公开(公告)号:ZA987447B
公开(公告)日:2000-04-03
申请号:ZA987447
申请日:1998-08-18
Applicant: HENKEL CORP
Inventor: JOHNSON PHILIP M , CARLSON LAWRENCE R , WOJCIECHOWSKI SCOTT A
IPC: C25D20060101 , C25D
-
公开(公告)号:AU8899898A
公开(公告)日:1999-03-16
申请号:AU8899898
申请日:1998-08-19
Applicant: HENKEL CORP
Inventor: JOHNSON PHILIP M , CARLSON LAWRENCE R , WOJCIECHOWSKI SCOTT A
Abstract: Anodized aluminum surfaces are advantageously sealed by an energy- and time-saving two step process, in which the first step is contact at not more than 75° C. with a solution containing lithium and fluoride ions and, optionally, surfactant. The second necessary step is treatment with hot water or steam, which may be completed in considerably less time when only hot water or steam is used for sealing. Conventional smut inhibitors and/or neutral buffers as used in hot water for single step sealing may advantageously be included in the second step of this process. 100-1000 ppm concentrations of nickel and/or cobalt ions in the treatment liquid for the second treatment step, if environmentally tolerable, make it possible to complete this step in as little as 10 minutes at a temperature as low as 88° C.
-
公开(公告)号:AU749026B2
公开(公告)日:2002-06-13
申请号:AU8899898
申请日:1998-08-19
Applicant: HENKEL CORP
Inventor: JOHNSON PHILIP M , CARLSON LAWRENCE R , WOJCIECHOWSKI SCOTT A
Abstract: Anodized aluminum surfaces are advantageously sealed by an energy- and time-saving two step process, in which the first step is contact at not more than 75° C. with a solution containing lithium and fluoride ions and, optionally, surfactant. The second necessary step is treatment with hot water or steam, which may be completed in considerably less time when only hot water or steam is used for sealing. Conventional smut inhibitors and/or neutral buffers as used in hot water for single step sealing may advantageously be included in the second step of this process. 100-1000 ppm concentrations of nickel and/or cobalt ions in the treatment liquid for the second treatment step, if environmentally tolerable, make it possible to complete this step in as little as 10 minutes at a temperature as low as 88° C.
-
公开(公告)号:ZA9807447B
公开(公告)日:2000-04-03
申请号:ZA9807447
申请日:1998-08-18
Applicant: HENKEL CORP
Inventor: JOHNSON PHILIP M , CARLSON LAWRENCE R , WOJCIECHOWSKI SCOTT A
IPC: C25D20060101 , C25D
-
公开(公告)号:CA2300859A1
公开(公告)日:1999-03-04
申请号:CA2300859
申请日:1998-08-19
Applicant: HENKEL CORP
Inventor: JOHNSON PHILIP M , WOJCIECHOWSKI SCOTT A , CARLSON LAWRENCE R
Abstract: Anodized aluminum surfaces are advantageously sealed by an energy- and timesaving two step process, in which the first step is contact at not more than 75 ~C with a solution containing lithium and fluoride ions and, optionaly, surfactant. The second necessary step is treatment with hot water or steam, which may be completed in considerably less time than when only hot water or steam is used for sealing. Conventional smut inhibitors and/or neutral buffers as used in hot water for single step sealing may advantageously be included in the second step of this process. 100 - 1000 ppm concentrations of nickel and/or cobalt ions in the treatment liquid for the second treatment step, if environmentally tolerable, make it possible to complete this step in as little as 10 minutes at a temperature as low as 88 ~C.
-
-
-
-