公开(公告)号:DK151570C
公开(公告)日:1988-06-06
申请号:DK550980
申请日:1980-12-23
Applicant: HOECHST AG , KRUPP STAHL AG
Inventor: BRAUN ALBERT , PORTZ WILLI , STRAUSS GEORG , DELHEY HANS-MARTIN
Abstract: The invention relates to agents for the desulfurization of metal melts, especially of steel and crude iron melts, based on mixtures of CaC2/CaO crystals produced in the fused mass. A portion of the CaO in the crystal mixture is hydrated to form Ca(OH)2. A process for the manufacture of these agents is also described.
-
公开(公告)号:DK151569B
公开(公告)日:1987-12-14
申请号:DK550880
申请日:1980-12-23
Applicant: HOECHST AG , KRUPP STAHL AG
Inventor: BRAUN ALBERT , PORTZ WILLI , STRAUSS GEORG , DELHEY HANS-MARTIN
IPC: C01B32/942 , C21C1/02 , C21C7/064 , C21C7/076
Abstract: The present invention relates to a process for the manufacture of desulfurizing agents containing 1-6% by weight of chemically bonded water, based on calcium oxide-containing calcium carbide, for crude iron and steel melts. To this end, a molten mixture of calcium carbide and calcium oxide with a CaO content of 20 to 80% by weight is produced, which is allowed to solidify into a block. Next, the block which still has an average temperature of more than 400 DEG C., is rough-crushed to particles with a size of less than 150 mm and calcium oxide is added to the comminuted mixture, which still has a temperature of at least 400 DEG C., in accordance with the CaO content desired in the end product. The mixture is finally ground in the presence of air or nitrogen with a moisture content of from 5 to 20 g/m3 (at 1.013 bar and 273.15 K) at temperatures below 100 DEG C. to particles with a size of less than 10 mm.
-
公开(公告)号:NO153500B
公开(公告)日:1985-12-23
申请号:NO803924
申请日:1980-12-23
Applicant: HOECHST AG , KRUPP STAHL AG
Inventor: BRAUN ALBERT , PORTZ WILLI , STRAUSS GEORG , DELHEY HANS-MARTIN
IPC: C01B32/942 , C21C1/02 , C21C7/064 , C21C7/076 , C01B31/32
Abstract: The present invention relates to a process for the manufacture of desulfurizing agents containing 1-6% by weight of chemically bonded water, based on calcium oxide-containing calcium carbide, for crude iron and steel melts. To this end, a molten mixture of calcium carbide and calcium oxide with a CaO content of 20 to 80% by weight is produced, which is allowed to solidify into a block. Next, the block which still has an average temperature of more than 400 DEG C., is rough-crushed to particles with a size of less than 150 mm and calcium oxide is added to the comminuted mixture, which still has a temperature of at least 400 DEG C., in accordance with the CaO content desired in the end product. The mixture is finally ground in the presence of air or nitrogen with a moisture content of from 5 to 20 g/m3 (at 1.013 bar and 273.15 K) at temperatures below 100 DEG C. to particles with a size of less than 10 mm.
-
公开(公告)号:NO803924L
公开(公告)日:1981-06-30
申请号:NO803924
申请日:1980-12-23
Applicant: HOECHST AG , KRUPP STAHL AG
Inventor: BRAUN ALBERT , PORTZ WILLI , STRAUSS GEORG , DELHEY HANS-MARTIN
IPC: C01B32/942 , C21C1/02 , C21C7/064 , C21C7/076 , C21C
Abstract: The present invention relates to a process for the manufacture of desulfurizing agents containing 1-6% by weight of chemically bonded water, based on calcium oxide-containing calcium carbide, for crude iron and steel melts. To this end, a molten mixture of calcium carbide and calcium oxide with a CaO content of 20 to 80% by weight is produced, which is allowed to solidify into a block. Next, the block which still has an average temperature of more than 400 DEG C., is rough-crushed to particles with a size of less than 150 mm and calcium oxide is added to the comminuted mixture, which still has a temperature of at least 400 DEG C., in accordance with the CaO content desired in the end product. The mixture is finally ground in the presence of air or nitrogen with a moisture content of from 5 to 20 g/m3 (at 1.013 bar and 273.15 K) at temperatures below 100 DEG C. to particles with a size of less than 10 mm.
-
公开(公告)号:MX154954A
公开(公告)日:1988-01-14
申请号:MX18547881
申请日:1981-01-05
Applicant: HOECHST AG , KRUPP STAHL AG
Inventor: BRAUN ALBERT , PORTZ WILLI , STRAUSS GEORGE , DELHEY HANS-MARTIN
IPC: C01B32/942 , C21C1/02 , C21C7/064 , C21C7/076
Abstract: The present invention relates to a process for the manufacture of desulfurizing agents containing 1-6% by weight of chemically bonded water, based on calcium oxide-containing calcium carbide, for crude iron and steel melts. To this end, a molten mixture of calcium carbide and calcium oxide with a CaO content of 20 to 80% by weight is produced, which is allowed to solidify into a block. Next, the block which still has an average temperature of more than 400 DEG C., is rough-crushed to particles with a size of less than 150 mm and calcium oxide is added to the comminuted mixture, which still has a temperature of at least 400 DEG C., in accordance with the CaO content desired in the end product. The mixture is finally ground in the presence of air or nitrogen with a moisture content of from 5 to 20 g/m3 (at 1.013 bar and 273.15 K) at temperatures below 100 DEG C. to particles with a size of less than 10 mm.
