公开(公告)号:ZA8405807B
公开(公告)日:1985-04-24
申请号:ZA8405807
申请日:1984-07-27
Applicant: HOECHST AG
Inventor: ERNST JOSEF , SEMMLER HANS-JOACHIM
-
公开(公告)号:DE59306073D1
公开(公告)日:1997-05-15
申请号:DE59306073
申请日:1993-01-26
Applicant: HOECHST AG
Inventor: ERNST JOSEF , SEMMLER HANS JOACHIM DR , WIRTZ PETER DR
Abstract: The invention relates to a dry, surfactant-free single-component alkali metal silicate cement composition containing as hardening agent condensed aluminum phosphate and at least one compound from the group comprising the ortho- and pyrophosphates of manganese, zinc, cobalt, iron(III) and chromium(III) and in addition containing the conventional components rounded quartz sand, clay, kieselguhr, mineral oil and solid powdered sodium water glass or potassium water glass.
-
公开(公告)号:CA2088212A1
公开(公告)日:1993-07-29
申请号:CA2088212
申请日:1993-01-27
Applicant: HOECHST AG
Inventor: ERNST JOSEF , SEMMLER HANS J , WIRTZ PETER
Abstract: HOE 92/F 023 Single-component alkali metal silicate cement composition The invention relates to a dry, surfactant-free singlecomponent alkali metal silicate cement composition containing as hardening agent condensed aluminum phosphate and at least one compound from the group comprising the ortho- and pyrophosphates of manganese, zinc, cobalt, iron(III) and chromium(III) and in addition containing the conventional components rounded quartz sand, clay, kieselguhr, mineral oil and solid powdered sodium water glass or potassium water glass.
-
公开(公告)号:ZA845807B
公开(公告)日:1985-04-24
申请号:ZA845807
申请日:1984-07-27
Applicant: HOECHST AG
Inventor: ERNST JOSEF , SEMMLER HANS-JOACHIM
Abstract: A dry one-component alkali metal silicate cement composition contains the following components: (a) condensed aluminum phosphate or condensed aluminum/iron phosphate as hardener in amounts between 2-10% by weight, (b) rounded quartz sand having a grain size between 0.01 and 0.5 mm in amounts of 30-70% by weight, (c) clay constituents in amounts of 10-40% by weight, (d) kieselguhr in amounts of 1-5% by weight, (e) mineral oil in amounts of 0.05-1% by weight and (f) solid pulverulent sodium silicate, potassium silicate or mixtures thereof in amounts of 10-25% by weight. The composition is free of surfactant. When combined with water the cement is slow to set into an acid-resistant mortar.
-
公开(公告)号:FI842980A0
公开(公告)日:1984-07-26
申请号:FI842980
申请日:1984-07-26
Applicant: HOECHST AG
Inventor: ERNST JOSEF , SEMMLER HANS-JOACHIM
Abstract: A dry one-component alkali metal silicate cement composition contains the following components: (a) condensed aluminum phosphate or condensed aluminum/iron phosphate as hardener in amounts between 2-10% by weight, (b) rounded quartz sand having a grain size between 0.01 and 0.5 mm in amounts of 30-70% by weight, (c) clay constituents in amounts of 10-40% by weight, (d) kieselguhr in amounts of 1-5% by weight, (e) mineral oil in amounts of 0.05-1% by weight and (f) solid pulverulent sodium silicate, potassium silicate or mixtures thereof in amounts of 10-25% by weight. The composition is free of surfactant. When combined with water the cement is slow to set into an acid-resistant mortar.
-
公开(公告)号:DE3466976D1
公开(公告)日:1987-12-03
申请号:DE3466976
申请日:1984-07-25
Applicant: HOECHST AG
Inventor: ERNST JOSEF , SEMMLER HANS-JOACHIM DR
Abstract: A dry one-component alkali metal silicate cement composition contains the following components: (a) condensed aluminum phosphate or condensed aluminum/iron phosphate as hardener in amounts between 2-10% by weight, (b) rounded quartz sand having a grain size between 0.01 and 0.5 mm in amounts of 30-70% by weight, (c) clay constituents in amounts of 10-40% by weight, (d) kieselguhr in amounts of 1-5% by weight, (e) mineral oil in amounts of 0.05-1% by weight and (f) solid pulverulent sodium silicate, potassium silicate or mixtures thereof in amounts of 10-25% by weight. The composition is free of surfactant. When combined with water the cement is slow to set into an acid-resistant mortar.
-
公开(公告)号:AT30409T
公开(公告)日:1987-11-15
申请号:AT84108802
申请日:1984-07-25
Applicant: HOECHST AG
Inventor: ERNST JOSEF , SEMMLER HANS-JOACHIM DR
-
公开(公告)号:FI842980A
公开(公告)日:1985-01-29
申请号:FI842980
申请日:1984-07-26
Applicant: HOECHST AG
Inventor: ERNST JOSEF , SEMMLER HANS-JOACHIM
Abstract: A dry one-component alkali metal silicate cement composition contains the following components: (a) condensed aluminum phosphate or condensed aluminum/iron phosphate as hardener in amounts between 2-10% by weight, (b) rounded quartz sand having a grain size between 0.01 and 0.5 mm in amounts of 30-70% by weight, (c) clay constituents in amounts of 10-40% by weight, (d) kieselguhr in amounts of 1-5% by weight, (e) mineral oil in amounts of 0.05-1% by weight and (f) solid pulverulent sodium silicate, potassium silicate or mixtures thereof in amounts of 10-25% by weight. The composition is free of surfactant. When combined with water the cement is slow to set into an acid-resistant mortar.
-
公开(公告)号:AT151395T
公开(公告)日:1997-04-15
申请号:AT93101113
申请日:1993-01-26
Applicant: HOECHST AG
Inventor: ERNST JOSEF , SEMMLER HANS JOACHIM DR , WIRTZ PETER DR
Abstract: The invention relates to a dry, surfactant-free single-component alkali metal silicate cement composition containing as hardening agent condensed aluminum phosphate and at least one compound from the group comprising the ortho- and pyrophosphates of manganese, zinc, cobalt, iron(III) and chromium(III) and in addition containing the conventional components rounded quartz sand, clay, kieselguhr, mineral oil and solid powdered sodium water glass or potassium water glass.
-
公开(公告)号:DE3327176A1
公开(公告)日:1985-02-07
申请号:DE3327176
申请日:1983-07-28
Applicant: HOECHST AG
Inventor: ERNST JOSEF , SEMMLER HANS-JOACHIM DR
Abstract: A dry one-component alkali metal silicate cement composition contains the following components: (a) condensed aluminum phosphate or condensed aluminum/iron phosphate as hardener in amounts between 2-10% by weight, (b) rounded quartz sand having a grain size between 0.01 and 0.5 mm in amounts of 30-70% by weight, (c) clay constituents in amounts of 10-40% by weight, (d) kieselguhr in amounts of 1-5% by weight, (e) mineral oil in amounts of 0.05-1% by weight and (f) solid pulverulent sodium silicate, potassium silicate or mixtures thereof in amounts of 10-25% by weight. The composition is free of surfactant. When combined with water the cement is slow to set into an acid-resistant mortar.
-
-
-
-
-
-
-
-
-