Abstract:
PROBLEM TO BE SOLVED: To provide a particulate material having dispersilibity.SOLUTION: The particulate material is made by: adding an inorganic salt comprising an oxidized metal anion to an alumina hydrate suspension; and further adding an acidifying agent to the alumina hydrate suspension; whereby a layer of metal oxide is precipitated onto alumina hydrate particles to form the particulate material comprising metal oxide-coated alumina hydrate. The particulate material has a 500 psi compaction volume ratio of at least about 4.0 cc/cc.
Abstract:
An abrasive grain is disclosed and may include a body. The body may define a length (l), a height (h), and a width (w). In a particular aspect, the length is greater than or equal to the height and the height is greater than or equal to the width. Further, in a particular aspect, the body may include a primary aspect ratio defined by the ratio of length:height of at least about 2:1. The body may also include an upright orientation probability of at least about 50%.
Abstract:
A shaped abrasive particle including a body having a first major surface, a second major surface, and a side surface extending between the first major surface and the second major surface, wherein the body includes a sharpness-shape-strength factor (3SF) within a range between about 0.7 and about 1.7 and a Shape Index within a range between at least about 0.51 and not greater than about 0.99.
Abstract:
Una partícula abrasiva que tiene un cuerpo que incluye una primera superficie principal, una segunda superficie principal opuesta a la primera superficie principal y una superficie lateral que se extiende entre la primera superficie principal y la segunda superficie principal, de modo que la mayoría de la superficie lateral comprende una pluralidad de microcrestas. (Traducción automática con Google Translate, sin valor legal)
Abstract:
A shaped abrasive particle including a body having a first major surface, a second major surface, and a side surface extending between the first major surface and the second major surface, wherein the body includes a sharpness-shape-strength factor (3SF) within a range between about 0.7 and about 1.7 and a Shape Index within a range between at least about 0.51 and not greater than about 0.99.
Abstract:
An abrasive grain is disclosed and may include a body. The body may define a length (l), a height (h), and a width (w). In a particular aspect, the length is greater than or equal to the height and the height is greater than or equal to the width. Further, in a particular aspect, the body may include a primary aspect ratio defined by the ratio of length:height of at least about 2:1. The body may also include an upright orientation probability of at least about 50%.
Abstract:
In a particular embodiment, a particulate material includes alumina hydrate. The particulate material has a 500 psi Compaction Volume Ratio of at least about 4.0 cc/cc.
Abstract:
A composite material includes a non-polar polymer and alumina hydrate particulate. The composite material has a Heat Distortion Performance of at least about 10% relative to the non-polar polymer absent the alumina hydrate particulate. The composite material may include a coupling agent including a phosphinic acid group, a phosphonic acid group or an ester derivative thereof.