2.
    发明专利
    未知

    公开(公告)号:SE393978B

    公开(公告)日:1977-05-31

    申请号:SE7401204

    申请日:1974-01-30

    Applicant: HOECHST AG

    Abstract: Production of vinyl chloride, wherein 1,2-dichloroethane is evaporated under pressure in an evaporation stage and resulting 1,2-dichloroethane in vapor form is thermally cracked at a temperature substantially within the range 450 DEG -650 DEG C with the resultant formation of vinyl chloride.

    3.
    发明专利
    未知

    公开(公告)号:DK143697B

    公开(公告)日:1981-09-28

    申请号:DK123774

    申请日:1974-03-07

    Applicant: HOECHST AG

    Abstract: Production of vinyl chloride, wherein 1,2-dichloroethane is evaporated under pressure in an evaporation stage and resulting 1,2-dichloroethane in vapor form is thermally cracked at a temperature substantially within the range 450 DEG -650 DEG C with the resultant formation of vinyl chloride.

    6.
    发明专利
    未知

    公开(公告)号:BR7802608A

    公开(公告)日:1978-12-19

    申请号:BR7802608

    申请日:1978-04-26

    Applicant: HOECHST AG

    Abstract: 1,2-dichloroethane is made by subjecting ethylene to an oxychlorination reaction with hydrogen chloride and a gas containing molecular oxygen in gas phase, at elevated temperature and in contact with a fluidized bed copper-II-chloride catalyst on a carrier, wherein the reaction gases are cooled under pressure in two condensation stages, condensed 1,2-dichloroethane and water are removed and the bulk of unreacted starting gas and inert gas are recycled. More specifically the reaction gases are delivered to a third condensation stage and cooled therein under pressure down to a temperature within the range 5 DEG to 18 DEG C. and to the extent necessary for the recycle gas to contain 0.5 to 3 volume % of 1,2-dichloroethane. Next, the recycle gas is directly admixed upstream of the reactor, with a quantity of pure oxygen necessary to replace consumed oxygen and re-establish an oxygen content of 12 to 25 volume % therein.

    10.
    发明专利
    未知

    公开(公告)号:SE442745B

    公开(公告)日:1986-01-27

    申请号:SE7804878

    申请日:1978-04-27

    Applicant: HOECHST AG

    Abstract: 1,2-dichloroethane is made by subjecting ethylene to an oxychlorination reaction with hydrogen chloride and a gas containing molecular oxygen in gas phase, at elevated temperature and in contact with a fluidized bed copper-II-chloride catalyst on a carrier, wherein the reaction gases are cooled under pressure in two condensation stages, condensed 1,2-dichloroethane and water are removed and the bulk of unreacted starting gas and inert gas are recycled. More specifically the reaction gases are delivered to a third condensation stage and cooled therein under pressure down to a temperature within the range 5 DEG to 18 DEG C. and to the extent necessary for the recycle gas to contain 0.5 to 3 volume % of 1,2-dichloroethane. Next, the recycle gas is directly admixed upstream of the reactor, with a quantity of pure oxygen necessary to replace consumed oxygen and re-establish an oxygen content of 12 to 25 volume % therein.

Patent Agency Ranking