Abstract:
An aqueous ionomer dispersion, and method of manufacturing thereof, comprising an ionomer composition and water, wherein the ionomer composition comprises: a) at least 20 wt.%, based on the total weight percent of the ionomer composition, of an ionomer; and b) up to 80 wt.%, based on the total weight percent of the ionomer composition, of a polyolefin.
Abstract:
The invention provides a composition comprising the following: A) a first polymer composition comprising an anhydride functionalized ethylene-based polymer, and optionally, an ethylene-based polymer; B) a filler; and wherein the anhydride functionalized ethylene-based polymer has a density from 0.855 g/cc to 0.900 g/cc and a melt viscosity, at 177°C, from 1000 to 50,000 cP.
Abstract:
A composition comprising from 10 wt% to 90 wt% of an ethylene component including at least one ethylene based polymer having an ethylene content of at least 50.0 wt%, a melt index from 0.1 g/10 min to 100.0 g/10 min, and a density from 0.935 g/cm 3 to 0.965 g/cm 3 ; from 10 wt% to 90 wt% of a propylene component including at least one propylene based polymer having a propylene content of at least 50.0 wt% and a melt flow rate from 0.5 g/10 min to 200.0 g/10 min; and from 1 wt% to 20 wt% of a composite component including a specified block composite, derived from at least ethylene and an alpha-olefin.
Abstract translation:包含10重量%至90重量%的包含至少一种乙烯含量为至少50.0重量%,熔体指数为0.1克/ 10分钟至100.0克/ 10分钟的乙烯基聚合物的乙烯组分的组合物,以及 密度为0.935g / cm 3至0.965g / cm 3; 10重量%至90重量%的丙烯组分,其包含至少一种丙烯含量为至少50.0重量%和熔体流动速率为0.5g / 10分钟至200.0g / 10分钟的丙烯基聚合物; 和1重量%至20重量%的包含至少乙烯和α-烯烃的特定嵌段复合材料的复合组分。
Abstract:
A composition comprising from 10 wt% to 86 wt% of an ethylene component including at least one ethylene based polymer having an ethylene content of at least 50.0 wt%, a melt index from 0.1 g/10 min to 100.0 g/10 min, and a density from 0.935 g/cm 3 to 0.965 g/cm 3 ; from 10 wt% to 86 wt% of a propylene component including at least one propylene based polymer having a propylene content of at least 50.0 wt% and a melt flow rate from 0.5 g/10 min to 200.0 g/10 min; from 2 wt% to 22 wt% of an octene component including at least one octene based polymer having an octene content of at least 80 wt%; and from 2 wt% to 20 wt% of a composite component including at least one selected from the group of a crystalline block composite and a specified block composite, derived from at least ethylene and an alpha-olefin.
Abstract translation:包含10重量%至86重量%的包含至少一种乙烯含量为至少50.0重量%,熔体指数为0.1g / 10min至100.0g / 10min的乙烯基聚合物的乙烯组分的组合物,以及 密度为0.935g / cm 3至0.965g / cm 3; 10重量%至86重量%的丙烯组分,其包含至少一种丙烯含量为至少50.0重量%和熔体流动速率为0.5g / 10min至200.0g / 10min的丙烯基聚合物; 2重量%至22重量%的包含至少一种辛烯含量为至少80重量%的辛烯基聚合物的辛烯组分; 和2重量%至20重量%的复合组分,其包含至少一种选自至少一种来自至少乙烯和α-烯烃的结晶嵌段复合材料和特定嵌段复合材料。
Abstract:
A functionalized ethylene-based polymer dissolved in an appropriate solvent and applied to a nonpolar surface can change the surface polarity/characteristics of the nonpolar surface. This change to the surface polarity/characteristics of the nonpolar surface allows adhesion of materials, such as paint, to surfaces such as polypropylene, polyethylene and polyolefin elastomers.
Abstract:
A composition comprising from 10 wt% to 90 wt% of an ethylene component including at least one ethylene based polymer having an ethylene content of at least 50.0 wt%, a melt index from 0.1 g/10 min to 100.0 g/10 min, and a density from 0.935 g/cm3 to 0.965 g/cm3; from 10 wt% to 90 wt% of a propylene component including at least one propylene based polymer having a propylene content of at least 50.0 wt% and a melt flow rate from 0.5 g/10 min to 200.0 g/10 min; and from 1 wt% to 20 wt% of a composite component including a specified block composite, derived from at least ethylene and an alpha-olefin.
Abstract:
The invention provides a composition comprising the following: A) a first polymer composition comprising an anhydride functionalized ethylene-based polymer, and optionally, an ethylene-based polymer; B) a filler; and wherein the anhydride functionalized ethylene-based polymer has a density from 0.855 g/cc to 0.900 g/cc and a melt viscosity, at 177° C., from 1000 to 50,000 cP.
Abstract:
A composition comprising from 10 wt % to 86 wt % of an ethylene component including at least one ethylene based polymer having an ethylene content of at least 50.0 wt %, a melt index from 0.1 g/10 min to 100.0 g/10 min, and a density from 0.935 g/cm3 to 0.965 g/cm3; from 10 wt % to 86 wt % of a propylene component including at least one propylene based polymer having a propylene content of at least 50.0 wt % and a melt flow rate from 0.5 g/10 min to 200.0 g/10 min; from 2 wt % to 22 wt % of an octene component including at least one octene based polymer having an octene content of at least 80 wt %; and from 2 wt % to 20 wt % of a composite component including at least one selected from the group of a crystalline block composite and a specified block composite, derived from at least ethylene and an alpha-olefin.