公开(公告)号:GB2191506A
公开(公告)日:1987-12-16
申请号:GB8713199
申请日:1987-06-05
Applicant: STANADYNE INC
Inventor: BIRMAN STEPHEN P , SMITH RICHARD B , THOMPSON RICHARD L
Abstract: Stanadyne Case 239 COLD DRAWN FREE-MACHINING RESULFURIZED AND REPHOSPHORIZED STEEL BARS HAVING CONTROLLED MECHANICAL PROPERTIES AND CONTROLLED MACHINABILITY A cold drawn resulfurized and rephosphorized freemachining steel bar has the composition, by weight, C up to 0.08%; Mn 0.6% to 1.4%; Si up to 0.1%; P at least 0.03%; S 0.25% to 0.50%; Cb 0.01% to 0.10%; V up to 0.1%; the sum of Ni, Cr, Mo, and Cu up to 0.15%; balance iron. The ratio of %Mn / %S is from 1.6 to 4.0, and the ratio of (%Mn - 1.62 X %S) / %Cb is from 2 to 50. The yield strength of the steel bar is further determined by the draft in cold drawing the bar from the hot rolled state and the size and cross section of the bar after draft.
-
公开(公告)号:FR2601697A1
公开(公告)日:1988-01-22
申请号:FR8707998
申请日:1987-06-09
Applicant: STANADYNE INC
Inventor: BIRMAN STEPHEN P , SMITH RICHARD B , THOMSON RICHARD L
Abstract: Stanadyne Case 239 COLD DRAWN FREE-MACHINING RESULFURIZED AND REPHOSPHORIZED STEEL BARS HAVING CONTROLLED MECHANICAL PROPERTIES AND CONTROLLED MACHINABILITY A cold drawn resulfurized and rephosphorized freemachining steel bar has the composition, by weight, C up to 0.08%; Mn 0.6% to 1.4%; Si up to 0.1%; P at least 0.03%; S 0.25% to 0.50%; Cb 0.01% to 0.10%; V up to 0.1%; the sum of Ni, Cr, Mo, and Cu up to 0.15%; balance iron. The ratio of %Mn / %S is from 1.6 to 4.0, and the ratio of (%Mn - 1.62 X %S) / %Cb is from 2 to 50. The yield strength of the steel bar is further determined by the draft in cold drawing the bar from the hot rolled state and the size and cross section of the bar after draft.
-
公开(公告)号:FR2601696A1
公开(公告)日:1988-01-22
申请号:FR8707997
申请日:1987-06-09
Applicant: STANADYNE INC
Inventor: BIRMAN STEPHEN P , SMITH RICHARD B , THOMSON RICHARD L
Abstract: A cold drawn free-machining steel bar having a composition consisting essentially of, in weight percent, C up to 0.15; Mn 0.7 to 1.3; P 0.03 to 0.09; S 0.30 to 0.50; Bi 0.05 to 0.25; the sum of Ni, Cr, Mo and Cu up to 0.15 and the balance iron. The ratio % Mn / %S is from 1.7 to 3.0 and the %Mn-1.62x%S is from 0.05 to 0.40. The ratio %Bi /(%Ni+%Cu) is at least 2.0. The yield strength of the steel bar is further determined by the draft in cold drawing the bar from the hot rolled state and the cross section of the bar prior to draft.
-
公开(公告)号:DE3718772A1
公开(公告)日:1987-12-17
申请号:DE3718772
申请日:1987-06-04
Applicant: STANADYNE INC
Inventor: BIRMAN STEPHEN P , SMITH RICHARD B , THOMPSON RICHARD L
Abstract: A cold drawn resulfurized and rephosphorized free-machining steel bar has the composition, by weight, C up to 0.08%; Mn 0.6% to 1.4%; Si up to 0.1%; P at least 0.03%; S 0.25% to 0.50%; Cb 0.01% to 0.10%; V up to 0.1%; the sum of Ni, Cr, Mo, and Cu up to 0.15%; balanced iron. The ratio of % Mn/%S is from 1.6 to 4.0, and the ratio of (%Mn- 1.62 x %S)/%Cb is from 2 to 50. The yield strength of the steel bar is further determined by the draft in cold drawing the bar from the hot rolled state and the size and cross section of the bar after draft.
-
公开(公告)号:FR2601697B1
公开(公告)日:1989-08-11
申请号:FR8707998
申请日:1987-06-09
Applicant: STANADYNE INC
Inventor: BIRMAN STEPHEN P , SMITH RICHARD B , THOMSON RICHARD L
Abstract: Stanadyne Case 239 COLD DRAWN FREE-MACHINING RESULFURIZED AND REPHOSPHORIZED STEEL BARS HAVING CONTROLLED MECHANICAL PROPERTIES AND CONTROLLED MACHINABILITY A cold drawn resulfurized and rephosphorized freemachining steel bar has the composition, by weight, C up to 0.08%; Mn 0.6% to 1.4%; Si up to 0.1%; P at least 0.03%; S 0.25% to 0.50%; Cb 0.01% to 0.10%; V up to 0.1%; the sum of Ni, Cr, Mo, and Cu up to 0.15%; balance iron. The ratio of %Mn / %S is from 1.6 to 4.0, and the ratio of (%Mn - 1.62 X %S) / %Cb is from 2 to 50. The yield strength of the steel bar is further determined by the draft in cold drawing the bar from the hot rolled state and the size and cross section of the bar after draft.
