公开(公告)号:BRPI0716232A2
公开(公告)日:2013-10-15
申请号:BRPI0716232
申请日:2007-08-02
Applicant: BRIDGESTONE CORP
Inventor: MUKAI UCHU , MISUMI KAZUHIKO , SHIMADA TAKASHI
Abstract: The present invention provides a rubber composite constituted of at least two layers of members comprising a rubber composition containing a diene base rubber cross-linked by sulfur, wherein a difference in a concentration of sulfur between adjacent members in the rubber composite described above is 1.5 part by mass or more based on 100 parts by mass of a rubber component in the rubber composition described above; zinc oxide is blended in an amount satisfying a condition shown in the following equation (I) based on 100 parts by mass of a rubber component in a low sulfur concentration rubber composition among the adjacent members, and an antioxidant and/or a naphthoic hydrazide compound are blended in an amount satisfying a condition shown in the following equation (II) based on 100 parts by mass of the rubber component in the low sulfur concentration rubber composition: blending amount parts by mass of zinc in the low sulfur concentration rubber composition > Sb × 1.3 + Sa - Sb × 0.3 (wherein Sa represents a blending amount (parts by mass) of sulfur in the high sulfur concentration rubber composition, and Sb represents a blending amount (parts by mass) of sulfur in the low sulfur concentration rubber composition) and blending amount mole of the antioxidant and / or the napthoic hydrazide compound in the low sulfur concentration rubber composition > 0.005 + Sa - Sb / 2000 (wherein Sa and Sb represent the same contents as described in the equation (I)); a rubber composite improved in a problem originating in a difference in a concentration of a blending agent, particularly sulfur between adjacent rubber compositions comprising a rubber composition cross-linked by sulfur without using new raw materials and members; and a tire prepared by using the same.
-
公开(公告)号:DE69817426T2
公开(公告)日:2004-06-24
申请号:DE69817426
申请日:1998-03-20
Applicant: BRIDGESTONE CORP , UBE INDUSTRIES
Inventor: MUKAI UCHU , OKAMOTO NAOMI
-
公开(公告)号:ES2437078T3
公开(公告)日:2014-01-08
申请号:ES07791856
申请日:2007-08-02
Applicant: BRIDGESTONE CORP
Inventor: MUKAI UCHU , MISUMI KAZUHIKO , SHIMADA TAKASHI
Abstract: Un material compuesto de caucho constituido por al menos dos capas de unos miembros que comprenden unacomposición de caucho que contiene un caucho a base de dieno reticulado con azufre, en donde la diferencia de laconcentración de azufre entre los miembros adyacentes del material compuesto de caucho descrito anteriormente es1,5 partes en masa o más, en base a 100 partes en masa del componente de caucho en la composición de cauchodescrita anteriormente; en donde se mezcla óxido de cinc en una cantidad que satisface la condición mostrada en lasiguiente ecuación (I), en base a 100 partes en masa del componente de caucho en la composición de caucho debaja concentración de azufre entre los miembros adyacentes; y en donde se mezcla un antioxidante y/o uncompuesto de hidracida naftoica en una cantidad que satisface la condición mostrada en la siguiente ecuación (II),en base a 100 partes en masa del componente de caucho en la composición de caucho de baja concentración deazufre: cantidad de mezcla (partes en masa) de óxido de cinc en la composición de caucho de baja concentración de azufre > Sb x 1,3 + (Sa - Sb) x 0,3 (I) (en donde Sa representa la cantidad de mezcla (partes en masa) de azufre en la composición de caucho de altaconcentración de azufre, y Sb representa la cantidad de mezcla (partes en masa) de azufre en la composición decaucho de baja concentración de azufre) y cantidad de mezcla (moles) del antioxidante y/o el compuesto de hidracida naftoica en la composición de caucho de baja concentración de azufre > 0,005 + (Sa - Sb) / 2.000 (II)(en donde Sa y Sb representan los mismos contenidos que se describen en la ecuación (I)).
-
4.
