1.
    发明专利
    未知

    公开(公告)号:DK0770149T3

    公开(公告)日:1999-09-13

    申请号:DK96910851

    申请日:1996-04-30

    Abstract: PCT No. PCT/AT96/00085 Sec. 371 Date Dec. 31, 1996 Sec. 102(e) Date Dec. 31, 1996 PCT Filed May 30, 1996 PCT Pub. No. WO96/34989 PCT Pub. Date Nov. 7, 1996In a process for the production of hydraulic binders, crude steel and/or alloys, such as, e.g., FeCr or FeV, from basic steel slags containing chromium and/or vanadium, the liquid steel slag is mixed with an additive selected from the group consisting of blast furnace slag, electric arc furnace slag, dusts from steel production, metallic waste substances or refuse incineration residues and/or with acid additives for lowering the viscosity, whereupon steel is sedimented out of the liquid slag and the remaining slag in a first reduction stage is reduced to metallic iron having an iron oxide content of below 5 wt. % and above 1 wt. %, whereupon the remaining slag melt in a second reduction stage having a higher reduction potential as compared to the first reduction stage is further reduced to metallic Cr or V or ferroalloys thereof and the hydraulically active slag is separated.

    PROCESS FOR PRODUCING HYDRAULIC BINDERS AND/OR ALLOYS, E.G. FERROCHROMIUM OR FERROVANADIUM

    公开(公告)号:GR3029712T3

    公开(公告)日:1999-06-30

    申请号:GR990400799

    申请日:1999-03-16

    Abstract: PCT No. PCT/AT96/00085 Sec. 371 Date Dec. 31, 1996 Sec. 102(e) Date Dec. 31, 1996 PCT Filed May 30, 1996 PCT Pub. No. WO96/34989 PCT Pub. Date Nov. 7, 1996In a process for the production of hydraulic binders, crude steel and/or alloys, such as, e.g., FeCr or FeV, from basic steel slags containing chromium and/or vanadium, the liquid steel slag is mixed with an additive selected from the group consisting of blast furnace slag, electric arc furnace slag, dusts from steel production, metallic waste substances or refuse incineration residues and/or with acid additives for lowering the viscosity, whereupon steel is sedimented out of the liquid slag and the remaining slag in a first reduction stage is reduced to metallic iron having an iron oxide content of below 5 wt. % and above 1 wt. %, whereupon the remaining slag melt in a second reduction stage having a higher reduction potential as compared to the first reduction stage is further reduced to metallic Cr or V or ferroalloys thereof and the hydraulically active slag is separated.

    3.
    发明专利
    未知

    公开(公告)号:DE59601179D1

    公开(公告)日:1999-03-04

    申请号:DE59601179

    申请日:1996-04-30

    Abstract: PCT No. PCT/AT96/00085 Sec. 371 Date Dec. 31, 1996 Sec. 102(e) Date Dec. 31, 1996 PCT Filed May 30, 1996 PCT Pub. No. WO96/34989 PCT Pub. Date Nov. 7, 1996In a process for the production of hydraulic binders, crude steel and/or alloys, such as, e.g., FeCr or FeV, from basic steel slags containing chromium and/or vanadium, the liquid steel slag is mixed with an additive selected from the group consisting of blast furnace slag, electric arc furnace slag, dusts from steel production, metallic waste substances or refuse incineration residues and/or with acid additives for lowering the viscosity, whereupon steel is sedimented out of the liquid slag and the remaining slag in a first reduction stage is reduced to metallic iron having an iron oxide content of below 5 wt. % and above 1 wt. %, whereupon the remaining slag melt in a second reduction stage having a higher reduction potential as compared to the first reduction stage is further reduced to metallic Cr or V or ferroalloys thereof and the hydraulically active slag is separated.

    6.
    发明专利
    未知

    公开(公告)号:TR199601046T1

    公开(公告)日:1997-04-22

    申请号:TR9601046

    申请日:1996-04-30

    Abstract: PCT No. PCT/AT96/00085 Sec. 371 Date Dec. 31, 1996 Sec. 102(e) Date Dec. 31, 1996 PCT Filed May 30, 1996 PCT Pub. No. WO96/34989 PCT Pub. Date Nov. 7, 1996In a process for the production of hydraulic binders, crude steel and/or alloys, such as, e.g., FeCr or FeV, from basic steel slags containing chromium and/or vanadium, the liquid steel slag is mixed with an additive selected from the group consisting of blast furnace slag, electric arc furnace slag, dusts from steel production, metallic waste substances or refuse incineration residues and/or with acid additives for lowering the viscosity, whereupon steel is sedimented out of the liquid slag and the remaining slag in a first reduction stage is reduced to metallic iron having an iron oxide content of below 5 wt. % and above 1 wt. %, whereupon the remaining slag melt in a second reduction stage having a higher reduction potential as compared to the first reduction stage is further reduced to metallic Cr or V or ferroalloys thereof and the hydraulically active slag is separated.

    PROCESS FOR PRODUCING HYDRAULIC BINDERS AND/OR ALLOYS, E.G. FERROCHROMIUM OR FERROVANADIUM

    公开(公告)号:SI0770149T1

    公开(公告)日:1999-06-30

    申请号:SI9630049

    申请日:1996-04-30

    Abstract: PCT No. PCT/AT96/00085 Sec. 371 Date Dec. 31, 1996 Sec. 102(e) Date Dec. 31, 1996 PCT Filed May 30, 1996 PCT Pub. No. WO96/34989 PCT Pub. Date Nov. 7, 1996In a process for the production of hydraulic binders, crude steel and/or alloys, such as, e.g., FeCr or FeV, from basic steel slags containing chromium and/or vanadium, the liquid steel slag is mixed with an additive selected from the group consisting of blast furnace slag, electric arc furnace slag, dusts from steel production, metallic waste substances or refuse incineration residues and/or with acid additives for lowering the viscosity, whereupon steel is sedimented out of the liquid slag and the remaining slag in a first reduction stage is reduced to metallic iron having an iron oxide content of below 5 wt. % and above 1 wt. %, whereupon the remaining slag melt in a second reduction stage having a higher reduction potential as compared to the first reduction stage is further reduced to metallic Cr or V or ferroalloys thereof and the hydraulically active slag is separated.

    Process for producing hydraulic binders and/or alloys, e.g. ferrochromium or ferrovanadium

    公开(公告)号:AU706170B2

    公开(公告)日:1999-06-10

    申请号:AU5392696

    申请日:1996-04-30

    Abstract: PCT No. PCT/AT96/00085 Sec. 371 Date Dec. 31, 1996 Sec. 102(e) Date Dec. 31, 1996 PCT Filed May 30, 1996 PCT Pub. No. WO96/34989 PCT Pub. Date Nov. 7, 1996In a process for the production of hydraulic binders, crude steel and/or alloys, such as, e.g., FeCr or FeV, from basic steel slags containing chromium and/or vanadium, the liquid steel slag is mixed with an additive selected from the group consisting of blast furnace slag, electric arc furnace slag, dusts from steel production, metallic waste substances or refuse incineration residues and/or with acid additives for lowering the viscosity, whereupon steel is sedimented out of the liquid slag and the remaining slag in a first reduction stage is reduced to metallic iron having an iron oxide content of below 5 wt. % and above 1 wt. %, whereupon the remaining slag melt in a second reduction stage having a higher reduction potential as compared to the first reduction stage is further reduced to metallic Cr or V or ferroalloys thereof and the hydraulically active slag is separated.