公开(公告)号:JPH10218621A
公开(公告)日:1998-08-18
申请号:JP30884997
申请日:1997-11-11
Applicant: KOREA ELECTRONICS TELECOMM
Inventor: SOON-HO CHAN , KI HO JAN , SEON-GU KAN , KWAN-SUN RYU
IPC: C01G39/00 , H01M4/02 , H01M4/04 , H01M4/131 , H01M4/136 , H01M4/48 , H01M4/485 , H01M4/58 , H01M10/05 , H01M10/052 , H01M10/40
Abstract: PROBLEM TO BE SOLVED: To enable the increase in the cell capacity and life prolongation of vanadium oxide based battery by mixing MoO3 with vanadium oxide in a dried chamber, enclosing the mixture in a silica tube and vacuum-sealing the tube and treating the vacuum-sealed mixture with heat. SOLUTION: MoO3 and vanadium oxide are quantitatively mixed in a dried argon atmosphere to prepare a mixture. The mixture is charged in a silica tube, vacuum-sealed, and heat-treated at 630-670 deg.C for 96-120 hours to prepare a vanadium oxide of the formula: Moy V2-y O5 ((y) is 0