公开(公告)号:DE60238358D1
公开(公告)日:2010-12-30
申请号:DE60238358
申请日:2002-07-22
Applicant: BRIDGESTONE CORP
Inventor: YANAGISAWA KAZUHIRO , SOMENO KAZUAKI , MUKAI UCHU
-
公开(公告)号:DE60231682D1
公开(公告)日:2009-05-07
申请号:DE60231682
申请日:2002-07-22
Applicant: BRIDGESTONE CORP
Inventor: YANAGISAWA KAZUHIRO , SOMENO KAZUAKI , MUKAI UCHU
Abstract: A method for producing a natural rubber master batch, which comprises a step for mixing a natural rubber latex with an aqueous slurry having been dispersed with at least one filler selected from the group consisting of carbon black, silica and an inorganic filler represented by the following Formula I: nM •xSiOy•zH2O wherein M is at least one member selected from the group consisting of metals of aluminium, magnesium, titanium, calcium and zirconium, oxides of the preceding metals, hydroxides of the preceding metals, hydrates of the preceding oxides and hydroxides, and carbonates of the preceding metals; n is an integer of 1 to 5; x is an integer of 0 to 10; y is an integer of 2 to 5; and z is an integer of 0 to 10; wherein (i) the particle size distribution of the filler in the aqueous slurry is 25 mu m or less in terms of a volume average particle size (mv) and 30 mu m or less in terms of a 90 volume % particle size (D90), and (ii) a 24M4DBP absorption of dried filler recovered from the aqueous slurry is maintained at 93% or more of that of the filler before being dispersed into water.
-
公开(公告)号:ES2202742T3
公开(公告)日:2004-04-01
申请号:ES98302103
申请日:1998-03-20
Applicant: BRIDGESTONE CORP , UBE INDUSTRIES
Inventor: MUKAI UCHU , OKAMOTO NAOMI
-
公开(公告)号:DE69702687D1
公开(公告)日:2000-09-07
申请号:DE69702687
申请日:1997-05-15
Applicant: BRIDGESTONE CORP
Inventor: MUKAI UCHU
IPC: C08L21/00
-
公开(公告)号:DE69502577T2
公开(公告)日:1998-11-26
申请号:DE69502577
申请日:1995-11-30
Applicant: BRIDGESTONE CORP
Inventor: YOKOYAMA HIDEAKI , MUKAI UCHU
Abstract: A pneumatic tire (1) has a tread (6) of cap and base structure, in which a rubber composition comprising 2-50 parts by weight of a rubber-reinforcing thermoplastic resin containing not less than 10% by weight of a conjugated diene rubber component and the balance being a resin component having a glass transition temperature of 100-140 DEG C, based on 100 parts by weight of rubber ingredient, is used in a tread base rubber (5) of the tread, and has good chipping resistance, cut resistance and durability to heat build-up.
-
公开(公告)号:ES2354430T3
公开(公告)日:2011-03-14
申请号:ES05014138
申请日:2002-07-22
Applicant: BRIDGESTONE CORP
Inventor: YANAGISAWA KAZUHIRO , SOMENO KAZUAKI , MUKAI UCHU
IPC: B60C1/00 , C08C1/04 , C08C19/08 , C08J3/215 , C08J3/22 , C08K3/22 , C08K3/26 , C08K3/36 , C08K5/057 , C08K5/5415 , C08L7/00
Abstract: Un procedimiento para producir una mezcla madre de caucho natural que comprende una etapa para mezclar un látex de caucho natural con una suspensión acuosa que ha sido dispersada con al menos una carga seleccionada del grupo constituido por negro de carbón, sílice y una carga inorgánica representada por la siguiente fórmula I: nM 1 -xSiOy-zH2O (I) en la que M 1 es al menos un miembro seleccionado del grupo constituido por metales de aluminio, magnesio, titanio, calcio y zirconio; óxidos de los anteriores metales; hidróxidos de los anteriores metales; hidratos de los anteriores óxidos e hidróxidos, y carbonatos de los anteriores metales; n es un número entero de 1 a 5; x es un número entero de 0 a 10; y es un número entero de 2 a 5; y z es un número entero de 0 a 10; en el que (i) la distribución de tamaño de partícula de la carga en la suspensión acuosa es de 25 µm o menor en términos del tamaño medio de partícula del volumen (mv) y de 30 µm o menor en términos del tamaño de partícula del 90% del volumen (D90) y (ii) una absorción 24M4DBP de la carga seca recuperada de la suspensión acuosa medida de acuerdo con ISO 6894, se mantiene al 93% o más de la de la carga antes de ser dispersada en el agua.
-
公开(公告)号:ES2116687T3
公开(公告)日:1998-07-16
申请号:ES95308643
申请日:1995-11-30
Applicant: BRIDGESTONE CORP
Inventor: YOKOYAMA HIDEAKI , MUKAI UCHU
Abstract: A pneumatic tire (1) has a tread (6) of cap and base structure, in which a rubber composition comprising 2-50 parts by weight of a rubber-reinforcing thermoplastic resin containing not less than 10% by weight of a conjugated diene rubber component and the balance being a resin component having a glass transition temperature of 100-140 DEG C, based on 100 parts by weight of rubber ingredient, is used in a tread base rubber (5) of the tread, and has good chipping resistance, cut resistance and durability to heat build-up.
-
-
-
-
-
-
-
-
-