-
公开(公告)号:AU532989B2
公开(公告)日:1983-10-20
申请号:AU6585480
申请日:1980-12-24
Applicant: HOECHST AG , KRUPP STAHL AG
Inventor: BRAUN ALBERT , PORTZ WILLI , STRAUSS GEORG , DELHEY HANS-MARTIN
IPC: C01B32/942 , C21C1/02 , C21C7/064 , C21C7/076
Abstract: The present invention relates to a process for the manufacture of desulfurizing agents containing 1-6% by weight of chemically bonded water, based on calcium oxide-containing calcium carbide, for crude iron and steel melts. To this end, a molten mixture of calcium carbide and calcium oxide with a CaO content of 20 to 80% by weight is produced, which is allowed to solidify into a block. Next, the block which still has an average temperature of more than 400 DEG C., is rough-crushed to particles with a size of less than 150 mm and calcium oxide is added to the comminuted mixture, which still has a temperature of at least 400 DEG C., in accordance with the CaO content desired in the end product. The mixture is finally ground in the presence of air or nitrogen with a moisture content of from 5 to 20 g/m3 (at 1.013 bar and 273.15 K) at temperatures below 100 DEG C. to particles with a size of less than 10 mm.
-
公开(公告)号:DD202183A5
公开(公告)日:1983-08-31
申请号:DD23830882
申请日:1982-03-19
Applicant: HOECHST AG
Inventor: BRAUN ALBERT , PORTZ WILLI , STRAUSS GEORG , DELHEY HANS-MARTIN
Abstract: The disclosure relates to a process for the manufacture of desulfurizing agents containing 1-6 weight % chemically combined water, based on calcium oxide and carbon-containing calcium carbide, for crude iron and steel melts. More particularly, the disclosure provides for a molten mixture of calcium carbide and calcium oxide containing 20 to 80 weight % CaO to be made from lime and coke; for the mixture to be allowed to cool and solidify into a block; for the solidified block while it still has an average temperature of more than 400 DEG C. to be crushed to particles with a size of less than 150 mm; for the comminuted mixture, which still has a temperature of at least 400 DEG C. to be admixed with a quantity of calcium oxide necessary to establish in the resulting mixture a total content of CaO corresponding to the CaO content desired in the end product; and for the mixture to be gound while intensively mixing it with free carbon and carbonate in the presence of air or nitrogen with a moisture content of 5 to 20 g/m3 (at 1.013 bar and 273.15 K.) at temperatures below 100 DEG C. to particles with a size of less than 10 mm.
-
公开(公告)号:DD202182A5
公开(公告)日:1983-08-31
申请号:DD23830682
申请日:1982-03-19
Applicant: HOECHST AG
Inventor: BRAUN ALBERT , PORTZ WILLI , STRAUSS GEORG , DELHEY HANS-MARTIN
-
公开(公告)号:NO153499B
公开(公告)日:1985-12-23
申请号:NO803923
申请日:1980-12-23
Applicant: HOECHST AG , KRUPP STAHL AG
Inventor: BRAUN ALBERT , PORTZ WILLI , STRAUSS GEORG , DELHEY HANS-MARTIN
Abstract: The invention relates to agents for the desulfurization of metal melts, especially of steel and crude iron melts, based on mixtures of CaC2/CaO crystals produced in the fused mass. A portion of the CaO in the crystal mixture is hydrated to form Ca(OH)2. A process for the manufacture of these agents is also described.
-
公开(公告)号:IN153342B
公开(公告)日:1984-07-07
申请号:IN1420CA1980
申请日:1980-12-23
Applicant: HOECHST AG , KRUPP STAHL AG
Inventor: BRAUN ALBERT , PORTZ WILLI , STRAUSS GEORG , DELHEY HANS-MARTIN
IPC: C01B32/942 , C21C1/02 , C21C7/064 , C21C7/076
Abstract: The present invention relates to a process for the manufacture of desulfurizing agents containing 1-6% by weight of chemically bonded water, based on calcium oxide-containing calcium carbide, for crude iron and steel melts. To this end, a molten mixture of calcium carbide and calcium oxide with a CaO content of 20 to 80% by weight is produced, which is allowed to solidify into a block. Next, the block which still has an average temperature of more than 400 DEG C., is rough-crushed to particles with a size of less than 150 mm and calcium oxide is added to the comminuted mixture, which still has a temperature of at least 400 DEG C., in accordance with the CaO content desired in the end product. The mixture is finally ground in the presence of air or nitrogen with a moisture content of from 5 to 20 g/m3 (at 1.013 bar and 273.15 K) at temperatures below 100 DEG C. to particles with a size of less than 10 mm.
-
-
-
-
-
-
-
-
-