    Abstract: PROBLEM TO BE SOLVED: To provide an improved catalyst for the catalytic hydrogenation of maleic acid, maleic anhydride or other hydrogenatable precursor to 1,4-butanediol and tetrahydrofuran.
    SOLUTION: The invention is a catalyst essentially comprising palladium, silver, rhenium and iron. Another embodiment of the invention is a method for making such catalyst for the production of 1,4-buthanediol comprising: (i) oxidizing a carbon support by bringing the carbon support contact with an oxidizing agent; (ii) impregnating in one or more impregnation steps comprising contacting a carbon support with a metal source of palladium, silver, rhenium and iron; (iii) drying the impregnated carbon support to remove solvent after each impregnation step; and (iv) heating the impregnated carbon support from ambient temperature to a temperature of between about 100°C and about 350°C under reducing conditions.
    COPYRIGHT: (C)2007,JPO&INPIT

    Abstract translation: 要解决的问题:为马来酸,马来酸酐或其他可氢化前体催化氢化成1,4-丁二醇和四氢呋喃提供改进的催化剂。 解决方案:本发明是一种主要包含钯,银,铼和铁的催化剂。 本发明的另一个实施方案是制备用于生产1,4-丁二醇的这种催化剂的方法,其包括:(i)通过使碳载体与氧化剂接触而氧化碳载体; (ii)浸渍在一个或多个浸渍步骤中,包括使碳载体与钯,银,铼和铁的金属源接触; (iii)在每次浸渍步骤之后干燥浸渍的碳载体以除去溶剂; 和(iv)在还原条件下将浸渍的碳载体从环境温度加热至约100℃至约350℃的温度。 版权所有(C)2007,JPO&INPIT