16 , C08K5/00
Abstract: A process for increasing MFR2 of a polyethylene copolymer or an ethylene plastomer or elastomer comprising: (I) extruding a copolymer of polyethylene copolymer having a density of 910 to 970 kg/m3 and an MFR2 of 1 and 100 g/10 min or an ethylene plastomer or elastomer having a density of 855 to 910 kg/m3 and an MFR2 of 0.5 and 100 g/10 min in the presence of 0.1 to 2 wt % of a non-peroxide radical initiator so as to produce a polyethylene copolymer having an MFR2 of 200 g/10 min or more, or an ethylene plastomer or elastomer having a MFR2 of 200 g/10 min or more.
-
公开(公告)号:US12146047B2
公开(公告)日:2024-11-19
申请号:US17618571
申请日:2020-06-15
Applicant: Borealis AG
Inventor: Johan DeFoer , Marc Knaepen
Abstract: A propylene copolymer composition is provided, wherein the composition includes from 50.0 to 90.0 wt %, based on the total amount of the propylene copolymer composition, of a heterophasic propylene copolymer having a matrix phase and an elastomeric phase dispersed in said matrix phase, wherein the matrix phase is a propylene random copolymer.
The composition also includes from 5.0 to 25.0 wt %, based on the total amount of the propylene copolymer composition, of a propylene based plastomer from 5.0 to 25.0 wt %, based on the total amount of the propylene copolymer composition, of an ethylene based plastomer. An article comprising said propylene copolymer composition and the use of said propylene copolymer composition in a single ply roofing membrane is also provided.-
公开(公告)号:US10793753B2
公开(公告)日:2020-10-06
申请号:US16095421
申请日:2017-04-21
Applicant: BOREALIS AG
Inventor: Tuan Anh Tran , Marc Knaepen
IPC: C08F8/50 , C09J123/08 , C08F210/02 , C08F10/02 , C08F210/16 , C08K5/00 , C08L23/26
Abstract: A process for increasing MFR2 of a polyethylene copolymer or an ethylene plastomer or elastomer comprising: (I) extruding a copolymer of polyethylene copolymer having a density of 910 to 970 kg/m3 and an MFR2 of 1 and 100 g/10 min or an ethylene plastomer or elastomer having a density of 855 to 910 kg/m3 and an MFR2 of 0.5 and 100 g/10 min in the presence of 0.1 to 2 wt % of a non-peroxide radical initiator so as to produce a polyethylene copolymer having an MFR2 of 200 g/10 min or more, or an ethylene plastomer or elastomer having a MFR2 of 200 g/10 min or more.
-
公开(公告)号:US20190136100A1
公开(公告)日:2019-05-09
申请号:US16095421
申请日:2017-04-21
Applicant: BOREALIS AG
Inventor: Tuan Anh Tran , Marc Knaepen
IPC: C09J123/08 , C08F210/02 , C08F210/16 , C08K5/00
Abstract: A process for increasing MFR2 of a polyethylene copolymer or an ethylene plastomer or elastomer comprising: (I) extruding a copolymer of polyethylene copolymer having a density of 910 to 970 kg/m3 and an MFR2 of 1 and 100 g/10 min or an ethylene plastomer or elastomer having a density of 855 to 910 kg/m3 and an MFR2 of 0.5 and 100 g/10 min in the presence of 0.1 to 2 wt % of a non-peroxide radical initiator so as to produce a polyethylene copolymer having an MFR2 of 200 g/10 min or more, or an ethylene plastomer or elastomer having a MFR2 of 200 g/10 min or more.
-
-
-
-
-
-