Abstract:
Described are bottles(s) comprising at least one polyester composition comprising at least one polyester which comprises terephthalic acid residues; 30 to 40 mole % of 2,2,4,4-tetramethyl-1,3-cyclobutanediol residues; and 60 to 70 mole % of 1,4-cyclohexanedimethanol residues, wherein the inherent viscosity of said polyester is from 0.50 to 0.68 dL/g as determined in 60/40 (wt/wt) phenol/tetrachloroethane at a concentration of 0.5 g/100 ml at 25° C.; wherein said polyester has a notched Izod impact strength of at least 7.5 ft-lb/inch at 23° C. according to ASTM D256 with a 10-mil notch in a ⅛-inch thick bar; wherein the melt viscosity of said polyester is less than 10,000 poise as measured at 1 radian/second on a rotary melt rheometer at 290° C.; and wherein said polyester composition contains no polycarbonate.
Abstract:
Described are polyester compositions comprising at least one polyester which comprises terephthalic acid residues, 2,2,4,4-tetramethyl-1,3-cyclobutanediol, and 1,4-cyclohexanedimethanol, wherein the inherent viscosity and the Tg of the polyester provides for certain polyester properties. The polyesters may be manufactured into articles such as fibers, films, bottles or sheets.
Abstract:
A molded article comprising at least one polyester which comprises: (a) a dicarboxylic acid component comprising: i) 95 to 99.99 mole % of terephthalic acid residues; and ii) 0.01 to 5 mole % of isophthalic acid; and (b) a glycol component comprising: i) 5 to 15 mole % of 2,2,4,4-tetramethyl-1,3-cyclobutanediol residues; ii) 85 to 95 mole % of 1,4-cyclohexanedimethanol residues; and iii) 5 mole % or less of modifying glycols which are not 2,2,4,4-tetramethyl-1,3-cyclobutanediol or cyclohexanedimethanol, wherein the polyester has an inherent viscosity from 0.80 to 1.0 dL/g and a glass transition temperature (Tg) of 90 to 110° C., and wherein the molded article does not contain polycarbonate.
Abstract:
Described are polyesters comprising (a) a dicarboxylic acid component comprising 80 to 100 mole % terephthalic acid residues; optionally, 0 to 20 mole % aromatic dicarboxylic acid residues or aliphatic dicarboxylic acid residues; 20 to 30 mole % of 2,2,4,4-tetramethyl-1,3-cyclobutanediol residues; and 70 to 80 mole % 1,4-cyclohexanedimethanol residues. The polyesters may be manufactured into articles such as fibers, films, bottles or sheets.
Abstract:
Articles, including water bottle(s) having a weight from 200 to 800 grams comprising a polyester composition comprising at least one polyester which comprises: (a) a dicarboxylic acid component comprising terephthalic acid residues; optionally, aromatic dicarboxylic acid or aliphatic dicarboxylic acid residues; and (b) a glycol component comprising 30 to 40 mole % of 2,2,4,4-tetramethyl-1,3-cyclobutanediol residues; and 60 to 70 mole % of 1,4-cyclohexanedimethanol residues; wherein the total mole % of the dicarboxylic acid component is 100 mole %, and the total mole % of the glycol component is 100 mole and the inherent viscosity of the polyester is from 0.50 to 0.68 dl/g as determined in 60/40 (wt/wt) phenol/tetrachloroethane at a concentration of 0.5 g/100 ml at 25° C.; and wherein the polyester has a Tg of from 100 to 140° C.; and wherein the polyester composition contains no polycarbonate.
Abstract:
Described are polyester compositions comprising at least one polyester which comprises terephthalic acid residues, 2,2,4,4-tetramethyl-1,3-cyclobutanediol, and 1,4-cyclohexanedimethanol, wherein the inherent viscosity and the Tg of the polyester provides for certain polyester properties. The polyesters may be manufactured into articles such as fibers, films, bottles or sheets.
Abstract:
Described as one aspect of the invention are polyester compositions containing: (I) at least one polyester which comprises: (a) a dicarboxylic acid component comprising: (i) 70 to 100 mole % of terephthalic acid residues; (ii) 0 to 30 mole % of aromatic dicarboxylic acid residues having up to 20 carbon atoms; and (iii) 0 to 10 mole % of aliphatic dicarboxylic acid residues having up to 16 carbon atoms; and (b) a glycol component comprising: (i) 1 to 99 mole % of 2,2,4,4-tetramethyl-1,3-cyclobutanediol residues; and (ii) 1 to 99 mole % of cyclohexanedimethanol residues; and (II) at least one thermal stabilizer chosen from at least one of alkyl phosphate esters, aryl phosphate esters, mixed alkyl aryl phosphate esters, reaction products thereof, and mixtures thereof; wherein the total mole % of the dicarboxylic acid component is 100 mole %, and wherein the total mole % of the glycol component is 100 mole %.
Abstract:
Described are polyesters comprising (a) a dicarboxylic acid component comprising 80 to 100 mole % terephthalic acid residues; optionally, 0 to 20 mole % aromatic dicarboxylic acid residues or aliphatic dicarboxylic acid residues; 20 to 30 mole % of 2,2,4,4-tetramethyl-1,3-cyclobutanediol residues; and 70 to 80 mole % 1,4-cyclohexanedimethanol residues. The polyesters may be manufactured into articles such as fibers, films, bottles or sheets.
Abstract:
This invention is related to coating compositions comprising a polyester which further comprises 2,2,4,4-tetramethyl-1,3-cyclobutanediol residues, 1,4-cyclohexanedimethanol residues, and residues of a modifying glycol other than ethylene glycol, chosen from at least one of diethylene glycol, triethylene glycol, propylene glycol, neopentyl glycol, and 1,6-hexanediol; and 50 to 100 mole % of residues of at least one of phthalic anhydride, isophthalic acid, and terephthalic acid.