公开(公告)号:EP2799491A4
公开(公告)日:2015-08-19
申请号:EP12861739
申请日:2012-12-20
Applicant: KAO CORP
Inventor: MORI MASAHIRO , KONISHI MOTOI , KIMURA AKIYOSHI , FUJIOKA MASAHIRO , MUKAI KENTA , KUMAMOTO YOSHIAKI
CPC classification number: C08L67/04 , B29C45/0001 , B29C45/0005 , B29C47/0004 , B29C47/0054 , B29K2001/08 , B29K2067/046 , B29K2105/0088 , C08B15/06 , C08J5/045 , C08J2367/04 , C08L1/02 , C08L1/08 , C08L2201/08 , C08L2201/10 , C08L2205/06 , C08L2205/16 , Y10T428/298
Abstract: A polyester resin composition containing a polyester resin, and a fine cellulose fiber composite having an average fiber diameter of from 0.1 to 200 nm, wherein the fine cellulose fiber composite contains fine cellulose fibers and hydrocarbon groups being connected thereto via an amide bond. The polyester resin composition of the present invention can be worked into a molded article by thermoforming or injection-molding, and is suitably used for various industrial applications, such as daily sundries, household electric appliance parts, packaging materials for household electric appliance parts, and automobile parts. In addition, the fine cellulose fiber composite has high dispersibility against various resins and can exhibit thickening effects, so that it is suitable as various thickeners or the like.
-
公开(公告)号:JP2013216998A
公开(公告)日:2013-10-24
申请号:JP2012090108
申请日:2012-04-11
Inventor: FUJIOKA MASAHIRO , KIMURA AKIKATSU , KONISHI MOTOI
IPC: D06M13/328 , D06M11/30 , D06M13/322 , D06M23/00
Abstract: PROBLEM TO BE SOLVED: To provide a surface-modified cellulose microfiber that has a high dispersibility regardless of the polarity of a solvent and is capable of developing a thickening effect.SOLUTION: A method for producing a surface-modified cellulose microfiber includes the steps of: oxidizing a natural cellulose fiber in the presence of a N-oxyl compound to obtain a cellulose microfiber containing a carboxyl group; and reacting the cellulose microfiber containing a carboxyl group with a primary or secondary amine having a 1-4C hydrocarbon group. The surface-modified cellulose microfiber has an average fiber diameter of 0.5-200 nm and is obtained by linking a 1-4C hydrocarbon group through an amide bond.
Abstract translation: 要解决的问题:提供一种具有高分散性的表面改性纤维素微纤维,与溶剂的极性无关,并且能够产生增稠效果。解决方案:一种表面改性纤维素微纤维的制造方法,包括以下步骤: :在N-氧基化合物存在下氧化天然纤维素纤维,得到含有羧基的纤维素微纤维; 并使含有羧基的纤维素微纤维与具有1-4C烃基的伯胺或仲胺反应。 表面改性的纤维素微纤维的平均纤维直径为0.5-200nm,通过使酰胺键连接1-4C的烃基而获得。
-
公开(公告)号:JP2013151636A
公开(公告)日:2013-08-08
申请号:JP2012152644
申请日:2012-07-06
Inventor: KONISHI MOTOI , KIMURA AKIKATSU , FUJIOKA MASAHIRO , MUKAI KENTA , KUMAMOTO YOSHIAKI
CPC classification number: C08L67/04 , B29C45/0001 , B29C45/0005 , B29C47/0004 , B29C47/0054 , B29K2001/08 , B29K2067/046 , B29K2105/0088 , C08B15/06 , C08J5/045 , C08J2367/04 , C08L1/02 , C08L1/08 , C08L2201/08 , C08L2201/10 , C08L2205/06 , C08L2205/16 , Y10T428/298
Abstract: PROBLEM TO BE SOLVED: To provide a polyester resin composition having good transparency and excellent mechanical strength, and placing few load on the environment.SOLUTION: There is provided a polyester resin composition comprising a polyester resin and a fine cellulose fiber composite having a mean fiber diameter of 0.1-200 nm, preferably 0.2-100 nm, and formed by joining a hydrocarbon group, preferably a 1C hydrocarbon group or a 2-30C saturated or unsaturated, linear or branched hydrocarbon group, to a fine cellulose fiber by amide bonding.
Abstract translation: 要解决的问题:提供一种具有良好的透明性和优异的机械强度并且对环境施加很少负载的聚酯树脂组合物。解决方案:提供一种聚酯树脂组合物,其包含聚酯树脂和具有平均纤维的细纤维素纤维复合材料 直径为0.1-200nm,优选为0.2-100nm,并通过酰胺键将烃基,优选1C烃基或2-30C饱和或不饱和直链或支链烃基与细纤维素纤维接合而形成。
-
公开(公告)号:JP2013151661A
公开(公告)日:2013-08-08
申请号:JP2012277750
申请日:2012-12-20
Inventor: KONISHI MOTOI , KIMURA AKIKATSU , FUJIOKA MASAHIRO , MORI MASAHIRO
Abstract: PROBLEM TO BE SOLVED: To provide a polyester resin composition having good transparency and excellent mechanical strength, and placing few load on the environment.SOLUTION: There is provided a polyester resin composition comprising a polyester resin, and a fine cellulose fiber composite having a mean fiber diameter of 0.1-200 nm, preferably 0.2-100 nm and formed by joining a hydrocarbon group, preferably a 1C hydrocarbon group or a 2-30C saturated or unsaturated, linear or branched hydrocarbon group to a fine cellulose fiber by amide bonding.
Abstract translation: 要解决的问题:提供一种具有良好的透明性和优异的机械强度并且在环境中施加很少负载的聚酯树脂组合物。解决方案:提供一种聚酯树脂组合物,其包含聚酯树脂和具有平均值的细纤维素纤维复合材料 纤维直径为0.1-200nm,优选为0.2-100nm,并通过酰胺键将烃基,优选1C烃基或2-30C饱和或不饱和直链或支链烃基与细纤维素纤维接合而形成。
-
-
-