公开(公告)号:US09475723B2
公开(公告)日:2016-10-25
申请号:US14836561
申请日:2015-08-26
Applicant: CORNING INCORPORATED
Inventor: Kristen Marie Horn , David Myron Lineman , Kevin Thomas Morris , Wenchao Wang , Kim E. Womer
IPC: C03B40/00 , C03B11/00 , C03B23/035 , C23C8/10 , C03B40/02 , C03B23/025 , C03B23/03 , C03B23/00 , C03B23/023
CPC classification number: C03B40/00 , C03B11/00 , C03B23/002 , C03B23/023 , C03B23/0252 , C03B23/0302 , C03B23/0355 , C03B23/0357 , C03B40/02 , C23C8/10 , Y02P40/57
Abstract: A mold for shaping glass can be made by a method that includes providing a mold body having a shaping surface comprising at least about 90% nickel and modifying the composition of the shaping surface of the mold body by exposing the shaping surface to an oxidizing heat treatment. The oxidizing heat treatment may include a ramping heat treatment, a fixed heat treatment, or both the ramping heat treatment and the fixed heat treatment. The ramping heat treatment may include increasing a heating temperature at a rate from about 20° C./hour to about 500° C./hour to a temperature from about 700° C. to about 1000° C. The fixed heat treatment may include holding the heating temperature from about 700° C. to about 1000° C. for a holding time of at least about 5 minutes.
-
2.
公开(公告)号:US20150360993A1
公开(公告)日:2015-12-17
申请号:US14836561
申请日:2015-08-26
Applicant: CORNING INCORPORATED
Inventor: Kristen Marie Horn , David Myron Lineman , Kevin Thomas Morris , Wenchao Wang , Kim E. Womer
IPC: C03B40/00 , C23C8/10 , C03B23/035 , C03B23/025 , C03B23/00 , C03B23/023
CPC classification number: C03B40/00 , C03B11/00 , C03B23/002 , C03B23/023 , C03B23/0252 , C03B23/0302 , C03B23/0355 , C03B23/0357 , C03B40/02 , C23C8/10 , Y02P40/57
Abstract: A mold for shaping glass can be made by a method that includes providing a mold body having a shaping surface comprising at least about 90% nickel and modifying the composition of the shaping surface of the mold body by exposing the shaping surface to an oxidizing heat treatment. The oxidizing heat treatment may include a ramping heat treatment, a fixed heat treatment, or both the ramping heat treatment and the fixed heat treatment. The ramping heat treatment may include increasing a heating temperature at a rate from about 20° C./hour to about 500° C./hour to a temperature from about 700° C. to about 1000° C. The fixed heat treatment may include holding the heating temperature from about 700° C. to about 1000° C. for a holding time of at least about 5 minutes.
Abstract translation: 用于成形玻璃的模具可以通过包括提供具有包括至少约90%的镍的成形表面的模具主体并通过将成形表面暴露于氧化热处理来改变模制体的成形表面的组成的方法来制备 。 氧化热处理可以包括斜坡热处理,固定热处理,或斜坡加热处理和固定热处理两者。 升温热处理可以包括以约20℃/小时至约500℃/小时的速度升高加热温度至约700℃至约1000℃的温度。固定热处理可包括 将加热温度保持在约700℃至约1000℃,保持时间至少约5分钟。
-
3.
公开(公告)号:US09145323B2
公开(公告)日:2015-09-29
申请号:US14158262
申请日:2014-01-17
Applicant: Corning Incorporated
Inventor: Kristen Marie Horn , David Myron Lineman , Kevin Thomas Morris , Wenchao Wang , Kim E Womer
IPC: C03B11/08 , C03B11/00 , C03B23/035 , C23C8/10 , C03B40/02 , C03B23/025 , C03B23/03
CPC classification number: C03B40/00 , C03B11/00 , C03B23/002 , C03B23/023 , C03B23/0252 , C03B23/0302 , C03B23/0355 , C03B23/0357 , C03B40/02 , C23C8/10 , Y02P40/57
Abstract: A mold for shaping glass can be made by a method that includes providing a mold body having a shaping surface comprising at least about 90% nickel and modifying the composition of the shaping surface of the mold body by exposing the shaping surface to an oxidizing heat treatment. The oxidizing heat treatment may include a ramping heat treatment, a fixed heat treatment, or both the ramping heat treatment and the fixed heat treatment. The ramping heat treatment may include increasing a heating temperature at a rate from about 20° C./hour to about 500° C./hour to a temperature from about 700° C. to about 1000° C. The fixed heat treatment may include holding the heating temperature from about 700° C. to about 1000° C. for a holding time of at least about 5 minutes.
