1.
    发明专利
    未知

    公开(公告)号:AT273780B

    公开(公告)日:1969-08-25

    申请号:AT622066

    申请日:1966-06-29

    Inventor: MILLER ELDON D

    Abstract: A refractory batch comprises: (i) 45-75% by weight high alumina refractory material analysing as at least 50% Al2O3; (ii) 10-30% amorphous SiO2 (+ 65 mesh, Tyler); (iii) 5-15% -65 mesh ball clay plasticizer; (iv) the remainder being finely divided calcined Al2O3, the total of (i) and (ii) forming 75-85% of the batch which has a sizing such that: (a) 50-70% of the batch is + 65 mesh; (b) 25-35% of the + 65 fraction is -3 + 10 mesh; (c) at least 70% of the -65 fraction is -150 mesh; (d) at least 10% of the total batch is -325 mesh and this portion comprises substantially equal amounts of calcined alumina and ball clay. Fired refractory shapes, e.g. conduits, may be formed by adding to a refractory batch of the invention a mixture of 6-10% of a tempering liquid (e.g. water) and 0.1-0.3% dispersant (e.g. sodium phosphates), casting in a mould, and firing e.g. to about 2000 DEG F. In comparative Examples II-V the amorphous SiO2 is replaced by zircon and silicon carbide.

    Alumina refractories
    2.
    发明专利

    公开(公告)号:GB1122888A

    公开(公告)日:1968-08-07

    申请号:GB2374167

    申请日:1967-05-22

    Abstract: A batch comprising, by weight, 40-80% fused alumina grain, 59-5% non-fused high alumina refractory material, and 1-15% waterinsoluble, pure Cr2O3, substantially all the discrete particles of the batch being of uniform size and averaging less than 1 m diameter, and the fused Al2O3 containing 0.5-5% TiO2, is formed into a shape and fired to give a ceramically bonded refractory shape containing at least 80% Al2O3, less than 3% SiO2 and less than 2% Fe2O3. Preferably, the fused grain is substantially all + 65 mesh (Tyler), the remainder of the batch being finely divided Cr2O3 and - 65 mesh tabular alumina and/or calcined Bayer process alumina.

Patent Agency Ranking