Abstract:
A coated fabric includes a reinforcement, a first coating disposed on the reinforcement, and a second coating disposed on the first coating. The first coating includes perfluoropolymer. The second coating includes perfluoropolymer and a silicone polymer in an amount in a range of 2wt% to 30wt%.
Abstract:
A grilling belt includes a flexible support having first and second major surfaces, an extruded fluoropolymer layer overlying the first major surface, and a cast or skived fluoropolymer layer overlying the extruded fluoropolymer layer. Another grilling belt can include a support having first and second major surfaces, and a first fluoropolymer film overlying the first major surface. The support can include a first fabric having a first bias angle, and a second fabric laminated to the first fabric and having a second bias angle different from the first bias angle by between 20° and 160°.
Abstract:
A cooking release material includes a layer comprising fluoropolymer. The cooking release material has a major surface having nucleation structures in a density of at least 10 per square inch. The cooking release material can include a reinforcement material, the layer coated over the reinforcement material. The cooking release material can include a second layer forming the major surface.
Abstract:
A cooking release material includes a layer comprising fluoropolymer. The cooking release material has a major surface having nucleation structures in a density of at least 10 per square inch. The cooking release material can include a reinforcement material, the layer coated over the reinforcement material. The cooking release material can include a second layer forming the major surface.
Abstract:
A coated fabric includes a reinforcement, a first coating disposed on the reinforcement, and a second coating disposed on the first coating. The first coating includes perfluoropolymer. The second coating includes perfluoropolymer and a silicone polymer in an amount in a range of 2 wt % to 30 wt %.
Abstract:
El tejido recubierto incluye un refuerzo, un primer recubrimiento dispuesto sobre el refuerzo y un segundo recubrimiento dispuesto sobre el primer recubrimiento. El primer recubrimiento incluye perfluoropolímero. El segundo recubrimiento incluye perfluoropolímero y un polímero de silicona en una cantidad en un intervalo de un 2% en peso a un 30% en peso.
Abstract:
A cooking release material includes a layer comprising fluoropolymer. The cooking release material has a major surface having nucleation structures in a density of at least 10 per square inch. The cooking release material can include a reinforcement material, the layer coated over the reinforcement material. The cooking release material can include a second layer forming the major surface.
Abstract:
A cooking release material includes a layer comprisig fhuompolymer. The cooking release material has a major sauce having nucleation suctures in a density otat lkast 10 per squreinch. The co0ki ngreleas matena can clde a rn eentte the laycr coa*ted over the enforcement material. The cooing rease matel can iClude a second layer fOrming the major surface.
Abstract:
A cooking release material includes a layer comprising fluoropolymer. The cooking release material has a major surface having nucleation structures in a density of at least 10 per square inch. The cooking release material can include a reinforcement material, the layer coated over the reinforcement material. The cooking release material can include a second layer forming the major surface.
Abstract:
A coated fabric includes a reinforcement, a first coating disposed on the reinforcement, and a second coating disposed on the first coating. The first coating includes perfluoropolymer. The second coating includes perfluoropolymer and a silicone polymer in an amount in a range of 2wt% to 30wt%.