公开(公告)号:EP0315566B1
公开(公告)日:1993-06-16
申请号:EP88630186.0
申请日:1988-11-03
Applicant: LANXIDE TECHNOLOGY COMPANY, LP.
Inventor: Dwivedi, Ratneshi Kumar , Irick, Virgil, Jr.
CPC classification number: B22D19/00 , F05C2251/042 , Y10T29/49984 , Y10T428/131 , Y10T428/249987 , Y10T428/31678
-
公开(公告)号:EP0315566A3
公开(公告)日:1989-10-18
申请号:EP88630186.0
申请日:1988-11-03
Applicant: LANXIDE TECHNOLOGY COMPANY, LP.
Inventor: Dwivedi, Ratneshi Kumar , Irick, Virgil, Jr.
CPC classification number: B22D19/00 , F05C2251/042 , Y10T29/49984 , Y10T428/131 , Y10T428/249987 , Y10T428/31678
Abstract: This invention relates to a new ceramic-metal composite body and a method for producing the same. Particularly, a compliant layer composition is utilized for preventing the rupture of a ceramic article (1) and/or the yielding or failure of a metal during the pouring, solidification and cooling of a molten metal which has been cast around the ceramic. A slurry composition for the compliant layer (2) includes plaster of paris, a liquid vehicle and a filler material. The slurry composition is coated on the ceramic article (1) and thereafter is heat-treated to form a compliant layer (2). Ceramic-metal composite bodies comprising low strength hollow articles and high expansion coefficient metals may be manufactured according to the method of this invention.
-
公开(公告)号:EP0315566A2
公开(公告)日:1989-05-10
申请号:EP88630186.0
申请日:1988-11-03
Applicant: LANXIDE TECHNOLOGY COMPANY, LP.
Inventor: Dwivedi, Ratneshi Kumar , Irick, Virgil, Jr.
CPC classification number: B22D19/00 , F05C2251/042 , Y10T29/49984 , Y10T428/131 , Y10T428/249987 , Y10T428/31678
Abstract: This invention relates to a new ceramic-metal composite body and a method for producing the same. Particularly, a compliant layer composition is utilized for preventing the rupture of a ceramic article (1) and/or the yielding or failure of a metal during the pouring, solidification and cooling of a molten metal which has been cast around the ceramic. A slurry composition for the compliant layer (2) includes plaster of paris, a liquid vehicle and a filler material. The slurry composition is coated on the ceramic article (1) and thereafter is heat-treated to form a compliant layer (2). Ceramic-metal composite bodies comprising low strength hollow articles and high expansion coefficient metals may be manufactured according to the method of this invention.
Abstract translation: 本发明涉及一种新的陶瓷 - 金属复合体及其制造方法。 特别地,柔性层组合物用于在铸造在陶瓷周围的熔融金属的浇注,固化和冷却期间防止陶瓷制品(1)的破裂和/或金属的产生或破坏。 用于柔顺层(2)的浆料组合物包括石膏,液体载体和填充材料。 将浆料组合物涂布在陶瓷制品(1)上,然后进行热处理以形成柔顺层(2)。 可以根据本发明的方法制造包括低强度中空制品和高膨胀系数金属的陶瓷 - 金属复合体。
-
-