公开(公告)号:US11834576B2
公开(公告)日:2023-12-05
申请号:US17385918
申请日:2021-07-27
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Te-Chao Liao , Sen-Huang Hsu , Chung-Chi Su
IPC: C08L67/06 , C08G63/183 , C08G63/21 , C08F12/08 , C08F220/20 , C08F220/10 , C08F222/10
CPC classification number: C08L67/06 , C08F12/08 , C08F220/20 , C08F222/102 , C08G63/183 , C08G63/21 , C08L2201/08 , C08L2203/30
Abstract: An unsaturated polyester resin composition with low styrene volatility and a molding article thereof are provided. The unsaturated polyester resin composition of includes: 30 to 60 parts by weight of unsaturated polyester resin and 2 to 30 parts by weight of comonomer, and the comonomer includes: (a) methyl styrene, (b) hydroxy acrylate monomer and (c) diallyl phthalate monomer, and the weight ratio of the content (a), (b), and (c) is 6:3:1 in the comonomer.
-
公开(公告)号:US20230073082A1
公开(公告)日:2023-03-09
申请号:US17499889
申请日:2021-10-13
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Te-Chao Liao , Jung-Jen Chuang , Zhang-Jian Huang , Chung-Chi Su
IPC: D06M13/192 , B01D39/10 , D06M13/188 , C08J11/26 , C08J11/16
Abstract: Provided is a recycling method of polyester wool blended fabric, which includes the following. A polyester wool blended fabric containing a dye is put into an acidic aqueous solution containing an oxidizing agent for heating and soaking, so as to degrade a wool in the polyester wool blended fabric, and perform decolorization at the same time to remove the dye. After that, a polyester fabric is obtained by filtration.
-
公开(公告)号:US20250066968A1
公开(公告)日:2025-02-27
申请号:US18472250
申请日:2023-09-22
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Te-Chao Liao , Jung-Jen Chuang , Chung-Chi Su
Abstract: A method for degumming and decolorizing polyester fabrics is provided. The method includes the following steps. A first polyester fabric attached with a dye and a gum-film or treatment agent is provided. The gum-film or treatment agent in the first polyester fabric is stripped through a combined formulation of an alkaline aqueous solution and a catalyst to obtain a second polyester fabric. Then, the second polyester fabric is decolorized by a combination of a chemical reduction method and a chemical oxidation method to obtain a third polyester fabric.
-
公开(公告)号:US11702503B2
公开(公告)日:2023-07-18
申请号:US17007031
申请日:2020-08-31
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Te-Chao Liao , Sen-Huang Hsu , Chung-Chi Su , Chuan Chou , Jui-Jung Lin
CPC classification number: C08G59/5013 , C08G59/4276 , C08G65/002 , C08G65/34 , C08L71/08
Abstract: A curing agent and method for producing the same are provided, the method includes: esterification reaction: reacting a polyhydric alcohol with a polybasic acid anhydride to obtain an ester-based emulsifier (A); chain extension reaction: reacting an ester-based emulsifier (A) with a bifunctional epoxy resin to obtain a polymer intermediate (B); and reacting the polymer intermediate (B) with a polyamine compound to obtain a curing agent (C).
-
公开(公告)号:US20230082196A1
公开(公告)日:2023-03-16
申请号:US17721339
申请日:2022-04-14
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Te-Chao Liao , Jung-Jen Chuang , Zhang-Jian Huang , Chung-Chi Su
IPC: D06M13/188 , D06P5/13
Abstract: Provided is a recycling method of a polyester cotton blended fabric, including the following steps. A dye-containing polyester cotton blended fabric is put into an acidic aqueous solution containing an oxidizing agent for heating and soaking, so as to degrade the cotton in the polyester cotton blended fabric into powder, and decolorization is performed at the same time to remove the dye. After that, a polyester fabric and cotton powder are obtained by double filtration.
-
公开(公告)号:US11767391B2
公开(公告)日:2023-09-26
申请号:US16887006
申请日:2020-05-29
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Te-Chao Liao , Sen-Huang Hsu , Chung-Chi Su , Chuan Chou , Jui-Jung Lin
IPC: C08F283/01 , C09D167/00 , C08G63/91 , C08G63/685 , C08G59/50 , C08G59/40 , C08G63/68 , C08G59/56 , C08G59/18 , C08G59/42 , C08K3/08 , C09D167/02 , C08L63/00 , C08L67/02 , C08L67/00 , C09D5/10 , C09D163/00 , C09D7/63
CPC classification number: C08F283/01 , C09D167/00 , C08G59/18 , C08G59/184 , C08G59/40 , C08G59/4014 , C08G59/42 , C08G59/4276 , C08G59/50 , C08G59/5013 , C08G59/56 , C08G63/68 , C08G63/685 , C08G63/6854 , C08G63/6856 , C08G63/91 , C08G63/914 , C08G63/916 , C08K2003/0812 , C08K2003/0893 , C08L63/00 , C08L67/00 , C08L67/02 , C09D5/10 , C09D5/103 , C09D5/106 , C09D7/63 , C09D163/00 , C09D167/02 , C09D163/00 , C08K3/08 , C08K5/06 , C08K5/5435
Abstract: A curing agent composition and a curing agent coating formula thereof are provided. The curing agent composition includes 5 to 25 wt % of an ester group-containing amine end group adduct, 2 to 25 wt % of a C8-C22 hydrophobic saturated or unsaturated fatty amine, 2 to 25 wt % of a polyamine compound, 2 to 20 wt % of a silane compound, and 10 to 60 wt % of an ether solvent.
-
公开(公告)号:US11168198B2
公开(公告)日:2021-11-09
申请号:US16678895
申请日:2019-11-08
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Te-Chao Liao , Chung-Chi Su , Chia-Sheng Lai
Abstract: A recycled polyester fiber is provided. The recycled polyester fiber is made of a raw material by melt spinning. The raw material includes 95.0 wt % to 99.99 wt % recycled polyester pellet formed from recycled bottle chip and 0.01 wt % to 5.0 wt % titanium dioxide slurry. Based on the total weight of the titanium dioxide slurry, the titanium dioxide slurry includes 20 wt % to 50 wt % bio-oil acting as carrier, 50 wt % to 80 wt % titanium dioxide powder, 0.1 wt % to 5 wt % dispersant, 0.01 wt % to 3 wt % antioxidant, and 0.001 wt % to 0.1 wt % dye.
-
-
-
-
-
-