公开(公告)号:JPH0225719B2
公开(公告)日:1990-06-05
申请号:JP4024181
申请日:1981-03-19
Applicant: COMP GENERALE ELECTRICITE
Inventor: JERAARU DESUPURANSHU , JATSUKU RUBUUKU
-
公开(公告)号:JPS5932424B2
公开(公告)日:1984-08-08
申请号:JP8667376
申请日:1976-07-22
Applicant: Comp Generale Electricite
Inventor: ZERAARU DESUPURANSHU , IBON RAZENETSUKU , JATSUKU RUBUUKU
IPC: C04B35/113 , C04B35/64 , C04B37/00 , H01M2/16 , H01M10/39
CPC classification number: C04B35/113 , C04B35/64 , C04B37/005 , C04B37/026 , C04B2235/6562 , C04B2235/658 , C04B2237/064 , C04B2237/12 , C04B2237/343 , C04B2237/406 , C04B2237/555 , C04B2237/765 , H01M10/3909
Abstract: The alpha alumina part is heated to between 1400 DEG C and 1600 DEG C for 10 to 20 hours in a mass of alkaline carbonate or aluminate. It is then disposed in contact with a blank of the alkaline beta alumina part in a sintering enclosure suitable for establishing an atmosphere which is rich in alkaline metal and in heating this enclosure to between 1600 DEG C and 1700 DEG C for between 30 minutes and 4 hours, so as to sinter the alkaline beta alumina part while effecting the connection thereof to the alpha alumina part. The invention is used in manufacturing sodium-sulphur type electric cells.
-