METHOD OF PRODUCING GLASS
    2.
    发明申请
    METHOD OF PRODUCING GLASS 审中-公开
    生产玻璃的方法

    公开(公告)号:WO2011152287A3

    公开(公告)日:2012-02-23

    申请号:PCT/JP2011062150

    申请日:2011-05-20

    CPC classification number: C03C11/005 C03C3/089

    Abstract: Provided a method of producing a glass having a silica skeleton with a phase-separated structure, particularly in the case of a phase-separated glass, by selectively removing a compositionally deviated layer on the surface of a phase-separated borosilicate glass. The method of producing a glass includes forming a glass body containing silicon oxide, boron oxide, and an alkali metal oxide; and bringing an alkaline aqueous solution having a viscosity of 5 mPa·s or more to 200 mPa·s or less into contact with a surface of the glass body.

    Abstract translation: 提供了通过选择性地除去相分离的硼硅酸盐玻璃的表面上的组成偏离层,制造具有相分离结构的二氧化硅骨架的玻璃的方法,特别是在相分离的玻璃的情况下。 制造玻璃的方法包括:形成含有氧化硅,氧化硼和碱金属氧化物的玻璃体; 并使粘度为5mPa·s以上至200mPa·s以下的碱性水溶液与玻璃体的表面接触。

    METHOD FOR MANUFACTURING OPTICAL MEMBER, OPTICAL MEMBER, AND IMAGE PICKUP APPARATUS
    3.
    发明申请
    METHOD FOR MANUFACTURING OPTICAL MEMBER, OPTICAL MEMBER, AND IMAGE PICKUP APPARATUS 审中-公开
    制造光学构件,光学构件和图像拾取装置的方法

    公开(公告)号:WO2013140717A2

    公开(公告)日:2013-09-26

    申请号:PCT/JP2013001109

    申请日:2013-02-26

    Applicant: CANON KK

    Abstract: To provide a method for manufacturing an optical member having a porous glass layer on a substrate, containing fewer voids, and undergoing less crystallization. A method for manufacturing an optical member having a porous glass layer 41 on a substrate 1 includes forming a glass powder layer 2 containing a plurality of glass powders on the substrate 1, fusing the glass powders in the glass powder layer 2 to form a mother glass layer 21 containing silicon and aluminum, causing phase separation of the mother glass layer 21 to form a phase-separated glass layer 31, and etching the phase-separated glass layer 31 to form a porous glass layer 41. The fusion index M and the ratio A of aluminum to silicon of the mother glass layer 21 in the forming of the mother glass layer 21 satisfy particular relations.

    Abstract translation: 为了提供一种在基板上制造具有多孔玻璃层的光学部件的方法,其包含更少的空隙,并且经历较少的结晶。 在基板1上制造具有多孔玻璃层41的光学部件的制造方法包括在基板1上形成含有多个玻璃粉末的玻璃粉末层2,将玻璃粉末层2中的玻璃粉末熔融而形成母玻璃 含有硅和铝的层21,引起母玻璃层21的相分离,形成相分离玻璃层31,并蚀刻相分离玻璃层31以形成多孔玻璃层41.熔融指数M和比例 在形成母玻璃层21时,母玻璃层21的铝与硅的A满足特定的关系。

    METHOD OF PRODUCING POROUS GLASS
    6.
    发明申请
    METHOD OF PRODUCING POROUS GLASS 审中-公开
    生产多孔玻璃的方法

    公开(公告)号:WO2011152289A3

    公开(公告)日:2012-04-12

    申请号:PCT/JP2011062152

    申请日:2011-05-20

    CPC classification number: C03C11/00 C03C3/089 C03C3/091 C03C11/005 C03C23/008

    Abstract: Provided is a method of producing porous glass having pores with a uniform pore diameter entirely, particularly in the case of phase-separated glass, including selectively removing a denatured layer formed on the surface of glass easily. The method of producing glass includes: forming phase-separated glass containing silicon oxide, boron oxide, and an alkali metal oxide; bringing an alkaline solution held by a porous supporting member into contact with the denatured layer formed on the surface of the phase-separated glass to remove the denatured layer; and immersing the phase-separated glass with the denatured layer removed therefrom in an acid solution to form pores in the phase-separated glass.

    Abstract translation: 本发明提供一种多孔玻璃的制造方法,特别是在相分离玻璃的情况下,特别是选择性地除去形成在玻璃表面的变性层的孔隙,其孔径均匀。 制造玻璃的方法包括:形成含有氧化硅,氧化硼和碱金属氧化物的相分离玻璃; 使由多孔支撑构件保持的碱性溶液与形成在相分离玻璃的表面上的变性层接触以除去变性层; 并将相分离的玻璃与其中除去的变性层浸入酸溶液中以在相分离的玻璃中形成孔。

    POROUS GLASS, METHOD FOR MANUFACTURING POROUS GLASS, OPTICAL MEMBER, AND IMAGE CAPTURE APPARATUS
    7.
    发明公开
    POROUS GLASS, METHOD FOR MANUFACTURING POROUS GLASS, OPTICAL MEMBER, AND IMAGE CAPTURE APPARATUS 有权
    多孔玻璃,法多孔玻璃,光学元件与成像设备的生产

    公开(公告)号:EP2625150A4

    公开(公告)日:2014-08-20

    申请号:EP11830334

    申请日:2011-09-21

    Applicant: CANON KK

    CPC classification number: C03C11/005 C03B32/00 G02B1/00

    Abstract: A porous glass having high strength and a low refractive index, an optical member by using the porous glass, and a method for manufacturing the porous glass are provided. A method for manufacturing a porous glass includes the steps of heat-treating a glass body, which can be phase-separated through heating and which is formed from a plurality of components, at a first temperature to effect the phase separation, heat-treating the glass body, which has been heat-treated at the first temperature, at a second temperature, higher than the first temperature, to effect the phase separation, and bringing the glass body, which has been heat-treated at the second temperature, into contact with an aqueous solution, wherein the total time of the heat treatment time at the first temperature and the heat treatment time at the second temperature is 7 hours or more.