公开(公告)号:KR820000228B1
公开(公告)日:1982-03-08
申请号:KR770002403
申请日:1977-10-17
Applicant: STANDARD OIL CO
Inventor: KLOTZ MARVIN R
IPC: C10G35/095 , B01D53/02 , B01J20/10 , B01J29/00 , B01J29/04 , B01J29/86 , C01B35/12 , C01B39/04 , C01B39/12 , C01B39/38 , C01B39/40 , C07C1/00 , C07C5/22 , C07C5/27 , C07C15/08 , C07C67/00 , C10G47/16 , B01J21/00
Abstract: Cryst. borosilicates with specified crystal structure were prepd. They resemble zeolites. They have the general formula(0.9±0.2) M2/n OB2O3YSiO2ZH2O, where M is cation, n is the charge on the cation, Y is 4-500 and Z is
-
公开(公告)号:CS271488B2
公开(公告)日:1990-10-12
申请号:CS347988
申请日:1988-05-23
Applicant: STANDARD OIL CO
Inventor: KLOTZ MARVIN R
IPC: C10G35/095 , B01D53/02 , B01J20/10 , B01J29/00 , B01J29/04 , B01J29/86 , C01B35/12 , C01B39/04 , C01B39/12 , C01B39/38 , C01B39/40 , C07C1/00 , C07C5/22 , C07C5/27 , C07C15/08 , C07C67/00 , C10G47/16
Abstract: The method of catalytic isomerization of xylene raw material consists of the fact that the xylene raw material is put into polymerisation conditions into contact with crystalline borosilicate as a catalyser with a composition expressed by the molar ratio of oxides where:M means at least one kation with valency n from group comprising tetraalkylammonium kation with 8 to 12 atoms of carbon, alkaline metal kation or mixture of these kations,Y's value is 4 to 500 andZ's value is 0 to 160,while this crystalline borosilicate is characterized by a defined x-ray pattern and assigned intensities. Isomerization conditions include temperatures of 121 to 482 degrees C, overpressure 0 to 7.03 MPa, a molar ratio of hydrogen to carbon within the range of 0 to 20 and a weight hour flow rate 1 to 20.
-
公开(公告)号:PL202144A1
公开(公告)日:1979-04-23
申请号:PL20214477
申请日:1977-11-15
Applicant: STANDARD OIL CO
Inventor: KLOTZ MARVIN R
IPC: B01J20060101 , B01J29/04 , C01B33/12 , C01B33/24 , C07C5/22 , C10G20060101 , B01J
-
公开(公告)号:CS8803479A2
公开(公告)日:1990-02-12
申请号:CS347988
申请日:1988-05-23
Applicant: STANDARD OIL CO
Inventor: KLOTZ MARVIN R
IPC: C10G35/095 , B01D53/02 , B01J20/10 , B01J29/00 , B01J29/04 , B01J29/86 , C01B35/12 , C01B39/04 , C01B39/12 , C01B39/38 , C01B39/40 , C07C1/00 , C07C5/22 , C07C5/27 , C07C15/08 , C07C67/00 , C10G47/16
CPC classification number: C07C5/2732 , B01D53/02 , B01J29/04 , C01B35/1009 , C07C5/2213 , C07C5/2735 , C07C2529/86 , Y02P20/52 , C07C15/08
-
5.
公开(公告)号:CS7706769A2
公开(公告)日:1989-04-14
申请号:CS676977
申请日:1977-10-18
Applicant: STANDARD OIL CO
Inventor: KLOTZ MARVIN R
IPC: B01D53/02 , B01J20/10 , B01J21/02 , B01J21/06 , B01J29/86 , C01B33/20 , C01B35/00 , C01B35/10 , C01B35/12 , C01B39/12 , C07B31/00 , C07B61/00 , C07C1/00 , C07C5/22 , C07C5/25 , C07C5/27 , C07C9/00 , C07C9/14 , C07C15/08 , C07C67/00 , C10G11/05 , C10G35/06 , C10G47/16 , B01J21/00
CPC classification number: C10G47/16 , B01D53/02 , B01J29/86 , C01B35/1009 , C07C5/2213 , C07C5/2732 , C07C5/2735 , C07C2529/86 , C10G11/05 , Y02P20/52 , C07C15/08
-
6.
公开(公告)号:CS676977A2
公开(公告)日:1989-04-14
申请号:CS676977
申请日:1977-10-18
Applicant: STANDARD OIL CO
Inventor: KLOTZ MARVIN R
-
公开(公告)号:RO76300A
公开(公告)日:1981-11-24
申请号:RO9211077
申请日:1977-11-14
Applicant: STANDARD OIL CO
Inventor: KLOTZ MARVIN R
IPC: B01J20060101 , B01J29/04 , C01B33/12 , C01B33/24 , C07C5/22 , C10G20060101
-
公开(公告)号:CS347988A2
公开(公告)日:1990-02-12
申请号:CS347988
申请日:1988-05-23
Applicant: STANDARD OIL CO
Inventor: KLOTZ MARVIN R
IPC: C10G35/095 , B01D53/02 , B01J20/10 , B01J29/00 , B01J29/04 , B01J29/86 , C01B35/12 , C01B39/04 , C01B39/12 , C01B39/38 , C01B39/40 , C07C1/00 , C07C5/22 , C07C5/27 , C07C15/08 , C07C67/00 , C10G47/16
Abstract: The method of catalytic isomerization of xylene raw material consists of the fact that the xylene raw material is put into polymerisation conditions into contact with crystalline borosilicate as a catalyser with a composition expressed by the molar ratio of oxides where:M means at least one kation with valency n from group comprising tetraalkylammonium kation with 8 to 12 atoms of carbon, alkaline metal kation or mixture of these kations,Y's value is 4 to 500 andZ's value is 0 to 160,while this crystalline borosilicate is characterized by a defined x-ray pattern and assigned intensities. Isomerization conditions include temperatures of 121 to 482 degrees C, overpressure 0 to 7.03 MPa, a molar ratio of hydrogen to carbon within the range of 0 to 20 and a weight hour flow rate 1 to 20.
-
9.
公开(公告)号:CS266302B2
公开(公告)日:1989-12-13
申请号:CS676977
申请日:1977-10-18
Applicant: STANDARD OIL CO
Inventor: KLOTZ MARVIN R
-
公开(公告)号:CA1101633A
公开(公告)日:1981-05-26
申请号:CA288362
申请日:1977-10-07
Applicant: STANDARD OIL CO
Inventor: KLOTZ MARVIN R
IPC: B01D53/02 , B01J20/10 , B01J21/02 , B01J21/06 , B01J29/86 , C01B33/20 , C01B35/00 , C01B35/10 , C01B35/12 , C01B39/12 , C07B31/00 , C07B61/00 , C07C1/00 , C07C5/22 , C07C5/25 , C07C5/27 , C07C9/00 , C07C9/14 , C07C15/08 , C07C67/00 , C10G11/05 , C10G35/06 , C10G47/16
Abstract: CRYSTALLINE BOROSILICATE (AMS-1B) AND PROCESS USE A new crystalline borosilicate composition of matter and process using it wherein the composition is expressed as mole ratios of oxides as follows: 0.9 ? 0.2 M2/nO : B2O3 : YSiO2 : ZH2O wherein M is at least one cation, n is the valence of the cation, Y is generally a value of from about 4 to about 500 or higher, and Z is a value of from 0 to about 160, and characterized by a specified X-ray powder diffraction pattern as is described herein. Catalytic conversion including processes such as isomerization, disproportionation, or transalkylation are also disclosed.
-
-
-
-
-
-
-
-
-