公开(公告)号:FR2535727B1
公开(公告)日:1986-11-14
申请号:FR8317483
申请日:1983-11-03
Applicant: MITSUI TOATSU CHEMICALS
Inventor: MATSUBARA TETSUYUKI , ITO NORIFUMI , ICHIKAWA KOUZO , ARAHARI KOUICHI , MAEDA TETSUO
IPC: C08F2/00 , C08F2/02 , C08F2/04 , C08F20/00 , C08F20/42 , C08F279/04 , C08F291/00 , C08F291/02
Abstract: In a continuous bulk or solution polymerization process for producing rubber modified high-impact resins which comprises continuously feeding a raw material solution comprising a mixture of an aromatic vinyl monomer and a vinyl cyanide monomer and a rubber component dissolved in the mixture, together with a radical polymerization initiator, to a first reactor, polymerizing the raw material solution under high-shear agitation to a conversion required to transform the rubber component phase into dispersed particles, withdrawing the reaction mixture continuously from the first reactor at a rate corresponding to the feed rate of the raw material solution, and feeding the reaction mixture to a second or more reactors for further polymerization, rubber modified high-impact resins exhibiting excellent chemical resistance, thermal resistance and rigidity and having a good surface gloss can be produced by properly determining the weight ratio of the aromatic vinyl monomer to the vinyl cyanide monomer present in the raw material solution, the content of the rubber component in the raw material solution, the content of the solvent in the raw material solution, the property of the rubber component, the property of the radical polymerization initiator and the amount of initiator used, as well as the conversion of the monomers at the first reactor.
-
公开(公告)号:GB2129433B
公开(公告)日:1986-09-24
申请号:GB8328583
申请日:1983-10-26
Applicant: MITSUI TOATSU CHEMICALS , TOYO ENGINEERING CORP
Inventor: MATSUBARA TETSUYUKI , ITO NORIFUMI , ICHIKAWA KOUZO , ARAHARI KOUICHI , MAEDA TETSUO
IPC: C08F2/00 , C08F2/02 , C08F2/04 , C08F20/00 , C08F20/42 , C08F279/04 , C08F291/00 , C08F291/02
Abstract: In a continuous bulk or solution polymerization process for producing rubber modified high-impact resins which comprises continuously feeding a raw material solution comprising a mixture of an aromatic vinyl monomer and a vinyl cyanide monomer and a rubber component dissolved in the mixture, together with a radical polymerization initiator, to a first reactor, polymerizing the raw material solution under high-shear agitation to a conversion required to transform the rubber component phase into dispersed particles, withdrawing the reaction mixture continuously from the first reactor at a rate corresponding to the feed rate of the raw material solution, and feeding the reaction mixture to a second or more reactors for further polymerization, rubber modified high-impact resins exhibiting excellent chemical resistance, thermal resistance and rigidity and having a good surface gloss can be produced by properly determining the weight ratio of the aromatic vinyl monomer to the vinyl cyanide monomer present in the raw material solution, the content of the rubber component in the raw material solution, the content of the solvent in the raw material solution, the property of the rubber component, the property of the radical polymerization initiator and the amount of initiator used, as well as the conversion of the monomers at the first reactor.
-
公开(公告)号:DE69405699T2
公开(公告)日:1998-04-02
申请号:DE69405699
申请日:1994-12-23
Applicant: MITSUI TOATSU CHEMICALS
-
公开(公告)号:CA2006738C
公开(公告)日:1995-09-26
申请号:CA2006738
申请日:1989-12-27
Applicant: MITSUI TOATSU CHEMICALS
Inventor: MATSUBARA TETSUYUKI , ITO NORIFUMI , IWAMOTO MUNE , SUGAZAKI KAZUO , ANDO TOSHIHIKO , FURUTA YASUO , ICHIKAWA KOUZO , OZASA HITOSHI
IPC: C08F279/02 , C08F291/02 , C08F279/04
Abstract: In a process for preparing rubber modified high impact resins (HI-PS and ABS) by polymerizing a starting monomer containing an aromatic vinyl monomer or a mixture of an aromatic vinyl monomer and a vinyl cyanide monomer and added with a rubber-like polymer and by using at least two polymerization reactors and a particle disperser placed between the both reactor, the process obtaining the resins of high grade by specifying the relationships between the concentration of the polymerized monomer in the first reactor and the content of the rubber-like polymer in the first reactor and between the volume occupied by the polyemrizing liquid in the first reactor and the inner volume of the particle disperser, and the peripheral linear velocity of a shearing stirrer in the particle disperser.
