CAN TOOLING COMPONENTS
    1.
    发明申请
    CAN TOOLING COMPONENTS 审中-公开
    可以工具组件

    公开(公告)号:WO1994005442A1

    公开(公告)日:1994-03-17

    申请号:PCT/US1993007733

    申请日:1993-08-17

    CPC classification number: B21D22/28 B21D37/01

    Abstract: The present invention relates to improvied materials for fabricating can bodies. In particular, the present invention relates to can tooling components (20) fabricated from whisker-reinforced silicon nitride having from about 5 to about 15 weight percent whiskers with an average diameter of at least about 0.75 micrometers. The material preferably has a thermal expansion coefficient of from about 0.20 to about 0.24. The present invention also provides a method for reducing the trim height of can bodies (30) formed using a can tooling apparatus (20, 40, 50, 60, 70, 80).

    Abstract translation: 本发明涉及用于制造罐体的改进材料。 特别地,本发明涉及由具有约5至约15重量%的平均直径为至少约0.75微米的晶须的晶须强化氮化硅制成的罐模具组件(20)。 该材料的热膨胀系数优选为约0.20至约0.24。 本发明还提供一种降低使用罐加工装置(20,40,50,60,70,80)形成的罐体(30)的装配高度的方法。

    CAN TOOLING COMPONENTS
    2.
    发明公开
    CAN TOOLING COMPONENTS 失效
    工具编辑部件饮料罐。

    公开(公告)号:EP0662870A1

    公开(公告)日:1995-07-19

    申请号:EP93920135.0

    申请日:1993-08-17

    CPC classification number: B21D22/28 B21D37/01

    Abstract: The present invention relates to improvied materials for fabricating can bodies. In particular, the present invention relates to can tooling components (20) fabricated from whisker-reinforced silicon nitride having from about 5 to about 15 weight percent whiskers with an average diameter of at least about 0.75 micrometers. The material preferably has a thermal expansion coefficient of from about 0.20 to about 0.24. The present invention also provides a method for reducing the trim height of can bodies (30) formed using a can tooling apparatus (20, 40, 50, 60, 70, 80).