公开(公告)号:WO2014194070A1
公开(公告)日:2014-12-04
申请号:PCT/US2014/039991
申请日:2014-05-29
Inventor: LIU, Hong , SMITH, Steven, W. , BIVIGOU KOUMBA, Achille, M. , HIETPAS, Geoffrey, D. , BAKKER, Willem
IPC: D01F6/70
CPC classification number: D01F8/16 , D03D15/0027 , D03D15/08 , D04B1/16 , D04B1/18 , D04H3/009 , D04H3/147 , D10B2201/02 , D10B2331/10
Abstract: Included are segmented polyurethane elastic fibers or spandex fibers, capable of bonding to polymer fiber such as nylon or polyamide fibers, in addition to bonding to itself, for apparel textile applications. More particularly the invention relates to bicomponent spandex fibers, with a heat resistant core and a heat sensitive sheath, spun from polymer solutions. The nylon fabrics containing such spandex fibers have enhanced stretch performance and improved surface appearance after heat treatment to activate the fusing and bonding between nylon fibers and spandex fibers.
Abstract translation: 包括的是分段聚氨酯弹性纤维或氨纶纤维,除了结合自身之外,还可以粘合到诸如尼龙或聚酰胺纤维的聚合物纤维上,用于服装纺织品应用。 更具体地,本发明涉及由聚合物溶液纺丝的双组分氨纶纤维,其具有耐热芯和热敏护套。 含有这种氨纶纤维的尼龙织物在热处理后具有增强的拉伸性能和改善的表面外观,以激活尼龙纤维和氨纶纤维之间的熔合和粘合。
-
公开(公告)号:WO2014210378A2
公开(公告)日:2014-12-31
申请号:PCT/US2014/044436
申请日:2014-06-26
Applicant: INVISTA TECHNOLOGIES S.A.R.L.
Inventor: LIU, Hong , BAKKER, Willem , FARMER, Douglas K. , LEUNG, Raymond S.P. , LI, Jin , LIAO, Tianyi , PROFIT, Michael , SMITH, Steven W. , TEERLINK, Thomas W. , CELEBI, Oguzhan , D'ALLURA, Norman J.
Abstract: Included is a polyurethane elastic fiber that includes a blended glycol. A polyether glycol, such as PTMEG is partially replaced with PPG. The ratio of total isocyanate (NCO) end groups from the prepolymer to total primary amine (NH 2 ) end groups from the diamine chain extender is about 0.99 to about 1.01; and the combined amount of non-reactive end groups from the PPG and dialkylurea end groups in the polyurethaneurea is less than about 50 meq/kg.
Abstract translation: 包括含有混合二醇的聚氨酯弹性纤维。 聚乙二醇如PTMEG被PPG部分置换。 来自二胺扩链剂的来自预聚物的总异氰酸酯(NCO)端基与总伯胺(NH 2)端基的比例为约0.99至约1.01; 并且来自聚氨酯脲中的PPG和二烷基脲端基的非反应性端基的组合量小于约50meq / kg。
-
公开(公告)号:WO2011097088A3
公开(公告)日:2011-08-11
申请号:PCT/US2011/022233
申请日:2011-01-24
Applicant: INVISTA TECHNOLOGIES S.A.R.L. , BAKKER, Willem , MAGGI, Daniele , PERRON, Maurice
Inventor: BAKKER, Willem , MAGGI, Daniele , PERRON, Maurice
Abstract: The invention provides hosiery including a panty portion that is assymetrical. The hosiery provides a comfortable fit for a variety of different sizes including larger sizes and maternity.
-
4.
公开(公告)号:WO2004088014A1
公开(公告)日:2004-10-14
申请号:PCT/US2004/009514
申请日:2004-03-26
Applicant: INVISTA TECHNOLOGIES S.A.R.L. , BAKKER, Willem , PULVERMACHER, Bernd , VERDAN, Michel , BERTHOUD, Nicolas, Philippe
Inventor: BAKKER, Willem , PULVERMACHER, Bernd , VERDAN, Michel , BERTHOUD, Nicolas, Philippe
IPC: D02G3/32
CPC classification number: D02G3/328
Abstract: A continuous method for producing composite elastic yarns at speeds up to 700 m/min by (a) stretching (drafting) an elastomeric yarn (e.g., spandex) by 2.0x (100%) to 10.5x (950%) while heating (max. heating temperature 220°C) in a single or double stage draft, (b) air-jet entangling with a relatively inelastic yarn component to create a composite elastic yarn, and then (c) in-line heat-treating (max. heating temperature 240°C) the composite elastic yarn. The initial draft stage(s) may also be carried out at ambient temperature. The resulting composite elastic yarn has improved stitch clarity, particularly suited for hosiery, and its properties can be tailored to provide fabric properties for knit and woven fabrics hitherto not possible with standard spandex yarns.
Abstract translation: (a)在加热时(a)将弹性纱线(例如氨纶)拉伸(牵伸)2.0倍(100%)至10.5×(950%)),以加速速度(最大值),以700m / min的速度生产复合弹性纱线的连续方法 加热温度220℃),(b)用相对非弹性的纱线组分进行空气喷射缠结以产生复合弹性纱线,然后(c)在线热处理(最大加热 温度240℃)复合弹力纱。 初始起始阶段也可以在环境温度下进行。 所得到的复合弹性纱线具有提高的针迹清晰度,特别适用于针织品,并且其性能可以被定制以提供迄今为止不能用标准氨纶纱线的针织和机织织物的织物性能。
-
-
-