Abstract:
A linear polyamide having a weight average molecular weight above 200,000 is made by heating a lower molecular weight molten polyamide with thorough mixing at a temperature of about 265-300 DEG C for at least 5 minutes while an inert gas is swept gently through the reactor, the increase of molecular weight of the polyamide being catalyzed by a particular phosphinic acid derivative.