Abstract: High modulus and high strength articles of polyvinyl-alcohol are obtained by thermoreversible gelation of a 5-50 wt.% solution of a polyvinylalcohol with an M w of 2.5 × 10⁴ to 5 × 10⁵ in water, followed by solvent removal and high stretching.Pref. gelation is obtained by cooling to a temperature of at least 40 ◊C below the gelation temperature.With this process low costs of solvent removal and regeneration are obtained.
-
公开(公告)号:ZA8606386B
公开(公告)日:1987-04-29
申请号:ZA8606386
申请日:1986-08-22
Applicant: STAMICARBON
CPC classification number: C08J5/18 , B29C55/005 , B29K2029/00 , B29K2105/0061 , C08J2329/04 , D01F6/14
-
公开(公告)号:AT48447T
公开(公告)日:1989-12-15
申请号:AT86201437
申请日:1986-08-19
Applicant: STAMICARBON
Abstract: High modulus and high strength articles of polyvinyl-alcohol are obtained by thermoreversible gelation of a 5-50 wt.% solution of a polyvinylalcohol with an M w of 2.5 × 10⁴ to 5 × 10⁵ in water, followed by solvent removal and high stretching.Pref. gelation is obtained by cooling to a temperature of at least 40 ◊C below the gelation temperature.With this process low costs of solvent removal and regeneration are obtained.
-
公开(公告)号:ZA866386B
公开(公告)日:1987-04-29
申请号:ZA866386
申请日:1986-08-22
Applicant: STAMICARBON
Abstract: High modulus and high strength articles of polyvinyl-alcohol are obtained by thermoreversible gelation of a 5-50 wt.% solution of a polyvinylalcohol with an M w of 2.5 × 10⁴ to 5 × 10⁵ in water, followed by solvent removal and high stretching.Pref. gelation is obtained by cooling to a temperature of at least 40 ◊C below the gelation temperature.With this process low costs of solvent removal and regeneration are obtained.
-
公开(公告)号:AU6165486A
公开(公告)日:1987-02-26
申请号:AU6165486
申请日:1986-08-20
Applicant: STAMICARBON
Abstract: High modulus and high strength articles of polyvinyl-alcohol are obtained by thermoreversible gelation of a 5-50 wt.% solution of a polyvinylalcohol with an M w of 2.5 × 10⁴ to 5 × 10⁵ in water, followed by solvent removal and high stretching.Pref. gelation is obtained by cooling to a temperature of at least 40 ◊C below the gelation temperature.With this process low costs of solvent removal and regeneration are obtained.
-
公开(公告)号:DE3667307D1
公开(公告)日:1990-01-11
申请号:DE3667307
申请日:1986-08-19
Applicant: STAMICARBON
Abstract: High modulus and high strength articles of polyvinyl-alcohol are obtained by thermoreversible gelation of a 5-50 wt.% solution of a polyvinylalcohol with an M w of 2.5 × 10⁴ to 5 × 10⁵ in water, followed by solvent removal and high stretching.Pref. gelation is obtained by cooling to a temperature of at least 40 ◊C below the gelation temperature.With this process low costs of solvent removal and regeneration are obtained.
-
-
-
-
-