1.
公开(公告)号:US20170283329A1
公开(公告)日:2017-10-05
申请号:US15509825
申请日:2014-09-09
Applicant: NANJING TECH UNIVERSITY
Inventor: Weihong Xing , Zhaoxiang Zhong , Feng HAN , Feng ZHANG , Nanping XU
IPC: C04B35/80 , C04B35/634 , C04B38/00 , C04B35/64 , C04B38/06 , C04B35/63 , C04B35/632
CPC classification number: C04B35/806 , C04B35/565 , C04B35/62615 , C04B35/62685 , C04B35/6303 , C04B35/632 , C04B35/63416 , C04B35/64 , C04B38/0003 , C04B38/0006 , C04B38/067 , C04B38/068 , C04B2235/3244 , C04B2235/3826 , C04B2235/422 , C04B2235/5244 , C04B2235/5276 , C04B2235/5427 , C04B2235/5436 , C04B2235/6021 , C04B2235/6562
Abstract: A preparation method of a SiC porous ceramic material and porous ceramic material manufactured by using the method, comprising: mixing a SiC aggregate, a sintering aid (zirconium oxide), a pore-forming agent (activated carbon) and a polymer binder with a reinforcing agent (SiC whiskers) according to a certain proportion, and obtaining a porous ceramic material via forming, drying and high-temperature sintering. The porous ceramic material has a high strength, a high porosity, a good thermal shock resistance and a low sintering temperature, and can server as a filter material of high-temperature flue gas and a carrier material in vehicle exhaust purification.
-
公开(公告)号:US20190211175A1
公开(公告)日:2019-07-11
申请号:US16099182
申请日:2017-06-30
Applicant: NANJING TECH UNIVERSITY
Inventor: Yong WANG , Weihong XING , Nanping XU
CPC classification number: C08J9/28 , C08J9/00 , C08J2201/0502 , C08J2201/0504 , C08J2205/042 , C08J2381/06 , C08J2387/00 , C08J2471/02 , C08L81/06 , C08L2203/14
Abstract: The present invention relates to a method for preparing nanoporous polysulfone-based polymers, including: a copolymer of a polysulfone polymer and a polar polymer is immersed into a compound swelling agent, and maintained for at least 1 minute above room temperature; the compound swelling agent is a “solvent pair” composed of the mixture of solvent A and solvent B; the solvent A has high affinity with the polysulfone polymer; and the solvent B has high affinity with the polar polymer; the treated copolymer is taken out from the compound swelling agent and then dried to remove the solvent to obtain the nanoporous polysulfone-based polymers.
-