Abstract:
An adhesive film can include a barrier layer and an adhesive layer. In an embodiment, the barrier layer can have a melting temperature of at least 230° C. and the adhesive layer having a melting temperature of no greater than 200° C. In an embodiment, an article can include the adhesive film bonded to a substrate.
Abstract:
The present disclosure is directed to laser-markable insulation material and cable or wire assemblies containing such insulation material. In certain embodiments, the laser-markable insulation material can include a fluoropolymer and an inorganic laser-markable pigment. The pigment can have a mean crystal size in a range of about 0.4 microns to about 2 microns and/or a median particle size (d50) in a range of about 0.45 microns to about 2 microns. The insulation material can exhibit improved initial and heat-aged contrast ratios without diminishing the ability of a cable or wire containing the insulation material to meet industry standards for electric-arc tracking and propagation resistance.
Abstract:
The present disclosure is directed to laser-markable insulation material and cable or wire assemblies containing such insulation material. In certain embodiments, the laser-markable insulation material can include a fluoropolymer and an inorganic laser-markable pigment. The pigment can have a mean crystal size in a range of about 0.4 microns to about 2 microns and/or a median particle size (d50) in a range of about 0.45 microns to about 2 microns. The insulation material can exhibit improved initial and heat-aged contrast ratios without diminishing the ability of a cable or wire containing the insulation material to meet industry standards for electric-arc tracking and propagation resistance.