公开(公告)号:US09187370B2
公开(公告)日:2015-11-17
申请号:US14529843
申请日:2014-10-31
Applicant: Rockwool International A/S
Inventor: Jean Marie Wilhelmus Cuypers , Andreas Leismann , Stuart Lambie
CPC classification number: C04B14/46 , B02C19/18 , C03B3/02 , C03C1/02 , C03C13/06 , C03C2213/00 , C04B16/04 , C04B18/026 , C04B28/02 , Y02P20/582 , Y10T428/2982
Abstract: The invention relates to a method of making a particulate material comprising; providing mineral wool base material in a form having size at least 80% not more than 40 mm, subjecting the mineral wool base material to sintering by use of a pulse combustor and thereby forming a particulate material in the form of particles having size at least 80% not more than 20 mm. An apparatus for carrying out the method comprises means for size reduction of coherent mineral wool substrate and a reaction chamber in communication with a pulse combustor.
Abstract translation: 本发明涉及一种制备颗粒材料的方法,包括: 提供具有至少80%不大于40mm的尺寸的矿棉基材,通过使用脉冲燃烧器对矿棉基材进行烧结,从而形成尺寸至少为80的颗粒形式的颗粒材料 %不超过20毫米。 用于执行该方法的装置包括用于缩小相干矿棉衬底和与脉冲燃烧器连通的反应室的装置。
-
公开(公告)号:US20150114265A1
公开(公告)日:2015-04-30
申请号:US14529843
申请日:2014-10-31
Applicant: Rockwool International A/S
Inventor: Jean Marie Wilhelmus Cuypers , Andreas Leismann , Stuart Lambie
CPC classification number: C04B14/46 , B02C19/18 , C03B3/02 , C03C1/02 , C03C13/06 , C03C2213/00 , C04B16/04 , C04B18/026 , C04B28/02 , Y02P20/582 , Y10T428/2982
Abstract: The invention relates to a method of making a particulate material comprising; providing mineral wool base material in a form having size at least 80% not more than 40 mm, subjecting the mineral wool base material to sintering by use of a pulse combustor and thereby forming a particulate material in the form of particles having size at least 80% not more than 20 mm. An apparatus for carrying out the method comprises means for size reduction of coherent mineral wool substrate and a reaction chamber in communication with a pulse combustor.
Abstract translation: 本发明涉及一种制备颗粒材料的方法,包括: 提供具有至少80%不大于40mm的尺寸的矿棉基材,通过使用脉冲燃烧器对矿棉基材进行烧结,从而形成尺寸至少为80的颗粒形式的颗粒材料 %不超过20毫米。 用于执行该方法的装置包括用于缩小相干矿棉衬底和与脉冲燃烧器连通的反应室的装置。
-