1.
公开(公告)号:US11760855B2
公开(公告)日:2023-09-19
申请号:US17023904
申请日:2020-09-17
Applicant: KANEKA CORPORATION
Inventor: Haruki Koyama , Hanako Hasebe , Katsumi Yamaguchi , Yukihiro Shimamoto
IPC: C08J7/048 , C08J7/046 , B32B27/08 , B32B27/30 , C08F265/06 , C08F285/00 , C08J5/18 , C08L51/04 , C08J7/043 , C08J7/044
CPC classification number: C08J7/048 , B32B27/08 , B32B27/308 , C08F265/06 , C08F285/00 , C08J5/18 , C08J7/043 , C08J7/044 , C08J7/046 , C08L51/04 , B32B2255/10 , B32B2255/26 , B32B2264/025 , B32B2305/72 , B32B2307/418 , B32B2307/536 , B32B2457/20 , B32B2605/003 , C08J2351/04 , C08J2483/04 , C08L2207/53
Abstract: An acrylic resin film is provided that may include graft copolymer particles (A) with a multilayer structure and graft copolymer particles (B) with a multilayer structure, wherein the graft copolymer particles (A) may have an average particle size in the range of 20 to 150 nm, the graft copolymer particles (B) may have a larger average particle size than the graft copolymer particles (A). The graft copolymer particles (A) may include a cross-linked elastomer (A1) and a graft polymer layer (A2), the graft polymer layer (A2) being closer to a surface layer than the cross-linked elastomer (A1). Further, a constituent unit may be derived from an acrylate with an alkyl ester moiety having two or more carbon atoms constitutes 8% or less by mass of the graft polymer layer (A2), the graft copolymer particles (B) may contain a cross-linked elastomer (B1).
-
公开(公告)号:US20230416556A1
公开(公告)日:2023-12-28
申请号:US18241465
申请日:2023-09-01
Applicant: KANEKA CORPORATION
Inventor: Hanako Hasebe , Haruki Koyama , Yukihiro Shimamoto
IPC: C09D133/18 , B05D1/00 , C08K3/36
CPC classification number: C09D133/18 , B05D1/00 , B05D2502/00 , B05D2201/04 , C08K3/36
Abstract: A laminate having excellent moldability and including an acrylic-based resin film is provided. A method for producing a laminate having a specific crack elongation, includes a step (A) of forming, on at least one side of a specific acrylic-based resin film, a hard coat layer that contains a urethane acrylate resin, and a step (B) of forming, on the hard coat layer obtained in the step (A), a low refractive index layer that contains, in an amount of not less than 40%, hollow fine silica particles having a particle size of less than 100 nm and that contains an acrylate-based resin.
-
公开(公告)号:US20230340218A1
公开(公告)日:2023-10-26
申请号:US18340504
申请日:2023-06-23
Applicant: KANEKA CORPORATION
Inventor: Haruki Koyama , Hanako Hasebe , Yukihiro Shimamoto
CPC classification number: C08J7/046 , C08J7/0427 , C08J2333/04 , C08J2375/14
Abstract: Provided is a laminate that has excellent moldability and excellent wear resistance, and that contains an acrylic-based resin film. Excellent mouldability and wear resistance can be attained by providing a laminate including a specific acrylic-based resin film, and a specific ultraviolet-curable hard coat layer that is laminated on at least one side of the acrylic-based resin film. The laminate has a specific crack elongation and exhibits a Δhaze of not more than 1.0% in a steel wool wear test at 50 g/cm2 and 5 reciprocating motions.
-
4.
公开(公告)号:US20210002437A1
公开(公告)日:2021-01-07
申请号:US17023904
申请日:2020-09-17
Applicant: KANEKA CORPORATION
Inventor: Haruki Koyama , Hanako Hasebe , Katsumi Yamaguchi , Yukihiro Shimamoto
IPC: C08J5/18 , C08L51/04 , B32B27/08 , C08F265/06 , B32B27/30 , C08J7/046 , C08F285/00
Abstract: An acrylic resin film is provided that may include graft copolymer particles (A) with a multilayer structure and graft copolymer particles (B) with a multilayer structure, wherein the graft copolymer particles (A) may have an average particle size in the range of 20 to 150 nm, the graft copolymer particles (B) may have a larger average particle size than the graft copolymer particles (A). The graft copolymer particles (A) may include a cross-linked elastomer (A1) and a graft polymer layer (A2), the graft polymer layer (A2) being closer to a surface layer than the cross-linked elastomer (A1). Further, a constituent unit may be derived from an acrylate with an alkyl ester moiety having two or more carbon atoms constitutes 8% or less by mass of the graft polymer layer (A2), the graft copolymer particles (B) may contain a cross-linked elastomer (B1).
-
-
-