Abstract translation: 用于成形玻璃的模具可以通过包括提供具有包括至少约90%的镍的成形表面的模具主体并通过将成形表面暴露于氧化热处理来改变模制体的成形表面的组成的方法来制备 。 氧化热处理可以包括斜坡热处理,固定热处理,或斜坡加热处理和固定热处理两者。 升温热处理可以包括以约20℃/小时至约500℃/小时的速度升高加热温度至约700℃至约1000℃的温度。固定热处理可包括 将加热温度保持在约700℃至约1000℃,保持时间至少约5分钟。
-
公开(公告)号:US09902641B2
公开(公告)日:2018-02-27
申请号:US15071889
申请日:2016-03-16
Applicant: CORNING INCORPORATED
Inventor: Jill Marie Hall , Nicholas Scott Ryan , Wenchao Wang , Kim E Womer
IPC: C03B23/035 , C03B23/023 , C23C8/10 , C22C19/03 , C22F1/10 , C03B11/08
CPC classification number: C03B23/0357 , C03B11/086 , C03B23/0235 , C03B2215/03 , C03B2215/11 , C03B2215/20 , C03B2215/32 , C22C19/03 , C22F1/10 , C23C8/10 , Y02P40/57
Abstract: A mold for shaping glass-based material can include a mold body having a surface, wherein at least a portion of the mold body near the surface comprises at least about 90% by weight nickel and from about 0.2% to about 0.35% by weight manganese; and a nickel oxide layer on the surface of the mold body. The nickel oxide layer has first and second opposing surfaces wherein the first surface of the nickel oxide layer contacts and faces the surface of the mold body and the second surface of the nickel oxide layer includes a plurality of grains. The plurality of grains has an average grain size of about 150 μm or less.
-
公开(公告)号:US20150041435A1
公开(公告)日:2015-02-12
申请号:US14446939
申请日:2014-07-30
Applicant: CORNING INCORPORATED
Inventor: Jianqiang Gu , Jean-Marc Martin Gerard Jouanno , William Brashear Mattingly, III , Wenchao Wang , Yoshiki Yamashita , Rui Zhang
CPC classification number: C03B23/0066 , B65D85/48 , B65G49/062 , C03B23/023 , C03C15/00 , C03C17/002 , C03C21/002 , C03C2218/31 , F26B5/14
Abstract: Methods provide for post processing at least one flexible glass sheet with the step of providing the glass sheet with an initial shape. The method then further includes the step of flexing the glass sheet into a secondary shape from the initial shape. The method then further includes the step of post processing the glass sheet while biasing the glass sheet into the secondary shape. The method then still further includes the step of releasing the glass sheet to at least partially return to the initial shape.
Abstract translation: 方法提供对至少一个柔性玻璃板的后处理,其中提供玻璃板具有初始形状的步骤。 该方法还包括从初始形状将玻璃板弯曲成二次形状的步骤。 该方法还包括在将玻璃板偏压成二次形状的同时对玻璃板进行后处理的步骤。 该方法然后还包括释放玻璃板以至少部分地恢复到初始形状的步骤。
-
公开(公告)号:US20140331718A1
公开(公告)日:2014-11-13
申请号:US14444482
申请日:2014-07-28
Applicant: CORNING INCORPORATED
Inventor: David Myron Lineman , Wenchao Wang , Randy Dean Ziegenhagen
CPC classification number: C04B37/026 , C03B5/43 , C03B7/02 , C03B7/04 , C04B37/025 , C04B2235/656 , C04B2235/6567 , C04B2237/068 , C04B2237/125 , C04B2237/343 , C04B2237/408 , C04B2237/52 , C04B2237/61 , C04B2237/62 , Y10S228/903 , Y10T156/10 , Y10T428/24339 , Y10T428/249953 , Y10T428/252
Abstract: A method is disclosed for mechanically bonding a metal component to a ceramic material, comprising providing a metal component comprising an anchor material attached to at least a first portion of one surface of the metal component; providing a ceramic material having a first surface and a second surface, wherein the ceramic material defines at least one conduit extending from the first surface to the second surface, wherein the at least one conduit has a first open end defined by the first surface, a second open end defined by the second surface, a continuous sidewall and a cross sectional area; positioning the ceramic material such that at least a portion of the at least one conduit is in overlying registration with at least a portion of the anchor material; and applying a bonding agent into at least a portion of the at least one conduit.
Abstract translation: 公开了一种用于将金属组分机械地结合到陶瓷材料的方法,包括提供金属组分,所述金属组分包含连接到所述金属组分的一个表面的至少第一部分的锚固材料; 提供具有第一表面和第二表面的陶瓷材料,其中所述陶瓷材料限定从所述第一表面延伸到所述第二表面的至少一个导管,其中所述至少一个导管具有由所述第一表面限定的第一开口端, 由第二表面限定的第二开口端,连续侧壁和横截面积; 定位陶瓷材料,使得至少一个导管的至少一部分与锚定材料的至少一部分重叠对齐; 以及将粘合剂施加到所述至少一个导管的至少一部分中。
-
7.
