公开(公告)号:CA2011683A1
公开(公告)日:1990-10-03
申请号:CA2011683
申请日:1990-03-07
Applicant: PHILLIPS PETROLEUM COMPANY
Inventor: BAILEY, FAY W. , RYAN, CHARLES L. JR.
IPC: B29C49/00 , B29C49/64 , B29K81/00 , B29L22/00 , B65D1/00 , C08G75/02 , C08G75/0209 , C08G75/0277 , C08G75/06 , C08K3/34 , C08L81/02
Abstract: Articles are blow-molded from a polyphenylene sulfide resin having a melt flow in a range of from about 1 to about 10 g/10 min., and preferably in a range of from about 4 to about 8 g/10 min. When filler materials such as mica are added, the upper end of the acceptable melt flow range is raised to about 15 g/10 min. By maintaining mold temperatures in a range of from about 250 DEG to about 400 DEG F., and preferably from about 275 DEG to about 325 DEG F., the polyphenylene sulfide material in the blow-molded article is provided with a semi-crystalline structure, and is dimensionally stable at temperatures of at least 500 DEG F. Filler materials are preferably provided in a range of from about 10 to about 20 weight percent.