Abstract:
Provided is a composite material including a plurality of porous silicate particles having a glass phase structure, a first active metal adsorbed into the glass phase structure of the porous silicate particles, and a modified layer containing a second active metal formed on the surfaces of the porous silicate particles. The porous silicate particles have an average pore diameter of from 3 nm to 50 nm, and the first active metal includes at least one of sodium, potassium, calcium, and magnesium.
Abstract:
An inorganic material for removing a harmful substance from wastewater is provided. The inorganic material includes a plurality of porous silicate particles having a glass phase structure, wherein the plurality of porous silicate particles include silicon dioxide, aluminum oxide, barium oxide, cesium oxide, and boron oxide, and have a zeta potential of a negative value at pH of from 1 to 5, and wherein the average pore diameter of the porous silicate particles is in a range of from 3 to 50 nm. Moreover, a method for preparing an inorganic material for removing a harmful substance from wastewater and a method for wastewater treatment are further provided.
Abstract:
An inorganic material for removing a harmful substance from wastewater is provided. The inorganic material includes a plurality of porous silicate particles having a glass phase structure, wherein the plurality of porous silicate particles include silicon dioxide, aluminum oxide, barium oxide, cesium oxide, and boron oxide, and have a zeta potential of a negative value at pH of from 1 to 5, and wherein the average pore diameter of the porous silicate particles is in a range of from 3 to 50 nm. Moreover, a method for preparing an inorganic material for removing a harmful substance from wastewater and a method for wastewater treatment are further provided.
Abstract:
Provided is an adsorption material including a plurality of porous silicate particles having a glass-phase structure and including silicon oxide, aluminum oxide, barium oxide, strontium oxide and boron oxide. An average pore size of the plurality of porous silicate particles is in a range of from 3 nm to 50 nm, and a zeta potential of the plurality of porous silicate particles is negative at a pH value of from 1 to 5. A method of fabricating the adsorption material is further provided.