公开(公告)号:US09266768B2
公开(公告)日:2016-02-23
申请号:US14158242
申请日:2014-01-17
Applicant: CORNING INCORPORATED
Inventor: Kristen Marie Horn , David Myron Lineman , Kevin Thomas Morris , Wenchao Wang
IPC: B32B9/00 , C03B40/00 , C03B11/00 , C03B23/035 , C23C8/10 , C03B40/02 , C03B23/025 , C03B23/03 , C03B23/00 , C03B23/023
CPC classification number: C03B40/00 , C03B11/00 , C03B23/002 , C03B23/023 , C03B23/0252 , C03B23/0302 , C03B23/0355 , C03B23/0357 , C03B40/02 , C23C8/10 , Y02P40/57
Abstract: The present disclosure relates to high purity nickel molds for use in forming three dimensional glass substrates, along with methods of making three dimensional glass substrates. The mold compositions minimize imperfections in the formed glass substrates providing optical quality shaped glass articles for use in electronics applications.
Abstract translation: 本公开涉及用于形成三维玻璃基板的高纯度镍模具以及制造三维玻璃基板的方法。 模具组合物使形成的玻璃基底中的缺陷最小化,提供用于电子应用的光学质量成形玻璃制品。
-
8.
公开(公告)号:US20240239702A1
公开(公告)日:2024-07-18
申请号:US18559683
申请日:2022-06-07
Applicant: CORNING INCORPORATED
Inventor: Tomohiro Aburada , Anmol Agrawal , Matthew John Cempa , Miki Eugene Kunitake , Francisco Javier Moraga , Shyam Prasad Mudiraj , Wenchao Wang
CPC classification number: C03B35/184 , C03B13/04
Abstract: An apparatus and method for manufacturing glass include a heat extractor configured to extract heat from molten glass. The heat extractor includes a first conduit and at least one second conduit which may include a plurality of second conduits circumferentially surrounding the first conduit. The first conduit and the at least one second conduit are configured to flow a fluid therethrough.
-
公开(公告)号:US09284211B2
公开(公告)日:2016-03-15
申请号:US14446939
申请日:2014-07-30
Applicant: CORNING INCORPORATED
Inventor: Jianqiang Gu , Jean-Marc Martin Gerard Jouanno , William Brashear Mattingly, III , Wenchao Wang , Yoshiki Yamashita , Rui Zhang
IPC: B44C1/22 , C03B23/00 , C03B23/023 , C03C15/00 , C03C17/00 , C03C21/00 , F26B5/14 , B65G49/06 , B65D85/48
CPC classification number: C03B23/0066 , B65D85/48 , B65G49/062 , C03B23/023 , C03C15/00 , C03C17/002 , C03C21/002 , C03C2218/31 , F26B5/14
Abstract: Methods provide for post processing at least one flexible glass sheet with the step of providing the glass sheet with an initial shape. The method then further includes the step of flexing the glass sheet into a secondary shape from the initial shape. The method then further includes the step of post processing the glass sheet while biasing the glass sheet into the secondary shape. The method then still further includes the step of releasing the glass sheet to at least partially return to the initial shape.
Abstract translation: 方法提供对至少一个柔性玻璃板的后处理,其中提供玻璃板具有初始形状的步骤。 该方法还包括从初始形状将玻璃板弯曲成二次形状的步骤。 该方法还包括在将玻璃板偏压成二次形状的同时对玻璃板进行后处理的步骤。 该方法然后还包括释放玻璃板以至少部分地恢复到初始形状的步骤。
-
10.
公开(公告)号:US20140202211A1
公开(公告)日:2014-07-24
申请号:US14158262
申请日:2014-01-17
Applicant: Corning Incorporated
Inventor: Kristen Marie Horn , David Myron Lineman , Kevin Thomas Morris , Wenchao Wang , Kim E. Womer
IPC: C03B11/08 , C03B23/023
CPC classification number: C03B40/00 , C03B11/00 , C03B23/002 , C03B23/023 , C03B23/0252 , C03B23/0302 , C03B23/0355 , C03B23/0357 , C03B40/02 , C23C8/10 , Y02P40/57
Abstract: A mold for shaping glass can be made by a method that includes providing a mold body having a shaping surface comprising at least about 90% nickel and modifying the composition of the shaping surface of the mold body by exposing the shaping surface to an oxidizing heat treatment. The oxidizing heat treatment may include a ramping heat treatment, a fixed heat treatment, or both the ramping heat treatment and the fixed heat treatment. The ramping heat treatment may include increasing a heating temperature at a rate from about 20° C./hour to about 500° C./hour to a temperature from about 700° C. to about 1000° C. The fixed heat treatment may include holding the heating temperature from about 700° C. to about 1000° C. for a holding time of at least about 5 minutes.
Abstract translation: 用于成形玻璃的模具可以通过包括提供具有包括至少约90%的镍的成形表面的模具主体并通过将成形表面暴露于氧化热处理来改变模制体的成形表面的组成的方法来制备 。 氧化热处理可以包括斜坡加热处理,固定热处理或斜坡热处理和固定热处理两者。 升温热处理可以包括以约20℃/小时至约500℃/小时的速度升高加热温度至约700℃至约1000℃的温度。固定热处理可包括 将加热温度保持在约700℃至约1000℃,保持时间至少约5分钟。
-
-
-
-
-
-
-
-
-