公开(公告)号:AU6808590A
公开(公告)日:1991-06-27
申请号:AU6808590
申请日:1990-12-14
Applicant: CORNING INC
Inventor: BACKER MARCELLA ROSE , BLANKENSHIP MICHAEL GREGG , CAVENDER RALSTON , JONG BERNARD J DE , ELDER MELANIE L , GLAESEMANN GREGORY SCOTT , JONES PETER CHRISTOPHER , MURPHY JAMES ANTHONY
IPC: C03B37/018 , C03B37/014 , C03C13/04 , G02B6/00 , G02B6/036 , G02B6/16
Abstract: An optical waveguide fiber with a fatigue resistant TiO2-SiO2 outer cladding including a cylindrical outermost layer with TiO2 concentration greater than 10.5 wt.% and thickness less than 3 mu m. The fiber may include a two layer outer cladding with higher TiO2 concentration in the outer layer. The outer cladding may ionclude a plurality of inhomogeneities dispersed in a TiO2-SiO2 matrix. A method of making an optical waveguide fiber with a fatigue resistant TiO2-SiO2 outer cladding, and a substantially glass blank for drawing into such fiber, wherein a glass soot TiO2-SiO2 outermost layer, with an initial TiO2 concentration greater than 10.5 wt.%, is deposited on a preform, and the preform is exposed to an atmosphere of chlorine at a high temperature, and the resulting TiO2 concentration in the outermost layer of the TiO2-SiO2 outer cladding of the substantially glass blank is less than the initial TiO2 concentration. In the glass blank form, the outermost layer includes a substantial volume percentage of crystalline phases and in the fiber form, the outermost layer includes inhomogeneities.
-
公开(公告)号:CA2030748C
公开(公告)日:2000-08-15
申请号:CA2030748
申请日:1990-11-23
Applicant: CORNING INC
Inventor: BACKER MARCELLA ROSE , BLANKENSHIP MICHAEL GREGG , CAVENDER RALSTON , DE JONG BERNARD J , ELDER MELANIE L , GLAESEMANN GREGORY SCOTT , JONES PETER CHRISTOPHER , MURPHY JAMES ANTHONY
IPC: C03B37/018 , C03B37/014 , C03C13/04 , G02B6/00 , G02B6/036 , C03B20/00 , C03B37/027 , G02B6/22
Abstract: An optical waveguide fiber with a fatigue resistant TiO2-SiO2 outer cladding including a cylindrical outermost layer with TiO2 concentration greater than 10.5 wt.% and thickness less than 3 .mu.m. The fiber may include a two layer outer cladding with higher TiO2 concentration in the outer layer. The outer cladding may ionclude a plurality of inhomogeneities dispersed in a TiO2-SiO2 matrix. A method of making an optical waveguide fiber with a fatigue resistant TiO2-SiO2 outer cladding, and a substantially glass blank for drawing into such fiber, wherein a glass soot TiO2-SiO2 outermost layer, with an initial TiO2 concentration greater than 10.5 wt.%, is deposited on a preform, and the preform is exposed to an atmosphere of chlorine at a high temperature, and the resulting TiO2 concentration in the outermost layer of the TiO2-SiO2 outer cladding of the substantially glass blank is less than the initial TiO2 concentration. In the glass blank form, the outermost layer includes a substantial volume percentage of crystalline phases and in the fiber form, the outermost layer includes inhomogeneities.
-
公开(公告)号:DE69022022T2
公开(公告)日:1996-06-13
申请号:DE69022022
申请日:1990-11-27
Applicant: CORNING INC
Inventor: BACKER MARCELLA ROSE , BLANKENSHIP MICHAEL GREGG , CAVENDER RALSTON , DE JONG BERNARD J , ELDER MELANIE L , GLAESEMANN GREGORY SCOTT , JONES PETER CHRISTOPHER , MURPHY JAMES ANTHONY
IPC: C03B37/018 , C03B37/014 , C03C13/04 , G02B6/00 , G02B6/036 , G02B6/16 , G02B6/22
Abstract: An optical waveguide fiber with a fatigue resistant TiO2-SiO2 outer cladding including a cylindrical outermost layer with TiO2 concentration greater than 10.5 wt.% and thickness less than 3 mu m. The fiber may include a two layer outer cladding with higher TiO2 concentration in the outer layer. The outer cladding may ionclude a plurality of inhomogeneities dispersed in a TiO2-SiO2 matrix. A method of making an optical waveguide fiber with a fatigue resistant TiO2-SiO2 outer cladding, and a substantially glass blank for drawing into such fiber, wherein a glass soot TiO2-SiO2 outermost layer, with an initial TiO2 concentration greater than 10.5 wt.%, is deposited on a preform, and the preform is exposed to an atmosphere of chlorine at a high temperature, and the resulting TiO2 concentration in the outermost layer of the TiO2-SiO2 outer cladding of the substantially glass blank is less than the initial TiO2 concentration. In the glass blank form, the outermost layer includes a substantial volume percentage of crystalline phases and in the fiber form, the outermost layer includes inhomogeneities.
-
公开(公告)号:DE69022022D1
公开(公告)日:1995-10-05
申请号:DE69022022
申请日:1990-11-27
Applicant: CORNING INC
Inventor: BACKER MARCELLA ROSE , BLANKENSHIP MICHAEL GREGG , CAVENDER RALSTON , DE JONG BERNARD J , ELDER MELANIE L , GLAESEMANN GREGORY SCOTT , JONES PETER CHRISTOPHER , MURPHY JAMES ANTHONY
IPC: C03B37/018 , C03B37/014 , C03C13/04 , G02B6/00 , G02B6/036 , G02B6/16 , G02B6/22
Abstract: An optical waveguide fiber with a fatigue resistant TiO2-SiO2 outer cladding including a cylindrical outermost layer with TiO2 concentration greater than 10.5 wt.% and thickness less than 3 mu m. The fiber may include a two layer outer cladding with higher TiO2 concentration in the outer layer. The outer cladding may ionclude a plurality of inhomogeneities dispersed in a TiO2-SiO2 matrix. A method of making an optical waveguide fiber with a fatigue resistant TiO2-SiO2 outer cladding, and a substantially glass blank for drawing into such fiber, wherein a glass soot TiO2-SiO2 outermost layer, with an initial TiO2 concentration greater than 10.5 wt.%, is deposited on a preform, and the preform is exposed to an atmosphere of chlorine at a high temperature, and the resulting TiO2 concentration in the outermost layer of the TiO2-SiO2 outer cladding of the substantially glass blank is less than the initial TiO2 concentration. In the glass blank form, the outermost layer includes a substantial volume percentage of crystalline phases and in the fiber form, the outermost layer includes inhomogeneities.
-
-
-