STAIN-RESISTANT GLASS AND METHOD OF MAKING SAME
    1.
    发明申请
    STAIN-RESISTANT GLASS AND METHOD OF MAKING SAME 审中-公开
    防锈玻璃及其制造方法

    公开(公告)号:WO1995005348A1

    公开(公告)日:1995-02-23

    申请号:PCT/US1994009307

    申请日:1994-08-19

    CPC classification number: C03C23/00 C03C23/008

    Abstract: The present invention provides a stain-resistant glass and a method of making such a glass. In accordance with the method of the invention, SO3 is applied to the upper surface of a sheet of float glass in an amount sufficient to reduce staining of the glass. In a preferred embodiment, the oxygen-containing gas and SO2 gas are supplied in a lehr adjacent the float bath at a temperature of at least about 800 DEG F (about 425 DEG C). In one aspect of the invention, a hood (30) having a gas delivery system (40) is provided, with the hood defining a downwardly open enclosure and enclosing a portion of the delivery system. The hood is optimally disposed above a ribbon of float glass (25) in an annealing lehr (20) and the delivery system may include a sparge pipe for delivering either SO2 or SO3 gas to the hood.

    Abstract translation: 本发明提供一种防污玻璃及其制造方法。 根据本发明的方法,将SO 3以足以减少玻璃污染的量施加到浮法玻璃片的上表面。 在一个优选的实施方案中,含氧气体和SO 2气体在至少约800°F(约425℃)的温度下在与浮液浴相邻的退火炉中供应。 在本发明的一个方面,提供了一种具有气体输送系统(40)的罩(30),其中罩罩限定向下开口的外壳并且包围输送系统的一部分。 发动机罩优选地设置在退火炉(20)中的浮法玻璃带(25)之上,并且输送系统可以包括用于将SO 2或SO 3气体输送到发动机罩的喷射管。

    STAIN-RESISTANT GLASS AND METHOD OF MAKING SAME
    2.
    发明公开
    STAIN-RESISTANT GLASS AND METHOD OF MAKING SAME 失效
    START耐用于其生产的玻璃和方法

    公开(公告)号:EP0714380A1

    公开(公告)日:1996-06-05

    申请号:EP94925285.0

    申请日:1994-08-19

    CPC classification number: C03C23/00 C03C23/008

    Abstract: The present invention provides a stain-resistant glass and a method of making such a glass. In accordance with the method of the invention, SO3 is applied to the upper surface of a sheet of float glass in an amount sufficient to reduce staining of the glass. In a preferred embodiment, the oxygen-containing gas and SO2 gas are supplied in a lehr adjacent the float bath at a temperature of at least about 800 DEG F (about 425 DEG C). In one aspect of the invention, a hood (30) having a gas delivery system (40) is provided, with the hood defining a downwardly open enclosure and enclosing a portion of the delivery system. The hood is optimally disposed above a ribbon of float glass (25) in an annealing lehr (20) and the delivery system may include a sparge pipe for delivering either SO2 or SO3 gas to the hood.

    STAIN-RESISTANT GLASS AND METHOD OF MAKING SAME
    3.
    发明授权
    STAIN-RESISTANT GLASS AND METHOD OF MAKING SAME 失效
    START耐用于其生产的玻璃和方法

    公开(公告)号:EP0714380B1

    公开(公告)日:1997-04-09

    申请号:EP94925285.2

    申请日:1994-08-19

    CPC classification number: C03C23/00 C03C23/008

    Abstract: The present invention provides a stain-resistant glass and a method of making such a glass. In accordance with the method of the invention, SO3 is applied to the upper surface of a sheet of float glass in an amount sufficient to reduce staining of the glass. In a preferred embodiment, the oxygen-containing gas and SO2 gas are supplied in a lehr adjacent the float bath at a temperature of at least about 800 °F (about 425 °C). In one aspect of the invention, a hood (30) having a gas delivery system (40) is provided, with the hood defining a downwardly open enclosure and enclosing a portion of the delivery system. The hood is optimally disposed above a ribbon of float glass (25) in an annealing lehr (20) and the delivery system may include a sparge pipe for delivering either SO2 or SO3 gas to the hood.

Patent Agency Ranking