Abstract:
Spalling of coke produced during the thermal cracking of hydrocarbon is promoted by contacting or treating the tubes of a thermal cracking furnace with a composition having an absence of silicon and comprising tin.
Abstract:
The energy required to achieve a given conversion in the thermal cracking of hydrocarbons is reduced by contacting or treating the tubes of a thermal cracking furnace with a composition comprising tin and silicon.
Abstract:
The rate of formation of carbon on the surfaces of thermal cracking tubes and the production of carbon monoxide during thermal cracking of hydrocarbons are inhibited by the use of cracking tubes treated with an antifoulant, including tin compound, silicon compound and sulfur compounds in the presence of a reducing gas such as hydrogen. Additionally, the concentration of carbon monoxide in a pyrolytic cracking process product stream is reduced by the treatment of the thermal cracking tubes of such process with a reducing gas having a concentration of a sulfur compound.
Abstract:
The incremental yield of hydrocarbons having five or more carbon atoms in a cracked product from a thermal cracking process is increased by contacting or treating the tubes of a thermal cracking furnace with a composition comprising tin and silicon.
Abstract:
The rate of formation of carbon on the surfaces of thermal cracking tubes and the production of carbon monoxide during thermal cracking of hydrocarbons are inhibited by the use of cracking tubes treated with an antifoulant, including tin compound, silicon compound and sulfur compounds in the presence of a reducing gas such as hydrogen. Additionally, the concentration of carbon monoxide in a pyrolytic cracking process product stream is reduced by the treatment of the thermal cracking tubes of such process with a reducing gas having a concentration of a sulfur compound.
Abstract:
The rate of formation of carbon on the surfaces of thermal cracking tubes and the production of carbon monoxide during thermal cracking of hydrocarbons are inhibited by the use of cracking tubes treated with an antifoulant, including tin compound, silicon compound and sulfur compounds in the presence of a reducing gas such as hydrogen. Additionally, the concentration of carbon monoxide in a pyrolytic cracking process product stream is reduced by the treatment of the thermal cracking tubes of such process with a reducing gas having a concentration of a sulfur compound.