Abstract:
Embodiments of the present disclosure are directed to multimodal elastomers produced by olefin polymerization with a mixed catalyst system, specifically, a constrained geometry catalyst and a biphenyl phenol catalyst. The multimodal elastomers may be incorporated as impact modifiers in thermoplastic olefins.
Abstract:
The present disclosure provides a composition. In an embodiment an adhesive composition is provided and includes A) a propylene based plastomer or elastomer (PBPE) comprising up to 10 wt % units derived from ethylene and having (i) a Koenig B-value less than 1.0; (ii) a total unsaturation per mole of propylene from 0.01% to 0.03 %; (iii) a density from 0.870 g/cc to 0.890 g/cc; (iv) a melt viscosity at 177°C from 800 mPa.s to 11,000 mPa.s; and (v) a weight average molecular weight from 20,000 to 50,000 g/mol; B) a tackifier; and C) a wax.
Abstract:
An article comprising a polymeric foam, wherein the polymeric foam contains a continuous polymer matrix defining cells therein, the polymer matrix containing: (a) from 25 to 65 weight percent of one or more olefin block copolymer having a melt index of two grams per ten minutes or more, (b) from 65 to 25 weight percent of one or more chlorinated olefin polymer having a Mooney viscosity less than 60 (ML 1+4, 125°C), and (c) from 5 to 30 weight parts of antimony trioxide relative to 100 weight parts of polymers in the polymeric foam, with weight percent values relative to total polymer weight in the polymeric foam; a process for preparing the article.
Abstract:
An article comprising a polymeric foam, wherein the polymeric foam contains a continuous polymer matrix defining cells therein, the polymer matrix containing: (a) from 25 to 65 weight percent of one or more olefin block copolymer having a melt index of two grams per ten minutes or more, (b) from 65 to 25 weight percent of one or more chlorinated olefin polymer having a Mooney viscosity less than 60 (ML 1+4, 125° C.), and (c) from 5 to 30 weight parts of antimony trioxide relative to 100 weight parts of polymers in the polymeric foam, with weight percent values relative to total polymer weight in the polymeric foam; a process for preparing the article.
Abstract:
Ethylenic polymers comprising low levels of total unsaturation are disclosed. Compositions using such ethylene polymers and fabricated articles made from them are also disclosed.
Abstract:
Embodiments of the invention provide a class of mesophase separated propylene/α-olefin block interpolymers with controlled block sequences. The propylene/α-olefin interpolymers are characterized by an average block index, ABI, which is greater than zero and up to about 1.0 and a molecular weight distribution, Mw/Mn, greater than about 1.4. Preferably, the block index is from about 0.2 to about 1. In addition or alternatively, the block propylene/α-olefin interpolymer is characterized by having at least one fraction obtained by Temperature Rising Elution Fractionation (“TREF”), wherein the fraction has a block index greater than about 0.3 and up to about 1.0 and the propylene/α-olefin interpolymer has a molecular weight distribution, Mw/Mn, greater than about 1.4.
Abstract:
The present disclosure provides a composition. In an embodiment an adhesive composition is provided and includes A) a propylene based plastomer or elastomer (PBPE) comprising up to 10 wt % units derived from ethylene and having (i) a Koenig B-value less than 1.0; (ii) a total unsaturation per mole of propylene from 0.01% to 0.03%; (iii) a density from 0.870 g/cc to 0.890 g/cc; (iv) a melt viscosity at 177° C. from 800 mPa·s to 11,000 mPa·s; and (v) a weight average molecular weight from 20,000 to 50,000 g/mol; B) a tackifier; and C) a wax.