-
公开(公告)号:CA2006738A1
公开(公告)日:1990-06-28
申请号:CA2006738
申请日:1989-12-27
Applicant: MITSUI TOATSU CHEMICALS
Inventor: MATSUBARA TETSUYUKI , ITO NORIFUMI , IWAMOTO MUNE , SUGAZAKI KAZUO , ANDO TOSHIHIKO , FURUTA YASUO , ICHIKAWA KOUZO , OZASA HITOSHI
IPC: C08F279/02 , C08F291/02
Abstract: In a process for preparing rubber modified high impact resins (HI-PS and ABS) by polymerizing a starting monomer containing an aromatic vinyl monomer or a mixture of an aromatic vinyl monomer and a vinyl cyanide monomer and added with a rubber-like polymer and by using at least two polymerization reactors and a particle disperser placed between the both reactor, the process obtaining the resins of high grade by specifying the relationships between the concentration of the polymerized monomer in the first reactor and the content of the rubber-like polymer in the first reactor and between the volume occupied by the polyemrizing liquid in the first reactor and the inner volume of the particle disperser, and the peripheral linear velocity of a shearing stirrer in the particle disperser.
-
公开(公告)号:IN161945B
公开(公告)日:1988-03-05
申请号:IN1338CA1983
申请日:1983-10-29
Applicant: MITSUI TOATSU CHEMICALS , TOYO ENGINEERING CORP
Inventor: MATSUBARA TETSUYUKI , ITO NORIFUMI , ICHIKAWA KOUZO , ARAHARI KOUICHI , MAEDA TETSUO
IPC: C08F2/00 , C08F2/02 , C08F2/04 , C08F20/00 , C08F20/42 , C08F279/04 , C08F291/00 , C08F291/02 , C08D1/04
Abstract: In a continuous bulk or solution polymerization process for producing rubber modified high-impact resins which comprises continuously feeding a raw material solution comprising a mixture of an aromatic vinyl monomer and a vinyl cyanide monomer and a rubber component dissolved in the mixture, together with a radical polymerization initiator, to a first reactor, polymerizing the raw material solution under high-shear agitation to a conversion required to transform the rubber component phase into dispersed particles, withdrawing the reaction mixture continuously from the first reactor at a rate corresponding to the feed rate of the raw material solution, and feeding the reaction mixture to a second or more reactors for further polymerization, rubber modified high-impact resins exhibiting excellent chemical resistance, thermal resistance and rigidity and having a good surface gloss can be produced by properly determining the weight ratio of the aromatic vinyl monomer to the vinyl cyanide monomer present in the raw material solution, the content of the rubber component in the raw material solution, the content of the solvent in the raw material solution, the property of the rubber component, the property of the radical polymerization initiator and the amount of initiator used, as well as the conversion of the monomers at the first reactor.
