Abstract:
A steel for high-strength spring has an Ac 3 transformation temperature as an indicator of the decarburization performance, which is calculated by Equation (1) below, is from 859 to 885°C, a maximum hardened diameter DI as an indicator of the hardening performance, which is calculated by Equation (2) below, is from 70 to 238 mm, and a temper hardness HRC as an indicator of the spring performance, which is calculated by Equation (3) below, is from 50 to 55. wherein, D 0 = 8.65 × C , f Si =1+0.64×Si, f Mn =1+4.10×%Mn, f P =1+2.83×%P, f S =1-0.62×%S, f Cu =1+0.27×%Cu, f Ni =1+0.52×%Ni, and f Cr =1+2.33×%Cr.
Abstract:
The reflection portion 20 of the reflection member 1 is moved along the inner surface in the hole of the pipe W from the entrance opening of the hole of the pipe W to the exit opening of the hole thereof. In this case, the reflection portion 20 is guided by the guide portion 30 provided at both sides of the reflection portion 20. The shots, which are projected toward the inner surface in the hole of the pipe W, reach the reflection portion 20 through the holes of the guide portion 30 of the entrance side, and they are reflected toward the inner surface in the hole of the pipe W. Since the shots can be reflected toward the inner surface inside in the hole of the pipe W, the tendency that shots may be moved toward the inner surface outside in the hole of the curved portion P can be small. Therefore, since thinning of the wall of the pipe W can be performed, the pipe W can be strong, and the weight reduction of the pipe W can be simultaneously performed. As a result, the workability and the versatility can be improved, and the reflection member 1 can be easily used on the inner surface in the hole of the pipe having the curved portion.
Abstract:
A steel for high-strength spring has an Ac 3 transformation temperature as an indicator of the decarburization performance, which is calculated by Equation (1) below, is from 859 to 885°C, a maximum hardened diameter DI as an indicator of the hardening performance, which is calculated by Equation (2) below, is from 70 to 238 mm, and a temper hardness HRC as an indicator of the spring performance, which is calculated by Equation (3) below, is from 50 to 55.
wherein, D 0 = 8.65 × C , f Si =1+0.64×Si, f Mn =1+4.10×%Mn, f P =1+2.83×%P, f S =1-0.62×%S, f Cu =1+0.27×%Cu, f Ni =1+0.52×%Ni, and f Cr =1+2.33×%Cr.
Abstract translation:一种用于高强度弹簧钢具有Ac3相变温度如在脱碳性能的指标,在所有这是由方程(1)的下方,是从859至885℃的最大硬化直径DI计算为硬化的指示器 这是由方程计算性能,在所有(2)所示,是从70至238毫米,和回火硬度HRC如弹簧性能,所有的指示器,其由等式(3)计算的下方,为50〜55 worin, D 0 = 8.65×C,硅F = 1 + 0.64×硅,锰= F 1 + 4.10×%的Mn,P F = 1 + 2.83×%S = F×1-0.62%S,F的Cu P,= 1 + 0:27×%铜,镍F = 1 + 0:52×%的Ni,及Cr F = 1 + 2:33×%的Cr。