Abstract: PROBLEM TO BE SOLVED: To provide a method for producing a crystalline zeolite-based solid. SOLUTION: In the method for producing a crystalline solid comprising at least one zeolite-based material, the solid is crystallized from at least one precursor compound and the reaction discharge of the crystallization is fed directly to a drying stage. COPYRIGHT: (C)2011,JPO&INPIT
Abstract translation: 待解决的问题:提供一种生产结晶沸石基固体的方法。 解决方案:在制备包含至少一种沸石基材料的结晶固体的方法中,固体从至少一种前体化合物结晶,并将结晶的反应放出直接送入干燥阶段。 版权所有(C)2011,JPO&INPIT
-
公开(公告)号:JP2012006835A
公开(公告)日:2012-01-12
申请号:JP2011216608
申请日:2011-09-30
Applicant: Basf Se , ビーエーエスエフ ソシエタス・ヨーロピアBasf Se
Inventor: GROSCH GEORG HEINRICH , MUELLER ULRICH DR , WALCH ANDREAS , RIEBER NORBERT DR , HARDER WOLFGANG DR
IPC: C01B39/04 , B01J29/04 , B01J29/89 , B01J37/00 , B01J37/04 , B01J37/08 , C01B37/02 , C01B39/00 , C04B38/08 , C07D301/12
CPC classification number: B01J37/0018 , B01J29/04 , B01J29/89 , C04B38/08 , C04B2111/00129 , C07D301/12 , C04B35/01 , C04B38/0051 , C04B35/16 , C04B35/6325 , C04B2103/0093
Abstract: PROBLEM TO BE SOLVED: To provide a shaped body containing at least one porous oxidic material and having sufficient mechanical stability usable as a catalyst in a fixed bed.SOLUTION: The shaped body includes at least one porous oxidic material which can be obtained according to a method comprising the following steps: (I) adding a mixture containing at least one alcohol and water to a mixture containing the porous oxidic material or a mixture of two or more materials of the same type and (II) kneading, molding, drying and firing the mixture added in step (I).
Abstract translation: 要解决的问题:提供一种含有至少一种多孔氧化材料的成形体,并且在固定床中具有用作催化剂的足够的机械稳定性。 成型体包括至少一种多孔氧化材料,其可以根据包括以下步骤的方法获得:(I)将含有至少一种醇和水的混合物加入到含有多孔氧化物质的混合物或 两种或更多种相同类型的材料的混合物,和(II)在步骤(I)中混合,成型,干燥和烧制混合物。 版权所有(C)2012,JPO&INPIT
-