-
公开(公告)号:IT1169921B
公开(公告)日:1987-06-03
申请号:IT2357983
申请日:1983-11-03
Applicant: MITSUI TOATSU CHEMICALS , TOYO ENGINEERING CORP
Inventor: MATSUBARA TETSUYUKI , ITO NORIFUMI , ICHIKAWA KOUZO , ARAHARI KOUICHI , MAEDA TETSUO
IPC: C08F2/00 , C08F2/02 , C08F2/04 , C08F20/00 , C08F20/42 , C08F279/04 , C08F291/00 , C08F291/02 , C08F
Abstract: In a continuous bulk or solution polymerization process for producing rubber modified high-impact resins which comprises continuously feeding a raw material solution comprising a mixture of an aromatic vinyl monomer and a vinyl cyanide monomer and a rubber component dissolved in the mixture, together with a radical polymerization initiator, to a first reactor, polymerizing the raw material solution under high-shear agitation to a conversion required to transform the rubber component phase into dispersed particles, withdrawing the reaction mixture continuously from the first reactor at a rate corresponding to the feed rate of the raw material solution, and feeding the reaction mixture to a second or more reactors for further polymerization, rubber modified high-impact resins exhibiting excellent chemical resistance, thermal resistance and rigidity and having a good surface gloss can be produced by properly determining the weight ratio of the aromatic vinyl monomer to the vinyl cyanide monomer present in the raw material solution, the content of the rubber component in the raw material solution, the content of the solvent in the raw material solution, the property of the rubber component, the property of the radical polymerization initiator and the amount of initiator used, as well as the conversion of the monomers at the first reactor.
-
公开(公告)号:IN161868B
公开(公告)日:1988-02-13
申请号:IN397CA1985
申请日:1985-05-24
Applicant: MITSUI TOATSU CHEMICALS , TOYO ENGINEERING CORP
Inventor: MATSUBARA TETSUYUKI , ITO NORIFUMI , SUGAZAKI KAZUO , ICHIKAWA KOUZO , IWAMOTO MUNE , ANDO TOSHIHIKO
Abstract: A process for producing a styrene-base resin having improved moldability and a good hue by continuously adding a specific higher fatty acid amide in a dissolved or molten state, and/or a mixture of a specific higher fatty acid amide and a specific metallic soap in a molten state, to a styrene-base resin in the course of its production by continuous bulk or solution polymerization. The above process is particularly effective for rubber-modified styrene-acrylonitrile resins.
-
公开(公告)号:CA1221786A
公开(公告)日:1987-05-12
申请号:CA440358
申请日:1983-11-03
Applicant: MITSUI TOATSU CHEMICALS , TOYO ENGINEERING CORP
Inventor: MATSUBARA TETSUYUKI , ITO NORIFUMI , ICHIKAWA KOUZO , ARAHARI KOUICHI , MAEDA TETSUO
IPC: C08F2/00 , C08F2/02 , C08F2/04 , C08F20/00 , C08F20/42 , C08F279/04 , C08F291/00 , C08F291/02
Abstract: SPECIFICATION Title of the Invention CONTINUOUS PROCESS FOR PRODUCING RUBBER MODIFIED HIGH-IMPACT RESINS In a continuous bulk or solution polymerization process for producing rubber modified high-impact resins which comprises continuously feeding a raw material solution comprising a mixture of an aromatic vinyl monomer and a vinyl cyanide monomer and a rubber component dissolved in the mixture, together with a radical polymerization initiator, to a first reactor, polymerizing the raw material solution under high-shear agitation to a conversion required to transform the rubber component phase into dispersed particles, withdrawing the reaction mixture continuously from the first reactor at a rate corresponding to the feed rate of the raw material solution, and feeding the reaction mixture to a second or more reactors for further polymerization, rubber modified high-impact resins exhibiting excellent chemical resistance, thermal resistance and righdity and having a good surface gloss can be produced by properly determining the weight ratio of the aromatic vinyl monomer to the vinyl cyanide monomer present in the raw material solution, the content of the rubber component in the raw material solution, the content of the solvent in the raw material solution, the property of the rubber component, the property of the radical polymerization initiator and the amount of initiator used, as well as the conversion of the monomers at the first reactor.
-
公开(公告)号:DE69405699D1
公开(公告)日:1997-10-23
申请号:DE69405699
申请日:1994-12-23
Applicant: MITSUI TOATSU CHEMICALS
-
-
-
-
-
-
-
-
-