-
公开(公告)号:BR8702911A
公开(公告)日:1988-03-08
申请号:BR8702911
申请日:1987-06-09
Applicant: STANADYNE INC
Inventor: BIRMAN STEPHEN P , SMITH RICHARD B , THOMPSON RICHARD L
Abstract: Stanadyne Case 239 COLD DRAWN FREE-MACHINING RESULFURIZED AND REPHOSPHORIZED STEEL BARS HAVING CONTROLLED MECHANICAL PROPERTIES AND CONTROLLED MACHINABILITY A cold drawn resulfurized and rephosphorized freemachining steel bar has the composition, by weight, C up to 0.08%; Mn 0.6% to 1.4%; Si up to 0.1%; P at least 0.03%; S 0.25% to 0.50%; Cb 0.01% to 0.10%; V up to 0.1%; the sum of Ni, Cr, Mo, and Cu up to 0.15%; balance iron. The ratio of %Mn / %S is from 1.6 to 4.0, and the ratio of (%Mn - 1.62 X %S) / %Cb is from 2 to 50. The yield strength of the steel bar is further determined by the draft in cold drawing the bar from the hot rolled state and the size and cross section of the bar after draft.
-
公开(公告)号:IT8748037D0
公开(公告)日:1987-06-09
申请号:IT4803787
申请日:1987-06-09
Applicant: STANADYNE INC
Inventor: BIRMAN STEPHEN P , SMITH RICHARD B , THOMPSON RICHARD L
Abstract: A cold drawn free-machining steel bar having a composition consisting essentially of, in weight percent, C up to 0.15; Mn 0.7 to 1.3; P 0.03 to 0.09; S 0.30 to 0.50; Bi 0.05 to 0.25; the sum of Ni, Cr, Mo and Cu up to 0.15 and the balance iron. The ratio % Mn / %S is from 1.7 to 3.0 and the %Mn-1.62x%S is from 0.05 to 0.40. The ratio %Bi /(%Ni+%Cu) is at least 2.0. The yield strength of the steel bar is further determined by the draft in cold drawing the bar from the hot rolled state and the cross section of the bar prior to draft.
-
公开(公告)号:CA1301490C
公开(公告)日:1992-05-26
申请号:CA538743
申请日:1987-06-03
Applicant: STANADYNE INC
Inventor: BIRMAN STEPHEN P , SMITH RICHARD B , THOMPSON RICHARD L
Abstract: Stanadyne Case 240 COLD DRAWN FREE-MACHINING STEEL BAR INCLUDING BISMUTH A cold drawn free-machining steel bar having a composition consisting essentially of, in weight percent, C up to 0.15 Mn 0.7 to 1.3; P 0.03 to 0.09: S 0.30 to 0.50; Bi 0.05 to 0.25; the sum of Ni, Cr, Mo and Cu up to 0.15 and the balance iron. The ratio %Mn / %S is from 1.7 to 3.0 and the %Mn - 1.62 X %S is from 0.05 to 0.40. The ratio %Bi / (%Ni + %Cu) is at least 2.0. The yield strength of the steel bar is further determined by the draft in cold drawing the bar from the hot rolled state and the cross section of the bar prior to draft.
-
公开(公告)号:GB2191506B
公开(公告)日:1990-01-04
申请号:GB8713199
申请日:1987-06-05
Applicant: STANADYNE INC , WESTERN STEEL GROUP
Inventor: BIRMAN STEPHEN P , SMITH RICHARD B , THOMPSON RICHARD L
Abstract: Stanadyne Case 239 COLD DRAWN FREE-MACHINING RESULFURIZED AND REPHOSPHORIZED STEEL BARS HAVING CONTROLLED MECHANICAL PROPERTIES AND CONTROLLED MACHINABILITY A cold drawn resulfurized and rephosphorized freemachining steel bar has the composition, by weight, C up to 0.08%; Mn 0.6% to 1.4%; Si up to 0.1%; P at least 0.03%; S 0.25% to 0.50%; Cb 0.01% to 0.10%; V up to 0.1%; the sum of Ni, Cr, Mo, and Cu up to 0.15%; balance iron. The ratio of %Mn / %S is from 1.6 to 4.0, and the ratio of (%Mn - 1.62 X %S) / %Cb is from 2 to 50. The yield strength of the steel bar is further determined by the draft in cold drawing the bar from the hot rolled state and the size and cross section of the bar after draft.
-
公开(公告)号:IT1206026B
公开(公告)日:1989-04-05
申请号:IT4803787
申请日:1987-06-09
Applicant: STANADYNE INC
Inventor: BIRMAN STEPHEN P , SMITH RICHARD B , THOMPSON RICHARD L
Abstract: A cold drawn free-machining steel bar having a composition consisting essentially of, in weight percent, C up to 0.15; Mn 0.7 to 1.3; P 0.03 to 0.09; S 0.30 to 0.50; Bi 0.05 to 0.25; the sum of Ni, Cr, Mo and Cu up to 0.15 and the balance iron. The ratio % Mn / %S is from 1.7 to 3.0 and the %Mn-1.62x%S is from 0.05 to 0.40. The ratio %Bi /(%Ni+%Cu) is at least 2.0. The yield strength of the steel bar is further determined by the draft in cold drawing the bar from the hot rolled state and the cross section of the bar prior to draft.
-
-
-
-
-
-
-
-
-